Atomic Layer Deposition of WS2 Using Organic Precursors

Hiroshi Yokota, Sota Higashi, Hideaki Machida, Masato Ishikawa, Hiroshi Sudoh, Hitoshi Wakabayashi, Naomi Sawamoto, Ryo Yokogawa, Atsushi Ogura

ECS Meeting Abstracts, MA2025-01(31), 1599 · Published 11 July 2025 · DOI 10.1149/ma2025-01311599mtgabs

View at the publisherCite this paper

In brief

“Atomic Layer Deposition of WS2 Using Organic Precursors” is a 2025 journal article by Hiroshi Yokota and 8 co-authors, published in ECS Meeting Abstracts. OpenAlex counts 0 citations as of 17 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
0
Authors
9

Abstract

Background and Objective Tungsten disulfide (WS2) is a representative two-dimensional layered transition metal dichalcogenide material that has attracted attention as a next-generation semiconductor device material due to its high carrier mobility and the tunable band gap by the number of layers. In particular, WS2 with a few layers or less is a promising channel material… Read the full abstract at the publisher.

Excerpt. This paper is not open access.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Yokota, H., Higashi, S., Machida, H., Ishikawa, M., Sudoh, H., Wakabayashi, H., Sawamoto, N., Yokogawa, R., & Ogura, A. (2025). Atomic Layer Deposition of WS2 Using Organic Precursors. ECS Meeting Abstracts, MA2025-01(31), 1599. https://doi.org/10.1149/ma2025-01311599mtgabs

MLA 9

Yokota, Hiroshi, et al. “Atomic Layer Deposition of WS2 Using Organic Precursors.” ECS Meeting Abstracts, vol. MA2025-01, no. 31, 2025, p. 1599. https://doi.org/10.1149/ma2025-01311599mtgabs.

Chicago

Yokota, Hiroshi, Sota Higashi, Hideaki Machida, Masato Ishikawa, Hiroshi Sudoh, Hitoshi Wakabayashi, Naomi Sawamoto, Ryo Yokogawa, and Atsushi Ogura. 2025. “Atomic Layer Deposition of WS2 Using Organic Precursors.” ECS Meeting Abstracts MA2025-01 (31): 1599. https://doi.org/10.1149/ma2025-01311599mtgabs.

Harvard

Yokota, H. et al. (2025) ‘Atomic Layer Deposition of WS2 Using Organic Precursors’, ECS Meeting Abstracts, MA2025-01(31), p. 1599. doi:10.1149/ma2025-01311599mtgabs.

IEEE

H. Yokota et al., “Atomic Layer Deposition of WS2 Using Organic Precursors,” ECS Meeting Abstracts, vol. MA2025-01, no. 31, p. 1599, 2025, doi: 10.1149/ma2025-01311599mtgabs.

BibTeX

@article{yokota2025atomic,
  title     = {{Atomic Layer Deposition of WS2 Using Organic Precursors}},
  author    = {Yokota, Hiroshi and Higashi, Sota and Machida, Hideaki and Ishikawa, Masato and Sudoh, Hiroshi and Wakabayashi, Hitoshi and Sawamoto, Naomi and Yokogawa, Ryo and Ogura, Atsushi},
  journal   = {ECS Meeting Abstracts},
  year      = {2025},
  volume    = {MA2025-01},
  number    = {31},
  pages     = {1599},
  doi       = {10.1149/ma2025-01311599mtgabs},
  url       = {https://doi.org/10.1149/ma2025-01311599mtgabs}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Topic and keywords

Physical Sciences › Materials Science › Materials Chemistry › 2D Materials and Applications

  • WS2 thin films
  • atomic layer deposition
  • organic precursors
  • 2H-WS2
  • low-temperature deposition
  • film uniformity
  • number of layers
  • Raman spectroscopy

Work with this paper

Most-cited papers in Materials Science

All highly cited Materials Science papers

Questions about this paper

How do I cite this paper in APA style?

Yokota, H., Higashi, S., Machida, H., Ishikawa, M., Sudoh, H., Wakabayashi, H., Sawamoto, N., Yokogawa, R., & Ogura, A. (2025). Atomic Layer Deposition of WS2 Using Organic Precursors. ECS Meeting Abstracts, MA2025-01(31), 1599. https://doi.org/10.1149/ma2025-01311599mtgabs

How many times has this paper been cited?

0 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Hiroshi Yokota, Sota Higashi, Hideaki Machida, Masato Ishikawa, Hiroshi Sudoh, Hitoshi Wakabayashi, Naomi Sawamoto, Ryo Yokogawa, Atsushi Ogura.

What is the DOI of this paper?

10.1149/ma2025-01311599mtgabs, permanently at https://doi.org/10.1149/ma2025-01311599mtgabs. Sign in and open it from this page.

Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.