Journal article · 2017 · Open access

Plasma-Enhanced Atomic Layer Deposition of Two-Dimensional WS2 from WF6, H2 Plasma, and H2S

Benjamin Groven, Markus Heyne, Ankit Nalin Mehta, Hugo Bender, Thomas Nuytten, Johan Meersschaut, Thierry S. Conard, Patrick Bernard Verdonck, Sven Van Elshocht, Wilfried Vandervorst, Stefan De Gendt, Marc Heyns and 3 more

Chemistry of Materials, 29(7), 2927–2938 · Published 7 March 2017 · DOI 10.1021/acs.chemmater.6b05214

Open PDFView at the publisherCite this paper

In brief

“Plasma-Enhanced Atomic Layer Deposition of Two-Dimensional WS2 from WF6, H2 Plasma, and H2S” is a 2017 journal article by Benjamin Groven and 14 co-authors, published in Chemistry of Materials. OpenAlex counts 89 citations as of 17 November 2026, which puts it in the top 7% of works published in 2017 by citations. It is open access: the full text is free to read at Lirias (KU Leuven).

Citations
89
Most cited in
2020 (17)
Field-weighted impact
4.67
References
66
Authors
15

Abstract

Two-dimensional (2D) transition metal dichalcogenides are potential low dissipative semiconductor materials for nanoelectronic devices. Such applications require the deposition of these materials in their crystalline form and with controlled number of monolayers on large area substrates, preferably using deposition temperatures compatible with temperature sensitive structures. This paper presents a low temperature plasma-enhanced atomic layer deposition (PEALD) process for 2D WS 2 based on a ternary reaction cycle consisting of consecutive WF 6, H 2 plasma, and H 2 S reactions. Strongly textured, nanocrystalline WS 2 is grown at 300 °C. The composition and crystallinity of these layers depends on the PEALD process conditions, as understood by a model for the redox chemistry of this process. The H 2 plasma is essential for the deposition of WS 2 as it enables the reduction of −W 6+ F x surface species. Nevertheless, the impact of subsurface reduction reactions needs to be minimized to obtain WS 2 with well-controlled composition (S/W ratio of 2).

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Groven, B., Heyne, M., Mehta, A. N., Bender, H., Nuytten, T., Meersschaut, J., Conard, T. S., Verdonck, P. B., Van Elshocht, S., Vandervorst, W., De Gendt, S., Heyns, M., Radu, I. P., Caymax, M. R., & Delabie, A. (2017). Plasma-Enhanced Atomic Layer Deposition of Two-Dimensional WS2 from WF6, H2 Plasma, and H2S. Chemistry of Materials, 29(7), 2927–2938. https://doi.org/10.1021/acs.chemmater.6b05214

MLA 9

Groven, Benjamin, et al. “Plasma-Enhanced Atomic Layer Deposition of Two-Dimensional WS2 from WF6, H2 Plasma, and H2S.” Chemistry of Materials, vol. 29, no. 7, 2017, pp. 2927–2938. https://doi.org/10.1021/acs.chemmater.6b05214.

Chicago

Groven, Benjamin, Markus Heyne, Ankit Nalin Mehta, Hugo Bender, Thomas Nuytten, Johan Meersschaut, Thierry S. Conard, et al. 2017. “Plasma-Enhanced Atomic Layer Deposition of Two-Dimensional WS2 from WF6, H2 Plasma, and H2S.” Chemistry of Materials 29 (7): 2927–2938. https://doi.org/10.1021/acs.chemmater.6b05214.

Harvard

Groven, B. et al. (2017) ‘Plasma-Enhanced Atomic Layer Deposition of Two-Dimensional WS2 from WF6, H2 Plasma, and H2S’, Chemistry of Materials, 29(7), pp. 2927–2938. doi:10.1021/acs.chemmater.6b05214.

IEEE

B. Groven et al., “Plasma-Enhanced Atomic Layer Deposition of Two-Dimensional WS2 from WF6, H2 Plasma, and H2S,” Chemistry of Materials, vol. 29, no. 7, pp. 2927–2938, 2017, doi: 10.1021/acs.chemmater.6b05214.

BibTeX

@article{groven2017plasma,
  title     = {{Plasma-Enhanced Atomic Layer Deposition of Two-Dimensional WS2 from WF6, H2 Plasma, and H2S}},
  author    = {Groven, Benjamin and Heyne, Markus and Mehta, Ankit Nalin and Bender, Hugo and Nuytten, Thomas and Meersschaut, Johan and Conard, Thierry S. and Verdonck, Patrick Bernard and Van Elshocht, Sven and Vandervorst, Wilfried and De Gendt, Stefan and Heyns, Marc and Radu, Iuliana P. and Caymax, Matty R. and Delabie, Annelies},
  journal   = {Chemistry of Materials},
  year      = {2017},
  volume    = {29},
  number    = {7},
  pages     = {2927--2938},
  doi       = {10.1021/acs.chemmater.6b05214},
  url       = {https://doi.org/10.1021/acs.chemmater.6b05214}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
201744
20181212
20191616
20201717
20211414
202288
202388
202444
202522
202644

Its field-weighted citation impact is 4.67: it has been cited 4.67 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Materials Science › Materials Chemistry › 2D Materials and Applications

  • plasma-enhanced atomic layer deposition
  • tungsten disulfide
  • transition metal dichalcogenides
  • WF6
  • hydrogen plasma
  • hydrogen sulfide
  • low-temperature deposition
  • redox chemistry

Work with this paper

Most-cited papers in Materials Science

All highly cited Materials Science papers

Questions about this paper

How do I cite this paper in APA style?

Groven, B., Heyne, M., Mehta, A. N., Bender, H., Nuytten, T., Meersschaut, J., Conard, T. S., Verdonck, P. B., Van Elshocht, S., Vandervorst, W., De Gendt, S., Heyns, M., Radu, I. P., Caymax, M. R., & Delabie, A. (2017). Plasma-Enhanced Atomic Layer Deposition of Two-Dimensional WS2 from WF6, H2 Plasma, and H2S. Chemistry of Materials, 29(7), 2927–2938. https://doi.org/10.1021/acs.chemmater.6b05214

How many times has this paper been cited?

89 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

Yes. It is open access at Lirias (KU Leuven): sign in and open the PDF from this page.

Who wrote this paper?

Benjamin Groven, Markus Heyne, Ankit Nalin Mehta, Hugo Bender, Thomas Nuytten, Johan Meersschaut, Thierry S. Conard, Patrick Bernard Verdonck, Sven Van Elshocht, Wilfried Vandervorst, Stefan De Gendt, Marc Heyns and 3 more.

What is the DOI of this paper?

10.1021/acs.chemmater.6b05214, permanently at https://doi.org/10.1021/acs.chemmater.6b05214. Sign in and open it from this page.

Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.