Journal article · 2021

Wafer-Scale Growth of a MoS2 Monolayer via One Cycle of Atomic Layer Deposition: An Adsorbate Control Method

Dae‐Hyun Kim, Jae Chan Park, Jeongwoo Park, Deok‐Yong Cho, Woo‐Hee Kim, Bonggeun Shong, Ji‐Hoon Ahn, Tae Joo Park

Chemistry of Materials, 33(11), 4099–4105 · Published 27 May 2021 · DOI 10.1021/acs.chemmater.1c00729

View at the publisherCite this paper

In brief

“Wafer-Scale Growth of a MoS2 Monolayer via One Cycle of Atomic Layer Deposition: An Adsorbate Control Method” is a 2021 journal article by Dae‐Hyun Kim and 7 co-authors, published in Chemistry of Materials. OpenAlex counts 47 citations as of 24 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
47
Most cited in
2023 (17)
Field-weighted impact
2.04
References
42
Authors
8

Abstract

Monolayer transition metal dichalcogenide compounds with two-dimensional (2D) layered structures may be used as next-generation active materials for electronic and optoelectronic devices. A reliable method for creating high-quality, wafer-scale material with well-controlled large-area growth is required for industrial applications. Two-dimensional material atomic layer deposition (ALD) can be used as an atomically flat monolayer film, but… Read the full abstract at the publisher.

Excerpt. This paper is not open access.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Kim, D., Park, J. C., Park, J., Cho, D., Kim, W., Shong, B., Ahn, J., & Park, T. J. (2021). Wafer-Scale Growth of a MoS2 Monolayer via One Cycle of Atomic Layer Deposition: An Adsorbate Control Method. Chemistry of Materials, 33(11), 4099–4105. https://doi.org/10.1021/acs.chemmater.1c00729

MLA 9

Kim, Dae‐Hyun, et al. “Wafer-Scale Growth of a MoS2 Monolayer via One Cycle of Atomic Layer Deposition: An Adsorbate Control Method.” Chemistry of Materials, vol. 33, no. 11, 2021, pp. 4099–4105. https://doi.org/10.1021/acs.chemmater.1c00729.

Chicago

Kim, Dae‐Hyun, Jae Chan Park, Jeongwoo Park, Deok‐Yong Cho, Woo‐Hee Kim, Bonggeun Shong, Ji‐Hoon Ahn, and Tae Joo Park. 2021. “Wafer-Scale Growth of a MoS2 Monolayer via One Cycle of Atomic Layer Deposition: An Adsorbate Control Method.” Chemistry of Materials 33 (11): 4099–4105. https://doi.org/10.1021/acs.chemmater.1c00729.

Harvard

Kim, D. et al. (2021) ‘Wafer-Scale Growth of a MoS2 Monolayer via One Cycle of Atomic Layer Deposition: An Adsorbate Control Method’, Chemistry of Materials, 33(11), pp. 4099–4105. doi:10.1021/acs.chemmater.1c00729.

IEEE

D. Kim et al., “Wafer-Scale Growth of a MoS2 Monolayer via One Cycle of Atomic Layer Deposition: An Adsorbate Control Method,” Chemistry of Materials, vol. 33, no. 11, pp. 4099–4105, 2021, doi: 10.1021/acs.chemmater.1c00729.

BibTeX

@article{kim2021wafer,
  title     = {{Wafer-Scale Growth of a MoS2 Monolayer via One Cycle of Atomic Layer Deposition: An Adsorbate Control Method}},
  author    = {Kim, Dae‐Hyun and Park, Jae Chan and Park, Jeongwoo and Cho, Deok‐Yong and Kim, Woo‐Hee and Shong, Bonggeun and Ahn, Ji‐Hoon and Park, Tae Joo},
  journal   = {Chemistry of Materials},
  year      = {2021},
  volume    = {33},
  number    = {11},
  pages     = {4099--4105},
  doi       = {10.1021/acs.chemmater.1c00729},
  url       = {https://doi.org/10.1021/acs.chemmater.1c00729}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
202111
202233
20231717
20241010
202588
202688

Its field-weighted citation impact is 2.04: it has been cited 2.04 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Materials Science › Materials Chemistry › 2D Materials and Applications

  • monolayer MoS2
  • atomic layer deposition
  • wafer-scale growth
  • two-dimensional materials
  • transition metal dichalcogenides
  • luminescence quantum efficiency
  • film uniformity

Work with this paper

Most-cited papers in Materials Science

All highly cited Materials Science papers

Questions about this paper

How do I cite this paper in APA style?

Kim, D., Park, J. C., Park, J., Cho, D., Kim, W., Shong, B., Ahn, J., & Park, T. J. (2021). Wafer-Scale Growth of a MoS2 Monolayer via One Cycle of Atomic Layer Deposition: An Adsorbate Control Method. Chemistry of Materials, 33(11), 4099–4105. https://doi.org/10.1021/acs.chemmater.1c00729

How many times has this paper been cited?

47 times, according to OpenAlex on 24 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Dae‐Hyun Kim, Jae Chan Park, Jeongwoo Park, Deok‐Yong Cho, Woo‐Hee Kim, Bonggeun Shong, Ji‐Hoon Ahn, Tae Joo Park.

What is the DOI of this paper?

10.1021/acs.chemmater.1c00729, permanently at https://doi.org/10.1021/acs.chemmater.1c00729. Sign in and open it from this page.

Bibliographic data from OpenAlex (CC0), last checked 24 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.