Nucleation mechanism during WS2 plasma enhanced atomic layer deposition on amorphous Al2O3 and sapphire substrates
Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 36(1) · Published 16 November 2017 · DOI 10.1116/1.5003361
In brief
“Nucleation mechanism during WS2 plasma enhanced atomic layer deposition on amorphous Al2O3 and sapphire substrates” is a 2017 journal article by Benjamin Groven and 13 co-authors, published in Journal of Vacuum Science & Technology A Vacuum Surfaces and Films. OpenAlex counts 42 citations as of 17 November 2026, which puts it in the top 7% of works published in 2017 by citations. It is open access: the full text is free to read at Lirias (KU Leuven).
- Citations
- 42
- Most cited in
- 2020 (9)
- Field-weighted impact
- 1.91
- References
- 46
- Authors
- 14
Abstract
The structure, crystallinity, and properties of as-deposited two-dimensional (2D) transition metal dichalcogenides are determined by nucleation mechanisms in the deposition process. 2D materials grown by atomic layer deposition (ALD) in the absence of a template are polycrystalline or amorphous. Little is known about their nucleation mechanisms. Therefore, the nucleation behavior of WS2 during plasma enhanced ALD from WF6, H2 plasma, and H2S at 300 °C is investigated on amorphous ALD Al2O3 starting surface and on monocrystalline, bulk sapphire. Preferential interaction of the precursors with the Al2O3 starting surface promotes fast closure of the WS2 layer. The WS2 layers are fully continuous at WS2 content corresponding to only 1.2 WS2 monolayers. On amorphous Al2O3, (0002) textured and polycrystalline WS2 layers form with grain size of 5 to 20 nm due to high nucleation density (∼1014 nuclei/cm2). The WS2 growth mode changes from 2D (layer-by-layer) growth on the initial Al2O3 surface to three-dimensional (Volmer–Weber) growth after WS2 layer closure. Further growth proceeds from both WS2 basal planes in register with the underlying WS2 grain, and from or over grain boundaries of the underlying WS2 layer with different in-plane orientation. In contrast, on monocrystalline sapphire, WS2 crystal grains can locally align along a preferred in-plane orientation. Epitaxial seeding occurs locally albeit a large portion of crystals remain randomly oriented, presumably due to the low deposition temperature. The WS2 sheet resistance is 168 MΩ μm, suggesting that charge transport in the WS2 layers is limited by grain boundaries.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Groven, B., Mehta, A. N., Bender, H., Smets, Q., Meersschaut, J., Franquet, A., Conard, T. S., Nuytten, T., Verdonck, P. B., Vandervorst, W., Heyns, M., Radu, I. P., Caymax, M. R., & Delabie, A. (2017). Nucleation mechanism during WS2 plasma enhanced atomic layer deposition on amorphous Al2O3 and sapphire substrates. Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 36(1). https://doi.org/10.1116/1.5003361
MLA 9
Groven, Benjamin, et al. “Nucleation mechanism during WS2 plasma enhanced atomic layer deposition on amorphous Al2O3 and sapphire substrates.” Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, vol. 36, no. 1, 2017. https://doi.org/10.1116/1.5003361.
Chicago
Groven, Benjamin, Ankit Nalin Mehta, Hugo Bender, Quentin Smets, Johan Meersschaut, Alexis Franquet, Thierry S. Conard, et al. 2017. “Nucleation mechanism during WS2 plasma enhanced atomic layer deposition on amorphous Al2O3 and sapphire substrates.” Journal of Vacuum Science & Technology A Vacuum Surfaces and Films 36 (1). https://doi.org/10.1116/1.5003361.
Harvard
Groven, B. et al. (2017) ‘Nucleation mechanism during WS2 plasma enhanced atomic layer deposition on amorphous Al2O3 and sapphire substrates’, Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 36(1). doi:10.1116/1.5003361.
IEEE
B. Groven et al., “Nucleation mechanism during WS2 plasma enhanced atomic layer deposition on amorphous Al2O3 and sapphire substrates,” Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, vol. 36, no. 1, 2017, doi: 10.1116/1.5003361.
BibTeX
@article{groven2017nucleation,
title = {{Nucleation mechanism during WS2 plasma enhanced atomic layer deposition on amorphous Al2O3 and sapphire substrates}},
author = {Groven, Benjamin and Mehta, Ankit Nalin and Bender, Hugo and Smets, Quentin and Meersschaut, Johan and Franquet, Alexis and Conard, Thierry S. and Nuytten, Thomas and Verdonck, Patrick Bernard and Vandervorst, Wilfried and Heyns, Marc and Radu, Iuliana P. and Caymax, Matty R. and Delabie, Annelies},
journal = {Journal of Vacuum Science \& Technology A Vacuum Surfaces and Films},
year = {2017},
volume = {36},
number = {1},
doi = {10.1116/1.5003361},
url = {https://doi.org/10.1116/1.5003361}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2018 | 5 | |
| 2019 | 4 | |
| 2020 | 9 | |
| 2021 | 8 | |
| 2022 | 3 | |
| 2023 | 2 | |
| 2024 | 3 | |
| 2025 | 6 | |
| 2026 | 2 |
Its field-weighted citation impact is 1.91: it has been cited 1.91 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Materials Science › Materials Chemistry › 2D Materials and Applications
- tungsten disulfide
- transition metal dichalcogenides
- nucleation mechanism
- plasma-enhanced atomic layer deposition
- amorphous Al2O3
- sapphire substrate
- Volmer-Weber growth
- sheet resistance
Work with this paper
Most-cited papers in Materials Science
- Electric Field Effect in Atomically Thin Carbon FilmsKostya S. Novoselov, Andre K. Geim, Sergey V. Morozov and 5 more · Science · 2004 · 67,474 citations
- Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenidesROBERT D. SHANNON · Acta Crystallographica Section A · 1976 · 66,944 citations
- Ab initio molecular dynamics for liquid metalsGeorg Kresse, J. Häfner · Physical review. B, Condensed matter · 1993 · 46,320 citations
- Helical microtubules of graphitic carbonSumio Iijima · Nature · 1991 · 43,639 citations
- The rise of grapheneAndre K. Geim, Kostya S. Novoselov · Nature Materials · 2007 · 40,328 citations
Questions about this paper
How do I cite this paper in APA style?
Groven, B., Mehta, A. N., Bender, H., Smets, Q., Meersschaut, J., Franquet, A., Conard, T. S., Nuytten, T., Verdonck, P. B., Vandervorst, W., Heyns, M., Radu, I. P., Caymax, M. R., & Delabie, A. (2017). Nucleation mechanism during WS2 plasma enhanced atomic layer deposition on amorphous Al2O3 and sapphire substrates. Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 36(1). https://doi.org/10.1116/1.5003361
How many times has this paper been cited?
42 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access at Lirias (KU Leuven): sign in and open the PDF from this page.
Who wrote this paper?
Benjamin Groven, Ankit Nalin Mehta, Hugo Bender, Quentin Smets, Johan Meersschaut, Alexis Franquet, Thierry S. Conard, Thomas Nuytten, Patrick Bernard Verdonck, Wilfried Vandervorst, Marc Heyns, Iuliana P. Radu and 2 more.
What is the DOI of this paper?
10.1116/1.5003361, permanently at https://doi.org/10.1116/1.5003361. Sign in and open it from this page.
Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.