Journal article · 2007 · Open access
In situ nanoindentation in the TEM
Materials Today, 10(4), 59–60 · Published 1 April 2007 · DOI 10.1016/s1369-7021(07)70051-2
In brief
“In situ nanoindentation in the TEM” is a 2007 journal article by Oden L. Warren and 5 co-authors, published in Materials Today. OpenAlex counts 60 citations as of 16 November 2026. It is open access under a CC BY-NC-ND licence: the full text is free to read at Materials Today.
- Citations
- 60
- Most cited in
- 2016 (9)
- Field-weighted impact
- 5.99
- References
- 12
- Authors
- 6
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Warren, O. L., Shan, Z., Asif, S. A. S., Stach, E. A., Jr., J. W. M., & Minor, A. M. (2007). In situ nanoindentation in the TEM. Materials Today, 10(4), 59–60. https://doi.org/10.1016/s1369-7021(07)70051-2
MLA 9
Warren, Oden L., et al. “In situ nanoindentation in the TEM.” Materials Today, vol. 10, no. 4, 2007, pp. 59–60. https://doi.org/10.1016/s1369-7021(07)70051-2.
Chicago
Warren, Oden L., Zhiwei Shan, S. A. Syed Asif, Eric A. Stach, John William Morris Jr., and Andrew M. Minor. 2007. “In situ nanoindentation in the TEM.” Materials Today 10 (4): 59–60. https://doi.org/10.1016/s1369-7021(07)70051-2.
Harvard
Warren, O. L. et al. (2007) ‘In situ nanoindentation in the TEM’, Materials Today, 10(4), pp. 59–60. doi:10.1016/s1369-7021(07)70051-2.
IEEE
O. L. Warren, Z. Shan, S. A. S. Asif, E. A. Stach, J. W. M. Jr., and A. M. Minor, “In situ nanoindentation in the TEM,” Materials Today, vol. 10, no. 4, pp. 59–60, 2007, doi: 10.1016/s1369-7021(07)70051-2.
BibTeX
@article{warren2007situ,
title = {{In situ nanoindentation in the TEM}},
author = {Warren, Oden L. and Shan, Zhiwei and Asif, S. A. Syed and Stach, Eric A. and Jr., John William Morris and Minor, Andrew M.},
journal = {Materials Today},
year = {2007},
volume = {10},
number = {4},
pages = {59--60},
doi = {10.1016/s1369-7021(07)70051-2},
url = {https://doi.org/10.1016/s1369-7021(07)70051-2}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2015 | 4 | |
| 2016 | 9 | |
| 2017 | 6 | |
| 2018 | 1 | |
| 2019 | 3 | |
| 2021 | 3 | |
| 2022 | 1 | |
| 2023 | 1 | |
| 2024 | 1 | |
| 2025 | 2 |
Its field-weighted citation impact is 5.99: it has been cited 5.99 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics
- in situ nanoindentation
- transmission electron microscopy
- nanoindentation
- mechanical properties
- microhardness
Work with this paper
Most-cited papers in Engineering
- A Closed‐form Equation for Predicting the Hydraulic Conductivity of Unsaturated SoilsMartinus Th. van Genuchten · Soil Science Society of America Journal · 1980 · 28,197 citations
- An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experimentsW. C. Oliver, George M. Pharr · Journal of materials research/Pratt's guide to venture capital sources · 1992 · 27,379 citations
- Digital communicationsOwen Bishop · Routledge eBooks · 2007 · 24,890 citations
- The empirical mode decomposition and the Hilbert spectrum for nonlinear and non-stationary time series analysisNorden Eh Huang, Zhengwei Shen, Steven R. Long and 6 more · Proceedings of the Royal Society A Mathematical Physical and Engineering Sciences · 1998 · 24,008 citations
- Numerical Heat Transfer and Fluid FlowSuhas V. Patankar · CRC Press eBooks · 2018 · 23,491 citations
Questions about this paper
How do I cite this paper in APA style?
Warren, O. L., Shan, Z., Asif, S. A. S., Stach, E. A., Jr., J. W. M., & Minor, A. M. (2007). In situ nanoindentation in the TEM. Materials Today, 10(4), 59–60. https://doi.org/10.1016/s1369-7021(07)70051-2
How many times has this paper been cited?
60 times, according to OpenAlex on 16 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access: read the free full text at Materials Today.
Who wrote this paper?
Oden L. Warren, Zhiwei Shan, S. A. Syed Asif, Eric A. Stach, John William Morris Jr., Andrew M. Minor.
What is the DOI of this paper?
10.1016/s1369-7021(07)70051-2. The permanent link is https://doi.org/10.1016/s1369-7021(07)70051-2.
Bibliographic data from OpenAlex (CC0), last checked 16 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.