Journal article · 2020

Atomic layer deposition of tungsten sulfide using a new metal-organic precursor and H 2 S: thin film catalyst for water splitting

Deok-Hyun Kim, Rahul Ramesh, Dip K. Nandi, Jong‐Seong Bae, Soo‐Hyun Kim

Nanotechnology, 32(7), 075405 · Published 27 October 2020 · DOI 10.1088/1361-6528/abc50b

View at the publisherCite this paper

In brief

“Atomic layer deposition of tungsten sulfide using a new metal-organic precursor and H 2 S: thin film catalyst for water splitting” is a 2020 journal article by Deok-Hyun Kim and 4 co-authors, published in Nanotechnology. OpenAlex counts 14 citations as of 17 November 2026, which puts it in the top 9% of works published in 2020 by citations. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
14
Most cited in
2025 (4)
Field-weighted impact
0.65
References
58
Authors
5

Abstract

Transition metal dichalcogenides (TMDs) are extensively researched in the past few years due to their two-dimensional layered structure similar to graphite. This group of materials offers tunable optoelectronic properties depending on the number of layers and therefore have a wide range of applications. Tungsten disulfide (WS 2 ) is one of such TMDs that has… Read the full abstract at the publisher.

Excerpt. This paper is not open access.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Kim, D.-H., Ramesh, R., Nandi, D. K., Bae, J., & Kim, S. (2020). Atomic layer deposition of tungsten sulfide using a new metal-organic precursor and H 2 S: thin film catalyst for water splitting. Nanotechnology, 32(7), 075405. https://doi.org/10.1088/1361-6528/abc50b

MLA 9

Kim, Deok-Hyun, et al. “Atomic layer deposition of tungsten sulfide using a new metal-organic precursor and H 2 S: thin film catalyst for water splitting.” Nanotechnology, vol. 32, no. 7, 2020, p. 075405. https://doi.org/10.1088/1361-6528/abc50b.

Chicago

Kim, Deok-Hyun, Rahul Ramesh, Dip K. Nandi, Jong‐Seong Bae, and Soo‐Hyun Kim. 2020. “Atomic layer deposition of tungsten sulfide using a new metal-organic precursor and H 2 S: thin film catalyst for water splitting.” Nanotechnology 32 (7): 075405. https://doi.org/10.1088/1361-6528/abc50b.

Harvard

Kim, D.-H. et al. (2020) ‘Atomic layer deposition of tungsten sulfide using a new metal-organic precursor and H 2 S: thin film catalyst for water splitting’, Nanotechnology, 32(7), p. 075405. doi:10.1088/1361-6528/abc50b.

IEEE

D.-H. Kim, R. Ramesh, D. K. Nandi, J. Bae, and S. Kim, “Atomic layer deposition of tungsten sulfide using a new metal-organic precursor and H 2 S: thin film catalyst for water splitting,” Nanotechnology, vol. 32, no. 7, p. 075405, 2020, doi: 10.1088/1361-6528/abc50b.

BibTeX

@article{kim2020atomic,
  title     = {{Atomic layer deposition of tungsten sulfide using a new metal-organic precursor and H 2 S: thin film catalyst for water splitting}},
  author    = {Kim, Deok-Hyun and Ramesh, Rahul and Nandi, Dip K. and Bae, Jong‐Seong and Kim, Soo‐Hyun},
  journal   = {Nanotechnology},
  year      = {2020},
  volume    = {32},
  number    = {7},
  pages     = {075405},
  doi       = {10.1088/1361-6528/abc50b},
  url       = {https://doi.org/10.1088/1361-6528/abc50b}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
202122
202222
202333
202422
202544
202611

Its field-weighted citation impact is 0.65: it has been cited 0.65 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Materials Science › Materials Chemistry › 2D Materials and Applications

  • tungsten disulfide
  • transition metal dichalcogenides
  • atomic layer deposition
  • metal-organic precursors
  • hydrogen sulfide
  • post-annealing
  • sulfur deficiency
  • hydrogen evolution reaction

Work with this paper

Most-cited papers in Materials Science

All highly cited Materials Science papers

Questions about this paper

How do I cite this paper in APA style?

Kim, D.-H., Ramesh, R., Nandi, D. K., Bae, J., & Kim, S. (2020). Atomic layer deposition of tungsten sulfide using a new metal-organic precursor and H 2 S: thin film catalyst for water splitting. Nanotechnology, 32(7), 075405. https://doi.org/10.1088/1361-6528/abc50b

How many times has this paper been cited?

14 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Deok-Hyun Kim, Rahul Ramesh, Dip K. Nandi, Jong‐Seong Bae, Soo‐Hyun Kim.

What is the DOI of this paper?

10.1088/1361-6528/abc50b, permanently at https://doi.org/10.1088/1361-6528/abc50b. Sign in and open it from this page.

Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.