In Situ Nanoindentation and Scratch Testing Inside Scanning Electron Microscopes: Opportunities and Challenges

Hu Huang, Hongwei Zhao

Science of Advanced Materials, 6(5), 875–889 · Published 1 May 2014 · DOI 10.1166/sam.2014.1868

View at the publisherCite this paper

In brief

“In Situ Nanoindentation and Scratch Testing Inside Scanning Electron Microscopes: Opportunities and Challenges” is a 2014 journal article by Hu Huang and Hongwei Zhao, published in Science of Advanced Materials. OpenAlex counts 15 citations as of 16 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
15
Most cited in
2017 (3)
Field-weighted impact
1.39
Authors
2

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Huang, H., & Zhao, H. (2014). In Situ Nanoindentation and Scratch Testing Inside Scanning Electron Microscopes: Opportunities and Challenges. Science of Advanced Materials, 6(5), 875–889. https://doi.org/10.1166/sam.2014.1868

MLA 9

Huang, Hu, and Hongwei Zhao. “In Situ Nanoindentation and Scratch Testing Inside Scanning Electron Microscopes: Opportunities and Challenges.” Science of Advanced Materials, vol. 6, no. 5, 2014, pp. 875–889. https://doi.org/10.1166/sam.2014.1868.

Chicago

Huang, Hu and Hongwei Zhao. 2014. “In Situ Nanoindentation and Scratch Testing Inside Scanning Electron Microscopes: Opportunities and Challenges.” Science of Advanced Materials 6 (5): 875–889. https://doi.org/10.1166/sam.2014.1868.

Harvard

Huang, H. and Zhao, H. (2014) ‘In Situ Nanoindentation and Scratch Testing Inside Scanning Electron Microscopes: Opportunities and Challenges’, Science of Advanced Materials, 6(5), pp. 875–889. doi:10.1166/sam.2014.1868.

IEEE

H. Huang and H. Zhao, “In Situ Nanoindentation and Scratch Testing Inside Scanning Electron Microscopes: Opportunities and Challenges,” Science of Advanced Materials, vol. 6, no. 5, pp. 875–889, 2014, doi: 10.1166/sam.2014.1868.

BibTeX

@article{huang2014situ,
  title     = {{In Situ Nanoindentation and Scratch Testing Inside Scanning Electron Microscopes: Opportunities and Challenges}},
  author    = {Huang, Hu and Zhao, Hongwei},
  journal   = {Science of Advanced Materials},
  year      = {2014},
  volume    = {6},
  number    = {5},
  pages     = {875--889},
  doi       = {10.1166/sam.2014.1868},
  url       = {https://doi.org/10.1166/sam.2014.1868}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
201511
201611
201733
202011
202122
202322
202411
202522
202622

Its field-weighted citation impact is 1.39: it has been cited 1.39 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics

  • in situ nanoindentation
  • scratch test
  • scanning electron microscopy
  • mechanical testing
  • mechanical properties

Work with this paper

Most-cited papers in Engineering

All highly cited Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Huang, H., & Zhao, H. (2014). In Situ Nanoindentation and Scratch Testing Inside Scanning Electron Microscopes: Opportunities and Challenges. Science of Advanced Materials, 6(5), 875–889. https://doi.org/10.1166/sam.2014.1868

How many times has this paper been cited?

15 times, according to OpenAlex on 16 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Hu Huang, Hongwei Zhao.

What is the DOI of this paper?

10.1166/sam.2014.1868. The permanent link is https://doi.org/10.1166/sam.2014.1868.

Bibliographic data from OpenAlex (CC0), last checked 16 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.