Journal article · 2022 · Open access
Nucleation and growth mechanism for atomic layer deposition of Al2O3 on two-dimensional WS2 monolayer
Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 41(1) · Published 29 November 2022 · DOI 10.1116/6.0001913
In brief
“Nucleation and growth mechanism for atomic layer deposition of Al2O3 on two-dimensional WS2 monolayer” is a 2022 journal article by Tsu-Ting Lee and 6 co-authors, published in Journal of Vacuum Science & Technology A Vacuum Surfaces and Films. OpenAlex counts 9 citations as of 17 November 2026, which puts it in the top 4% of works published in 2022 by citations. It is open access under a CC BY licence: the full text is free to read at Journal of Vacuum Science & Technology A Vacuum Surfaces and Films.
- Citations
- 9
- Most cited in
- 2025 (5)
- Field-weighted impact
- 0.33
- References
- 45
- Authors
- 7
Abstract
Nanoelectronics holds significant promise for two-dimensional (2D) semiconducting transition metal dichalcogenide (TMD) applications. On a polycrystalline WS2 monolayer created by metal-organic chemical vapor deposition (MOCVD) at 950 °C, we studied the nucleation, growth, and development of Al2O3 atomic layer deposition (ALD) on a SiO2/Si substrate. In this investigation, we used various complementary characterization methods, such as Raman spectroscopy, elastic recoil detection, atomic force microscopy, and time-of-flight secondary ion mass spectrometry, to understand thoroughly the intrinsic reactivity of WS2. Strong peak intensity changes at the interfaces in the Raman line scans of the SiO2/Si patterns suggest extremely crystalline WS2. After multiple ALD cycles, triangular WS2 crystals were decorated to provide a two-dimensional growth mode with a great selectivity for grain boundaries and step edges. The results of this work can be used for further exploration of the TMD monolayer structure and properties, which is essential for tailoring 2D materials for a specific application in devices.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Lee, T.-T., Chiranjeevulu, K., Sireesha, P., Cott, D. J., Delabie, A., Dee, C. F., & Chang, E. Y. (2022). Nucleation and growth mechanism for atomic layer deposition of Al2O3 on two-dimensional WS2 monolayer. Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 41(1). https://doi.org/10.1116/6.0001913
MLA 9
Lee, Tsu-Ting, et al. “Nucleation and growth mechanism for atomic layer deposition of Al2O3 on two-dimensional WS2 monolayer.” Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, vol. 41, no. 1, 2022. https://doi.org/10.1116/6.0001913.
Chicago
Lee, Tsu-Ting, Kashi Chiranjeevulu, Pedaballi Sireesha, Dáire J. Cott, Annelies Delabie, Chang Fu Dee, and Edward Yi Chang. 2022. “Nucleation and growth mechanism for atomic layer deposition of Al2O3 on two-dimensional WS2 monolayer.” Journal of Vacuum Science & Technology A Vacuum Surfaces and Films 41 (1). https://doi.org/10.1116/6.0001913.
Harvard
Lee, T.-T. et al. (2022) ‘Nucleation and growth mechanism for atomic layer deposition of Al2O3 on two-dimensional WS2 monolayer’, Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 41(1). doi:10.1116/6.0001913.
IEEE
T.-T. Lee et al., “Nucleation and growth mechanism for atomic layer deposition of Al2O3 on two-dimensional WS2 monolayer,” Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, vol. 41, no. 1, 2022, doi: 10.1116/6.0001913.
BibTeX
@article{lee2022nucleation,
title = {{Nucleation and growth mechanism for atomic layer deposition of Al2O3 on two-dimensional WS2 monolayer}},
author = {Lee, Tsu-Ting and Chiranjeevulu, Kashi and Sireesha, Pedaballi and Cott, Dáire J. and Delabie, Annelies and Dee, Chang Fu and Chang, Edward Yi},
journal = {Journal of Vacuum Science \& Technology A Vacuum Surfaces and Films},
year = {2022},
volume = {41},
number = {1},
doi = {10.1116/6.0001913},
url = {https://doi.org/10.1116/6.0001913}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Topic and keywords
Physical Sciences › Materials Science › Materials Chemistry › 2D Materials and Applications
- atomic layer deposition
- alumina
- monolayer WS2
- transition metal dichalcogenides
- nucleation and growth
- two-dimensional materials
- two-dimensional growth
- SiO2/Si substrate
Work with this paper
Most-cited papers in Materials Science
- Electric Field Effect in Atomically Thin Carbon FilmsKostya S. Novoselov, Andre K. Geim, Sergey V. Morozov and 5 more · Science · 2004 · 67,474 citations
- Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenidesROBERT D. SHANNON · Acta Crystallographica Section A · 1976 · 66,944 citations
- Ab initio molecular dynamics for liquid metalsGeorg Kresse, J. Häfner · Physical review. B, Condensed matter · 1993 · 46,320 citations
- Helical microtubules of graphitic carbonSumio Iijima · Nature · 1991 · 43,639 citations
- The rise of grapheneAndre K. Geim, Kostya S. Novoselov · Nature Materials · 2007 · 40,328 citations
Questions about this paper
How do I cite this paper in APA style?
Lee, T.-T., Chiranjeevulu, K., Sireesha, P., Cott, D. J., Delabie, A., Dee, C. F., & Chang, E. Y. (2022). Nucleation and growth mechanism for atomic layer deposition of Al2O3 on two-dimensional WS2 monolayer. Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 41(1). https://doi.org/10.1116/6.0001913
How many times has this paper been cited?
9 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access at Journal of Vacuum Science & Technology A Vacuum Surfaces and Films: sign in and open the PDF from this page.
Who wrote this paper?
Tsu-Ting Lee, Kashi Chiranjeevulu, Pedaballi Sireesha, Dáire J. Cott, Annelies Delabie, Chang Fu Dee, Edward Yi Chang.
What is the DOI of this paper?
10.1116/6.0001913, permanently at https://doi.org/10.1116/6.0001913. Sign in and open it from this page.
Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.