Journal article · 2020 · Open access
Area-Selective Atomic Layer Deposition of Two-Dimensional WS2 Nanolayers
ACS Materials Letters, 2(5), 511–518 · Published 8 April 2020 · DOI 10.1021/acsmaterialslett.0c00093
In brief
“Area-Selective Atomic Layer Deposition of Two-Dimensional WS2 Nanolayers” is a 2020 journal article by Shashank Balasubramanyam and 5 co-authors, published in ACS Materials Letters. OpenAlex counts 91 citations as of 17 November 2026, which puts it in the top 2% of works published in 2020 by citations. It is open access under a CC BY-NC-ND licence: the full text is free to read at ACS Materials Letters.
- Citations
- 91
- Most cited in
- 2025 (20)
- Field-weighted impact
- 3.92
- References
- 50
- Authors
- 6
Abstract
With downscaling of device dimensions, two-dimensional (2D) semiconducting transition metal dichalcogenides (TMDs) such as WS2 are being considered as promising materials for future applications in nanoelectronics. However, at these nanoscale regimes, incorporating TMD layers in the device architecture with precise control of critical features is challenging using current top-down processing techniques. In this contribution, we pioneer the combination of two key avenues in atomic-scale processing: area-selective atomic layer deposition (AS-ALD) and growth of 2D materials, and demonstrate bottom-up processing of 2D WS2 nanolayers. Area-selective deposition of WS2 nanolayers is enabled using an ABC-type plasma-enhanced ALD process involving acetylacetone (Hacac) as inhibitor (A), bis(tert-butylimido)-bis(dimethylamido)-tungsten as precursor (B), and H2S plasma as the co-reactant (C) at a low deposition temperature of 250 °C. The developed AS-ALD process results in the immediate growth of WS2 on SiO2 while effectively blocking growth on Al2O3 as confirmed by in situ spectroscopic ellipsometry and ex situ X-ray photoelectron spectroscopy measurements. As a proof of concept, the AS-ALD process is demonstrated on patterned Al2O3/SiO2 surfaces. The AS-ALD WS2 films exhibited sharp Raman (E2g1 and A1g) peaks on SiO2, a fingerprint of crystalline WS2 layers, upon annealing at temperatures within the thermal budget of semiconductor back-end-of-line processing (≤450 °C). Our AS-ALD process also allows selective growth on various TMDs and transition metal oxides while blocking growth on HfO2 and TiO2. It is expected that this work will lay the foundation for area-selective ALD of other 2D materials.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Balasubramanyam, S., Merkx, M. J. M., Verheijen, M. A., Kessels, W. M. M., Mackus, A. J. M., & Bol, A. A. (2020). Area-Selective Atomic Layer Deposition of Two-Dimensional WS2 Nanolayers. ACS Materials Letters, 2(5), 511–518. https://doi.org/10.1021/acsmaterialslett.0c00093
MLA 9
Balasubramanyam, Shashank, et al. “Area-Selective Atomic Layer Deposition of Two-Dimensional WS2 Nanolayers.” ACS Materials Letters, vol. 2, no. 5, 2020, pp. 511–518. https://doi.org/10.1021/acsmaterialslett.0c00093.
Chicago
Balasubramanyam, Shashank, Marc J. M. Merkx, Marcel A. Verheijen, W. M. M. Kessels, Adriaan J. M. Mackus, and Ageeth Anke Bol. 2020. “Area-Selective Atomic Layer Deposition of Two-Dimensional WS2 Nanolayers.” ACS Materials Letters 2 (5): 511–518. https://doi.org/10.1021/acsmaterialslett.0c00093.
Harvard
Balasubramanyam, S. et al. (2020) ‘Area-Selective Atomic Layer Deposition of Two-Dimensional WS2 Nanolayers’, ACS Materials Letters, 2(5), pp. 511–518. doi:10.1021/acsmaterialslett.0c00093.
IEEE
S. Balasubramanyam, M. J. M. Merkx, M. A. Verheijen, W. M. M. Kessels, A. J. M. Mackus, and A. A. Bol, “Area-Selective Atomic Layer Deposition of Two-Dimensional WS2 Nanolayers,” ACS Materials Letters, vol. 2, no. 5, pp. 511–518, 2020, doi: 10.1021/acsmaterialslett.0c00093.
BibTeX
@article{balasubramanyam2020area,
title = {{Area-Selective Atomic Layer Deposition of Two-Dimensional WS2 Nanolayers}},
author = {Balasubramanyam, Shashank and Merkx, Marc J. M. and Verheijen, Marcel A. and Kessels, W. M. M. and Mackus, Adriaan J. M. and Bol, Ageeth Anke},
journal = {ACS Materials Letters},
year = {2020},
volume = {2},
number = {5},
pages = {511--518},
doi = {10.1021/acsmaterialslett.0c00093},
url = {https://doi.org/10.1021/acsmaterialslett.0c00093}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2020 | 6 | |
| 2021 | 14 | |
| 2022 | 13 | |
| 2023 | 10 | |
| 2024 | 17 | |
| 2025 | 20 | |
| 2026 | 11 |
Its field-weighted citation impact is 3.92: it has been cited 3.92 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Materials Science › Materials Chemistry › 2D Materials and Applications
- area-selective atomic layer deposition
- transition metal dichalcogenides
- two-dimensional materials
- bottom-up growth
- plasma-enhanced ALD
- annealing
- nanoelectronics
Work with this paper
Most-cited papers in Materials Science
- Electric Field Effect in Atomically Thin Carbon FilmsKostya S. Novoselov, Andre K. Geim, Sergey V. Morozov and 5 more · Science · 2004 · 67,474 citations
- Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenidesROBERT D. SHANNON · Acta Crystallographica Section A · 1976 · 66,944 citations
- Ab initio molecular dynamics for liquid metalsGeorg Kresse, J. Häfner · Physical review. B, Condensed matter · 1993 · 46,320 citations
- Helical microtubules of graphitic carbonSumio Iijima · Nature · 1991 · 43,639 citations
- The rise of grapheneAndre K. Geim, Kostya S. Novoselov · Nature Materials · 2007 · 40,328 citations
Questions about this paper
How do I cite this paper in APA style?
Balasubramanyam, S., Merkx, M. J. M., Verheijen, M. A., Kessels, W. M. M., Mackus, A. J. M., & Bol, A. A. (2020). Area-Selective Atomic Layer Deposition of Two-Dimensional WS2 Nanolayers. ACS Materials Letters, 2(5), 511–518. https://doi.org/10.1021/acsmaterialslett.0c00093
How many times has this paper been cited?
91 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access at ACS Materials Letters: sign in and open the PDF from this page.
Who wrote this paper?
Shashank Balasubramanyam, Marc J. M. Merkx, Marcel A. Verheijen, W. M. M. Kessels, Adriaan J. M. Mackus, Ageeth Anke Bol.
What is the DOI of this paper?
10.1021/acsmaterialslett.0c00093, permanently at https://doi.org/10.1021/acsmaterialslett.0c00093. Sign in and open it from this page.
Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.