Journal article · 2026 · Open access
Structuring large area WS2 layers grown by atomic layer deposition
Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 44(3) · Published 2 April 2026 · DOI 10.1116/6.0005225
In brief
“Structuring large area WS2 layers grown by atomic layer deposition” is a 2026 journal article by Leon Doman and 4 co-authors, published in Journal of Vacuum Science & Technology A Vacuum Surfaces and Films. OpenAlex counts 2 citations as of 17 November 2026, which puts it in the top 5% of works published in 2026 by citations. It is open access under a CC BY-NC-ND licence: the full text is free to read at Journal of Vacuum Science & Technology A Vacuum Surfaces and Films.
- Citations
- 2
- Most cited in
- 2026 (2)
- Field-weighted impact
- 2.08
- References
- 58
- Authors
- 5
Abstract
The large-scale deposition and integration of 2D materials on 200 mm wafers for emerging microelectronic applications are highly challenging. Throughout the processing, significant issues in controlling material growth and patterning must be addressed. Therefore, this study introduces a new approach for bottom-up growth and subsequent patterning of ultrathin 2D WS2 layers on 200 mm wafers. To achieve this, atomic layer deposition (ALD) was used to grow WS2 thin films directly on 200 mm wafers, which were then patterned by photolithography and ion-beam etching. To prevent degradation and delamination of the WS2 layer during patterning, an in situ Al2O3 ALD capping layer is employed. Even after treatment in boiling de-ionized water, which porosifies the Al2O3 as needed for sensing applications, the WS2 and underlying features remain intact. To investigate the effects of patterning and capping processes in detail, Raman spectroscopy, scanning electron microscopy, and transmission electron microscopy were used. The detailed analysis shows that the proposed strategies enable patterning of WS2 layers on 200 mm wafers using Al2O3 capping layers. Electrical measurements of the WS2 patterned on interdigitated electrodes show a linear current response and an average resistance of 0.4 ± 0.26 MΩ across the 200 mm wafer. Overall, our findings indicate a promising step toward the scalable integration of WS2 into various micro- and nanosystems, especially sensors, and support future scaling of these processes.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Doman, L., Boysen, N., Gemming, T., Shi, H., & Devi, A. (2026). Structuring large area WS2 layers grown by atomic layer deposition. Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 44(3). https://doi.org/10.1116/6.0005225
MLA 9
Doman, Leon, et al. “Structuring large area WS2 layers grown by atomic layer deposition.” Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, vol. 44, no. 3, 2026. https://doi.org/10.1116/6.0005225.
Chicago
Doman, Leon, Nils Boysen, Thomas Gemming, Haowen Shi, and Anjana Devi. 2026. “Structuring large area WS2 layers grown by atomic layer deposition.” Journal of Vacuum Science & Technology A Vacuum Surfaces and Films 44 (3). https://doi.org/10.1116/6.0005225.
Harvard
Doman, L. et al. (2026) ‘Structuring large area WS2 layers grown by atomic layer deposition’, Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 44(3). doi:10.1116/6.0005225.
IEEE
L. Doman, N. Boysen, T. Gemming, H. Shi, and A. Devi, “Structuring large area WS2 layers grown by atomic layer deposition,” Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, vol. 44, no. 3, 2026, doi: 10.1116/6.0005225.
BibTeX
@article{doman2026structuring,
title = {{Structuring large area WS2 layers grown by atomic layer deposition}},
author = {Doman, Leon and Boysen, Nils and Gemming, Thomas and Shi, Haowen and Devi, Anjana},
journal = {Journal of Vacuum Science \& Technology A Vacuum Surfaces and Films},
year = {2026},
volume = {44},
number = {3},
doi = {10.1116/6.0005225},
url = {https://doi.org/10.1116/6.0005225}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Topic and keywords
Physical Sciences › Materials Science › Materials Chemistry › 2D Materials and Applications
- tungsten disulfide
- transition metal dichalcogenides
- two-dimensional materials
- atomic layer deposition
- 200 mm wafers
- bottom-up growth
- photolithography
- ion beam etching
Work with this paper
Most-cited papers in Materials Science
- Electric Field Effect in Atomically Thin Carbon FilmsKostya S. Novoselov, Andre K. Geim, Sergey V. Morozov and 5 more · Science · 2004 · 67,474 citations
- Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenidesROBERT D. SHANNON · Acta Crystallographica Section A · 1976 · 66,944 citations
- Ab initio molecular dynamics for liquid metalsGeorg Kresse, J. Häfner · Physical review. B, Condensed matter · 1993 · 46,320 citations
- Helical microtubules of graphitic carbonSumio Iijima · Nature · 1991 · 43,639 citations
- The rise of grapheneAndre K. Geim, Kostya S. Novoselov · Nature Materials · 2007 · 40,328 citations
Questions about this paper
How do I cite this paper in APA style?
Doman, L., Boysen, N., Gemming, T., Shi, H., & Devi, A. (2026). Structuring large area WS2 layers grown by atomic layer deposition. Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 44(3). https://doi.org/10.1116/6.0005225
How many times has this paper been cited?
2 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access at Journal of Vacuum Science & Technology A Vacuum Surfaces and Films: sign in and open the full text from this page.
Who wrote this paper?
Leon Doman, Nils Boysen, Thomas Gemming, Haowen Shi, Anjana Devi.
What is the DOI of this paper?
10.1116/6.0005225, permanently at https://doi.org/10.1116/6.0005225. Sign in and open it from this page.
Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.