THE EFFECT OF RESIDUAL STRESSES ON NANOINDENTATION BEHAVIOR OF THIN W-C BASED COATINGS

Michal Novák, František Lofaj

Published 1 January 2013

View at the publisherCite this paper

In brief

“THE EFFECT OF RESIDUAL STRESSES ON NANOINDENTATION BEHAVIOR OF THIN W-C BASED COATINGS” is a 2013 paper by Michal Novák and František Lofaj. OpenAlex counts 6 citations as of 17 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
6
Most cited in
2017 (2)
Field-weighted impact
0.31
References
2
Authors
2

Abstract

The work investigates the effect of compressive residual stresses generated in thin W-C based coatings during DC magnetron deposition process on nanohardness (HIT) and indentation modulus (EIT). It was discovered that the hardness values increase approximately linearly from 16.5 to 19.5 GPa with an increase of the compressive residual stresses from 1.5 to 4.5 GPa.… Read the full abstract at the publisher.

Excerpt. This paper is not open access.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Novák, M., & Lofaj, F. (2013). THE EFFECT OF RESIDUAL STRESSES ON NANOINDENTATION BEHAVIOR OF THIN W-C BASED COATINGS. http://www.imr.saske.sk/pmp/issue/3-4-2013/PMP_Vol13_No3-4_p_132-138.pdf

MLA 9

Novák, Michal, and František Lofaj. “THE EFFECT OF RESIDUAL STRESSES ON NANOINDENTATION BEHAVIOR OF THIN W-C BASED COATINGS.” 2013. http://www.imr.saske.sk/pmp/issue/3-4-2013/PMP_Vol13_No3-4_p_132-138.pdf.

Chicago

Novák, Michal and František Lofaj. 2013. “THE EFFECT OF RESIDUAL STRESSES ON NANOINDENTATION BEHAVIOR OF THIN W-C BASED COATINGS.” http://www.imr.saske.sk/pmp/issue/3-4-2013/PMP_Vol13_No3-4_p_132-138.pdf.

Harvard

Novák, M. and Lofaj, F. (2013) ‘THE EFFECT OF RESIDUAL STRESSES ON NANOINDENTATION BEHAVIOR OF THIN W-C BASED COATINGS’. Available at: http://www.imr.saske.sk/pmp/issue/3-4-2013/PMP_Vol13_No3-4_p_132-138.pdf.

IEEE

M. Novák and F. Lofaj, “THE EFFECT OF RESIDUAL STRESSES ON NANOINDENTATION BEHAVIOR OF THIN W-C BASED COATINGS,” 2013.

BibTeX

@article{novak2013effect,
  title     = {{THE EFFECT OF RESIDUAL STRESSES ON NANOINDENTATION BEHAVIOR OF THIN W-C BASED COATINGS}},
  author    = {Novák, Michal and Lofaj, František},
  year      = {2013},
  url       = {http://www.imr.saske.sk/pmp/issue/3-4-2013/PMP_Vol13_No3-4_p_132-138.pdf}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
201511
201722
201822
202311

Its field-weighted citation impact is 0.31: it has been cited 0.31 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics

  • residual stress
  • tungsten carbide coatings
  • thin film coatings
  • nanohardness
  • indentation modulus
  • DC magnetron sputtering
  • thermal stress
  • coating thickness

Work with this paper

Most-cited papers in Engineering

All highly cited Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Novák, M., & Lofaj, F. (2013). THE EFFECT OF RESIDUAL STRESSES ON NANOINDENTATION BEHAVIOR OF THIN W-C BASED COATINGS. http://www.imr.saske.sk/pmp/issue/3-4-2013/PMP_Vol13_No3-4_p_132-138.pdf

How many times has this paper been cited?

6 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Michal Novák, František Lofaj.

Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.