Nanoindentation: considerations on the area function calibration
Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles) · Published 1 January 2009
In brief
“Nanoindentation: considerations on the area function calibration” is a 2009 paper by Péter Nagy and Marie‐Paule Delplancke, published in Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles). OpenAlex counts 0 citations as of 16 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.
- Citations
- 0
- Authors
- 2
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Nagy, P., & Delplancke, M. (2009). Nanoindentation: considerations on the area function calibration. Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles). http://hdl.handle.net/2013/ULB-DIPOT:oai:dipot.ulb.ac.be:2013/71050
MLA 9
Nagy, Péter, and Marie‐Paule Delplancke. “Nanoindentation: considerations on the area function calibration.” Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles), 2009. http://hdl.handle.net/2013/ULB-DIPOT:oai:dipot.ulb.ac.be:2013/71050.
Chicago
Nagy, Péter and Marie‐Paule Delplancke. 2009. “Nanoindentation: considerations on the area function calibration.” Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles). http://hdl.handle.net/2013/ULB-DIPOT:oai:dipot.ulb.ac.be:2013/71050.
Harvard
Nagy, P. and Delplancke, M. (2009) ‘Nanoindentation: considerations on the area function calibration’, Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles). Available at: http://hdl.handle.net/2013/ULB-DIPOT:oai:dipot.ulb.ac.be:2013/71050.
IEEE
P. Nagy and M. Delplancke, “Nanoindentation: considerations on the area function calibration,” Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles), 2009.
BibTeX
@article{nagy2009nanoindentation,
title = {{Nanoindentation: considerations on the area function calibration}},
author = {Nagy, Péter and Delplancke, Marie‐Paule},
journal = {Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles)},
year = {2009},
url = {http://hdl.handle.net/2013/ULB-DIPOT:oai:dipot.ulb.ac.be:2013/71050}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Topic and keywords
Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics
- nanoindentation
- contact area
- mechanical properties
Work with this paper
Most-cited papers in Engineering
- A Closed‐form Equation for Predicting the Hydraulic Conductivity of Unsaturated SoilsMartinus Th. van Genuchten · Soil Science Society of America Journal · 1980 · 28,197 citations
- An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experimentsW. C. Oliver, George M. Pharr · Journal of materials research/Pratt's guide to venture capital sources · 1992 · 27,379 citations
- Digital communicationsOwen Bishop · Routledge eBooks · 2007 · 24,890 citations
- The empirical mode decomposition and the Hilbert spectrum for nonlinear and non-stationary time series analysisNorden Eh Huang, Zhengwei Shen, Steven R. Long and 6 more · Proceedings of the Royal Society A Mathematical Physical and Engineering Sciences · 1998 · 24,008 citations
- Numerical Heat Transfer and Fluid FlowSuhas V. Patankar · CRC Press eBooks · 2018 · 23,491 citations
Questions about this paper
How do I cite this paper in APA style?
Nagy, P., & Delplancke, M. (2009). Nanoindentation: considerations on the area function calibration. Dépôt institutionnel de l'Université libre de Bruxelles (Université Libre de Bruxelles). http://hdl.handle.net/2013/ULB-DIPOT:oai:dipot.ulb.ac.be:2013/71050
How many times has this paper been cited?
0 times, according to OpenAlex on 16 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.
Who wrote this paper?
Péter Nagy, Marie‐Paule Delplancke.
Bibliographic data from OpenAlex (CC0), last checked 16 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.