Journal article · 2018 · Open access

Influence of welding procedure and PWHT on HSLA steel weld metals

Jorge Carlos Ferreira Jorge, Joel Lemos Dias Monteiro, Antonio José de Carvalho Gomes, Ivaní de Souza Bott, Luís Felipe Guimarães de Souza, Matheus Campolina Mendes, Leonardo Sales Araújo

Journal of Materials Research and Technology, 8(1), 561–571 · Published 19 June 2018 · DOI 10.1016/j.jmrt.2018.05.007

Open PDFView at the publisherCite this paper

In brief

“Influence of welding procedure and PWHT on HSLA steel weld metals” is a 2018 journal article by Jorge Carlos Ferreira Jorge and 6 co-authors, published in Journal of Materials Research and Technology. OpenAlex counts 73 citations as of 22 November 2026, which puts it in the top 3% of works published in 2018 by citations. It is open access under a CC BY-NC-ND licence: the full text is free to read at Journal of Materials Research and Technology.

Citations
73
Most cited in
2023 (15)
Field-weighted impact
2.87
References
55
Authors
7

Abstract

The development of consumables for welding of high strength steels represents a continuous challenge taking into account the great variety of alloy systems. In this regard, there are many applications, such as offshore structures, where the welding is still preferably done by the SMAW process. In order to evaluate the properties of weld metals obtained by other processes with higher productivity, the present work presents a comparative analysis between the mechanical properties of high strength steel weld metals obtained by shielded metal arc (SMAW) and gas metal arc (GMAW) welding processes. Multipass welding by SMAW and GMAW processes was performed with preheating of 200 °C, in 750 × 150 × 19 mm plates. After welding, a post weld heat treatment (PWHT) at 600 °C for 1 h was performed and this condition was compared to the as welded one. Mechanical tests and metallographic examination by optical microscopy (OM), scanning electron microscopy (SEM) and electron backscattered diffraction (EBSD) were performed for mechanical and microstructural characterization. Thermodynamic calculations were also performed by using Thermo-Calc software, in order to evaluate the occurrence of carbides as a consequence of the PWHT. Although presenting impact toughness behavior slightly different due to the chemical composition and carbide precipitates, as predicted by computational simulation, both processes showed a good relationship between mechanical strength and impact toughness for all analyzed conditions, even after PWHT. Based on this scenario, it can be inferred that GMAW process can be applied as an interesting alternative for welding of high strength steels, once this process promotes a significant improvement in productivity with good quality.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Jorge, J. C. F., Monteiro, J. L. D., Gomes, A. J. D. C., Bott, I. D. S., de Souza, L. F. G., Mendes, M. C., & Araújo, L. S. (2018). Influence of welding procedure and PWHT on HSLA steel weld metals. Journal of Materials Research and Technology, 8(1), 561–571. https://doi.org/10.1016/j.jmrt.2018.05.007

MLA 9

Jorge, Jorge Carlos Ferreira, et al. “Influence of welding procedure and PWHT on HSLA steel weld metals.” Journal of Materials Research and Technology, vol. 8, no. 1, 2018, pp. 561–571. https://doi.org/10.1016/j.jmrt.2018.05.007.

Chicago

Jorge, Jorge Carlos Ferreira, Joel Lemos Dias Monteiro, Antonio José de Carvalho Gomes, Ivaní de Souza Bott, Luís Felipe Guimarães de Souza, Matheus Campolina Mendes, and Leonardo Sales Araújo. 2018. “Influence of welding procedure and PWHT on HSLA steel weld metals.” Journal of Materials Research and Technology 8 (1): 561–571. https://doi.org/10.1016/j.jmrt.2018.05.007.

Harvard

Jorge, J. C. F. et al. (2018) ‘Influence of welding procedure and PWHT on HSLA steel weld metals’, Journal of Materials Research and Technology, 8(1), pp. 561–571. doi:10.1016/j.jmrt.2018.05.007.

IEEE

J. C. F. Jorge et al., “Influence of welding procedure and PWHT on HSLA steel weld metals,” Journal of Materials Research and Technology, vol. 8, no. 1, pp. 561–571, 2018, doi: 10.1016/j.jmrt.2018.05.007.

BibTeX

@article{jorge2018influence,
  title     = {{Influence of welding procedure and PWHT on HSLA steel weld metals}},
  author    = {Jorge, Jorge Carlos Ferreira and Monteiro, Joel Lemos Dias and Gomes, Antonio José de Carvalho and Bott, Ivaní de Souza and de Souza, Luís Felipe Guimarães and Mendes, Matheus Campolina and Araújo, Leonardo Sales},
  journal   = {Journal of Materials Research and Technology},
  year      = {2018},
  volume    = {8},
  number    = {1},
  pages     = {561--571},
  doi       = {10.1016/j.jmrt.2018.05.007},
  url       = {https://doi.org/10.1016/j.jmrt.2018.05.007}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
201955
202066
202188
20221010
20231515
20241313
202588
202688

Its field-weighted citation impact is 2.87: it has been cited 2.87 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Engineering › Mechanical Engineering › Welding Techniques and Residual Stresses

  • high-strength low-alloy steel
  • weld metal
  • post-weld heat treatment
  • shielded metal arc welding
  • gas metal arc welding
  • multi-pass welding
  • carbide precipitation
  • impact toughness

Work with this paper

Most-cited papers in Engineering

All highly cited Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Jorge, J. C. F., Monteiro, J. L. D., Gomes, A. J. D. C., Bott, I. D. S., de Souza, L. F. G., Mendes, M. C., & Araújo, L. S. (2018). Influence of welding procedure and PWHT on HSLA steel weld metals. Journal of Materials Research and Technology, 8(1), 561–571. https://doi.org/10.1016/j.jmrt.2018.05.007

How many times has this paper been cited?

73 times, according to OpenAlex on 22 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

Yes. It is open access at Journal of Materials Research and Technology: sign in and open the PDF from this page.

Who wrote this paper?

Jorge Carlos Ferreira Jorge, Joel Lemos Dias Monteiro, Antonio José de Carvalho Gomes, Ivaní de Souza Bott, Luís Felipe Guimarães de Souza, Matheus Campolina Mendes, Leonardo Sales Araújo.

What is the DOI of this paper?

10.1016/j.jmrt.2018.05.007, permanently at https://doi.org/10.1016/j.jmrt.2018.05.007. Sign in and open it from this page.

Bibliographic data from OpenAlex (CC0), last checked 22 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.