In brief
“Combination of Instrumented Nanoindentation and Scanning Probe Microscopy for Adequate Mechanical Surface Testing” is a 2009 paper by Enrico Enrico and 7 co-authors, published in Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles). OpenAlex counts 8 citations as of 16 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.
- Citations
- 8
- Most cited in
- 2013 (3)
- Field-weighted impact
- 0.42
- Authors
- 8
Abstract
The elastic indentation modulus and hardness of standard bulk materials and advanced thin films were determined by using the nanoindentation technique followed by the OliverPharr post-treatment. After measurements with different loading/unloading schemes on chemically polished bulk titanium a substantial decrease of both modulus and hardness vs an increasing loading time was found. Then, hard nanostructured… Read the full abstract at the publisher.
Excerpt. This paper is not open access.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Enrico, E., Иванович, П. М., Mikhail, Petrzhik, Dmitry, Shtansky, Marie-Paule, & Delplancke-Ogletree. (2009). Combination of Instrumented Nanoindentation and Scanning Probe Microscopy for Adequate Mechanical Surface Testing. Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles), 25(01), 63–68. http://hdl.handle.net/2013/ULB-DIPOT:oai:dipot.ulb.ac.be:2013/68244
MLA 9
Enrico, Enrico, et al. “Combination of Instrumented Nanoindentation and Scanning Probe Microscopy for Adequate Mechanical Surface Testing.” Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles), vol. 25, no. 01, 2009, pp. 63–68. http://hdl.handle.net/2013/ULB-DIPOT:oai:dipot.ulb.ac.be:2013/68244.
Chicago
Enrico, Enrico, Петржик Михаил Иванович, Mikhail, Petrzhik, Dmitry, Shtansky, Marie-Paule, and Delplancke-Ogletree. 2009. “Combination of Instrumented Nanoindentation and Scanning Probe Microscopy for Adequate Mechanical Surface Testing.” Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles) 25 (01): 63–68. http://hdl.handle.net/2013/ULB-DIPOT:oai:dipot.ulb.ac.be:2013/68244.
Harvard
Enrico, E. et al. (2009) ‘Combination of Instrumented Nanoindentation and Scanning Probe Microscopy for Adequate Mechanical Surface Testing’, Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles), 25(01), pp. 63–68. Available at: http://hdl.handle.net/2013/ULB-DIPOT:oai:dipot.ulb.ac.be:2013/68244.
IEEE
E. Enrico et al., “Combination of Instrumented Nanoindentation and Scanning Probe Microscopy for Adequate Mechanical Surface Testing,” Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles), vol. 25, no. 01, pp. 63–68, 2009.
BibTeX
@article{enrico2009combination,
title = {{Combination of Instrumented Nanoindentation and Scanning Probe Microscopy for Adequate Mechanical Surface Testing}},
author = {Enrico, Enrico and Иванович, Петржик Михаил and Mikhail and Petrzhik and Dmitry and Shtansky and Marie-Paule and Delplancke-Ogletree},
journal = {Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles)},
year = {2009},
volume = {25},
number = {01},
pages = {63--68},
url = {http://hdl.handle.net/2013/ULB-DIPOT:oai:dipot.ulb.ac.be:2013/68244}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2012 | 1 | |
| 2013 | 3 | |
| 2014 | 1 | |
| 2016 | 1 | |
| 2018 | 1 | |
| 2020 | 1 |
Its field-weighted citation impact is 0.42: it has been cited 0.42 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics
- nanoindentation
- scanning probe microscopy
- hardness
- thin films
- titanium nitride
- surface roughness
- loading time
- normal distribution
Work with this paper
Most-cited papers in Engineering
- A Closed‐form Equation for Predicting the Hydraulic Conductivity of Unsaturated SoilsMartinus Th. van Genuchten · Soil Science Society of America Journal · 1980 · 28,197 citations
- An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experimentsW. C. Oliver, George M. Pharr · Journal of materials research/Pratt's guide to venture capital sources · 1992 · 27,379 citations
- Digital communicationsOwen Bishop · Routledge eBooks · 2007 · 24,890 citations
- The empirical mode decomposition and the Hilbert spectrum for nonlinear and non-stationary time series analysisNorden Eh Huang, Zhengwei Shen, Steven R. Long and 6 more · Proceedings of the Royal Society A Mathematical Physical and Engineering Sciences · 1998 · 24,008 citations
- Numerical Heat Transfer and Fluid FlowSuhas V. Patankar · CRC Press eBooks · 2018 · 23,491 citations
Questions about this paper
How do I cite this paper in APA style?
Enrico, E., Иванович, П. М., Mikhail, Petrzhik, Dmitry, Shtansky, Marie-Paule, & Delplancke-Ogletree. (2009). Combination of Instrumented Nanoindentation and Scanning Probe Microscopy for Adequate Mechanical Surface Testing. Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles), 25(01), 63–68. http://hdl.handle.net/2013/ULB-DIPOT:oai:dipot.ulb.ac.be:2013/68244
How many times has this paper been cited?
8 times, according to OpenAlex on 16 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.
Who wrote this paper?
Enrico Enrico, Петржик Михаил Иванович, Mikhail, Petrzhik, Dmitry, Shtansky, Marie-Paule, Delplancke-Ogletree.
Bibliographic data from OpenAlex (CC0), last checked 16 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.