Journal article · 1993 · Open access

The nanoindentation response of systems with thin hard carbon coatings

S. V. Hainsworth, T. Bartlett, T. F. Page

Thin Solid Films, 236(1-2), 214–218 · Published 1 December 1993 · DOI 10.1016/0040-6090(93)90672-c

Open full textView at the publisherCite this paper

In brief

“The nanoindentation response of systems with thin hard carbon coatings” is a 1993 journal article by S. V. Hainsworth and 2 co-authors, published in Thin Solid Films. OpenAlex counts 62 citations as of 19 November 2026. It is open access under a CC BY licence: the full text is free to read at Durham Research Online (Durham University).

Citations
62
Most cited in
2015 (2)
Field-weighted impact
9.03
References
6
Authors
3

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Hainsworth, S. V., Bartlett, T., & Page, T. F. (1993). The nanoindentation response of systems with thin hard carbon coatings. Thin Solid Films, 236(1-2), 214–218. https://doi.org/10.1016/0040-6090(93)90672-c

MLA 9

Hainsworth, S. V., et al. “The nanoindentation response of systems with thin hard carbon coatings.” Thin Solid Films, vol. 236, no. 1-2, 1993, pp. 214–218. https://doi.org/10.1016/0040-6090(93)90672-c.

Chicago

Hainsworth, S. V., T. Bartlett, and T. F. Page. 1993. “The nanoindentation response of systems with thin hard carbon coatings.” Thin Solid Films 236 (1-2): 214–218. https://doi.org/10.1016/0040-6090(93)90672-c.

Harvard

Hainsworth, S. V., Bartlett, T. and Page, T. F. (1993) ‘The nanoindentation response of systems with thin hard carbon coatings’, Thin Solid Films, 236(1-2), pp. 214–218. doi:10.1016/0040-6090(93)90672-c.

IEEE

S. V. Hainsworth, T. Bartlett, and T. F. Page, “The nanoindentation response of systems with thin hard carbon coatings,” Thin Solid Films, vol. 236, no. 1-2, pp. 214–218, 1993, doi: 10.1016/0040-6090(93)90672-c.

BibTeX

@article{hainsworth1993nanoindentation,
  title     = {{The nanoindentation response of systems with thin hard carbon coatings}},
  author    = {Hainsworth, S. V. and Bartlett, T. and Page, T. F.},
  journal   = {Thin Solid Films},
  year      = {1993},
  volume    = {236},
  number    = {1-2},
  pages     = {214--218},
  doi       = {10.1016/0040-6090(93)90672-c},
  url       = {https://doi.org/10.1016/0040-6090(93)90672-c}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
201211
201311
201411
201522
201611
201711
201811

Its field-weighted citation impact is 9.03: it has been cited 9.03 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics

  • nanoindentation
  • coating thickness
  • substrate effects
  • magnesium oxide single crystals
  • polytetrafluoroethylene
  • load-displacement curve
  • hardness
  • elastic recovery

Work with this paper

Most-cited papers in Engineering

All highly cited Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Hainsworth, S. V., Bartlett, T., & Page, T. F. (1993). The nanoindentation response of systems with thin hard carbon coatings. Thin Solid Films, 236(1-2), 214–218. https://doi.org/10.1016/0040-6090(93)90672-c

How many times has this paper been cited?

62 times, according to OpenAlex on 19 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

Yes. It is open access at Durham Research Online (Durham University): sign in and open the full text from this page.

Who wrote this paper?

S. V. Hainsworth, T. Bartlett, T. F. Page.

What is the DOI of this paper?

10.1016/0040-6090(93)90672-c, permanently at https://doi.org/10.1016/0040-6090(93)90672-c. Sign in and open it from this page.

Bibliographic data from OpenAlex (CC0), last checked 19 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.