Journal article · 2018 · Open access
Two-Dimensional Crystal Grain Size Tuning in WS 2 Atomic Layer Deposition: An Insight in the Nucleation Mechanism
Chemistry of Materials, 30(21), 7648–7663 · Published 17 September 2018 · DOI 10.1021/acs.chemmater.8b02924
In brief
“Two-Dimensional Crystal Grain Size Tuning in WS 2 Atomic Layer Deposition: An Insight in the Nucleation Mechanism” is a 2018 journal article by Benjamin Groven and 16 co-authors, published in Chemistry of Materials. OpenAlex counts 82 citations as of 24 November 2026. It is open access: the full text is free to read at Lirias.
- Citations
- 82
- Most cited in
- 2023 (15)
- Field-weighted impact
- 2.54
- References
- 84
- Authors
- 17
Abstract
When two-dimensional (2D) group-VI transition metal dichalcogenides such as tungsten disulfide (WS 2 ) are grown by atomic layer deposition (ALD) for atomic growth control at low deposition temperatures (≤450 °C), they often suffer from a nanocrystalline grain structure limiting the carrier mobility. The crystallinity and monolayer thickness control during ALD of 2D materials is determined by the nucleation mechanism, which is currently not well understood. Here, we propose a qualitative model for the WS 2 nucleation behavior on dielectric surfaces during plasma-enhanced (PE-) ALD using tungsten hexafluoride (WF 6 ), dihydrogen (H 2 ) plasma and dihydrogen sulfide (H 2 S) based on analyses of the morphology of the WS 2 crystals. The WS 2 crystal grain size increases from ∼20 to 200 nm by lowering the nucleation density. This is achieved by lowering the precursor adsorption rate on the starting surface using an inherently less reactive starting surface, by decreasing the H 2 plasma reactivity, and by enhancing the mobility of the adsorbed species at higher deposition temperature. Since silicon dioxide (SiO 2 ) is less reactive than aluminum oxide (Al 2 O 3 ), and diffusion and crystal ripening is enhanced at higher deposition temperature, WS 2 nucleates in an anisotropic island-like growth mode with preferential lateral growth from the WS 2 crystal edges. This work emphasizes that increasing the crystal grain size while controlling the basal plane orientation is possible during ALD at low deposition temperatures, based on insight in the nucleation behavior, which is key to advance the field of ALD of 2D materials. Moreover, this work demonstrates the conformal deposition on three-dimensional (3D) structures, with WS 2 retaining the basal plane orientation along topographic structures.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Groven, B., Mehta, A. N., Bender, H., Meersschaut, J., Nuytten, T., Verdonck, P. B., Conard, T. S., Smets, Q., Schram, T., Schoenaers, B., Stesmans, A. L., Afanas'ev, V. V., Vandervorst, W., Heyns, M., Caymax, M. R., Radu, I. P., & Delabie, A. (2018). Two-Dimensional Crystal Grain Size Tuning in WS 2 Atomic Layer Deposition: An Insight in the Nucleation Mechanism. Chemistry of Materials, 30(21), 7648–7663. https://doi.org/10.1021/acs.chemmater.8b02924
MLA 9
Groven, Benjamin, et al. “Two-Dimensional Crystal Grain Size Tuning in WS 2 Atomic Layer Deposition: An Insight in the Nucleation Mechanism.” Chemistry of Materials, vol. 30, no. 21, 2018, pp. 7648–7663. https://doi.org/10.1021/acs.chemmater.8b02924.
Chicago
Groven, Benjamin, Ankit Nalin Mehta, Hugo Bender, Johan Meersschaut, Thomas Nuytten, Patrick Bernard Verdonck, Thierry S. Conard, et al. 2018. “Two-Dimensional Crystal Grain Size Tuning in WS 2 Atomic Layer Deposition: An Insight in the Nucleation Mechanism.” Chemistry of Materials 30 (21): 7648–7663. https://doi.org/10.1021/acs.chemmater.8b02924.
Harvard
Groven, B. et al. (2018) ‘Two-Dimensional Crystal Grain Size Tuning in WS 2 Atomic Layer Deposition: An Insight in the Nucleation Mechanism’, Chemistry of Materials, 30(21), pp. 7648–7663. doi:10.1021/acs.chemmater.8b02924.
IEEE
B. Groven et al., “Two-Dimensional Crystal Grain Size Tuning in WS 2 Atomic Layer Deposition: An Insight in the Nucleation Mechanism,” Chemistry of Materials, vol. 30, no. 21, pp. 7648–7663, 2018, doi: 10.1021/acs.chemmater.8b02924.
BibTeX
@article{groven2018dimensional,
title = {{Two-Dimensional Crystal Grain Size Tuning in WS 2 Atomic Layer Deposition: An Insight in the Nucleation Mechanism}},
author = {Groven, Benjamin and Mehta, Ankit Nalin and Bender, Hugo and Meersschaut, Johan and Nuytten, Thomas and Verdonck, Patrick Bernard and Conard, Thierry S. and Smets, Quentin and Schram, Tom and Schoenaers, Ben and Stesmans, André L. and Afanas'ev, Valery V. and Vandervorst, Wilfried and Heyns, Marc and Caymax, Matty R. and Radu, Iuliana P. and Delabie, Annelies},
journal = {Chemistry of Materials},
year = {2018},
volume = {30},
number = {21},
pages = {7648--7663},
doi = {10.1021/acs.chemmater.8b02924},
url = {https://doi.org/10.1021/acs.chemmater.8b02924}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2018 | 1 | |
| 2019 | 11 | |
| 2020 | 11 | |
| 2021 | 9 | |
| 2022 | 11 | |
| 2023 | 15 | |
| 2024 | 9 | |
| 2025 | 7 | |
| 2026 | 8 |
Its field-weighted citation impact is 2.54: it has been cited 2.54 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Materials Science › Materials Chemistry › 2D Materials and Applications
- tungsten disulfide
- atomic layer deposition
- nucleation mechanism
- crystal grain size
- two-dimensional materials
- transition metal dichalcogenides
- plasma-enhanced ALD
- tungsten hexafluoride
Work with this paper
Most-cited papers in Materials Science
- Electric Field Effect in Atomically Thin Carbon FilmsKostya S. Novoselov, Andre K. Geim, Sergey V. Morozov and 5 more · Science · 2004 · 67,474 citations
- Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenidesROBERT D. SHANNON · Acta Crystallographica Section A · 1976 · 66,944 citations
- Ab initio molecular dynamics for liquid metalsGeorg Kresse, J. Häfner · Physical review. B, Condensed matter · 1993 · 46,320 citations
- Helical microtubules of graphitic carbonSumio Iijima · Nature · 1991 · 43,639 citations
- The rise of grapheneAndre K. Geim, Kostya S. Novoselov · Nature Materials · 2007 · 40,328 citations
Questions about this paper
How do I cite this paper in APA style?
Groven, B., Mehta, A. N., Bender, H., Meersschaut, J., Nuytten, T., Verdonck, P. B., Conard, T. S., Smets, Q., Schram, T., Schoenaers, B., Stesmans, A. L., Afanas'ev, V. V., Vandervorst, W., Heyns, M., Caymax, M. R., Radu, I. P., & Delabie, A. (2018). Two-Dimensional Crystal Grain Size Tuning in WS 2 Atomic Layer Deposition: An Insight in the Nucleation Mechanism. Chemistry of Materials, 30(21), 7648–7663. https://doi.org/10.1021/acs.chemmater.8b02924
How many times has this paper been cited?
82 times, according to OpenAlex on 24 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access at Lirias: sign in and open the PDF from this page.
Who wrote this paper?
Benjamin Groven, Ankit Nalin Mehta, Hugo Bender, Johan Meersschaut, Thomas Nuytten, Patrick Bernard Verdonck, Thierry S. Conard, Quentin Smets, Tom Schram, Ben Schoenaers, André L. Stesmans, Valery V. Afanas'ev and 5 more.
What is the DOI of this paper?
10.1021/acs.chemmater.8b02924, permanently at https://doi.org/10.1021/acs.chemmater.8b02924. Sign in and open it from this page.
Bibliographic data from OpenAlex (CC0), last checked 24 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.