The influence of sputtering procedure on nanoindentation and nanoscratch behaviour of W–S–C film
Applied Surface Science, 256(22), 6850–6858 · Published 3 May 2010 · DOI 10.1016/j.apsusc.2010.04.100
In brief
“The influence of sputtering procedure on nanoindentation and nanoscratch behaviour of W–S–C film” is a 2010 journal article by Manish Roy and 2 co-authors, published in Applied Surface Science. OpenAlex counts 19 citations as of 17 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.
- Citations
- 19
- Most cited in
- 2013 (4)
- Field-weighted impact
- 2.85
- References
- 41
- Authors
- 3
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Roy, M., Koch, T., & Pauschitz, A. (2010). The influence of sputtering procedure on nanoindentation and nanoscratch behaviour of W–S–C film. Applied Surface Science, 256(22), 6850–6858. https://doi.org/10.1016/j.apsusc.2010.04.100
MLA 9
Roy, Manish, et al. “The influence of sputtering procedure on nanoindentation and nanoscratch behaviour of W–S–C film.” Applied Surface Science, vol. 256, no. 22, 2010, pp. 6850–6858. https://doi.org/10.1016/j.apsusc.2010.04.100.
Chicago
Roy, Manish, Thomas Koch, and Andreas Pauschitz. 2010. “The influence of sputtering procedure on nanoindentation and nanoscratch behaviour of W–S–C film.” Applied Surface Science 256 (22): 6850–6858. https://doi.org/10.1016/j.apsusc.2010.04.100.
Harvard
Roy, M., Koch, T. and Pauschitz, A. (2010) ‘The influence of sputtering procedure on nanoindentation and nanoscratch behaviour of W–S–C film’, Applied Surface Science, 256(22), pp. 6850–6858. doi:10.1016/j.apsusc.2010.04.100.
IEEE
M. Roy, T. Koch, and A. Pauschitz, “The influence of sputtering procedure on nanoindentation and nanoscratch behaviour of W–S–C film,” Applied Surface Science, vol. 256, no. 22, pp. 6850–6858, 2010, doi: 10.1016/j.apsusc.2010.04.100.
BibTeX
@article{roy2010influence,
title = {{The influence of sputtering procedure on nanoindentation and nanoscratch behaviour of W–S–C film}},
author = {Roy, Manish and Koch, Thomas and Pauschitz, Andreas},
journal = {Applied Surface Science},
year = {2010},
volume = {256},
number = {22},
pages = {6850--6858},
doi = {10.1016/j.apsusc.2010.04.100},
url = {https://doi.org/10.1016/j.apsusc.2010.04.100}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2012 | 1 | |
| 2013 | 4 | |
| 2014 | 1 | |
| 2015 | 1 | |
| 2016 | 2 | |
| 2017 | 1 | |
| 2019 | 1 | |
| 2020 | 4 | |
| 2024 | 1 | |
| 2026 | 1 |
Its field-weighted citation impact is 2.85: it has been cited 2.85 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics
- tungsten disulfide
- co-sputtering
- reactive sputtering
- carbon incorporation
- self-lubricating coatings
- MEMS applications
- nanoindentation
- hardness
Work with this paper
Most-cited papers in Engineering
- A Closed‐form Equation for Predicting the Hydraulic Conductivity of Unsaturated SoilsMartinus Th. van Genuchten · Soil Science Society of America Journal · 1980 · 28,197 citations
- An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experimentsW. C. Oliver, George M. Pharr · Journal of materials research/Pratt's guide to venture capital sources · 1992 · 27,379 citations
- Digital communicationsOwen Bishop · Routledge eBooks · 2007 · 24,890 citations
- The empirical mode decomposition and the Hilbert spectrum for nonlinear and non-stationary time series analysisNorden Eh Huang, Zhengwei Shen, Steven R. Long and 6 more · Proceedings of the Royal Society A Mathematical Physical and Engineering Sciences · 1998 · 24,008 citations
- Numerical Heat Transfer and Fluid FlowSuhas V. Patankar · CRC Press eBooks · 2018 · 23,491 citations
Questions about this paper
How do I cite this paper in APA style?
Roy, M., Koch, T., & Pauschitz, A. (2010). The influence of sputtering procedure on nanoindentation and nanoscratch behaviour of W–S–C film. Applied Surface Science, 256(22), 6850–6858. https://doi.org/10.1016/j.apsusc.2010.04.100
How many times has this paper been cited?
19 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.
Who wrote this paper?
Manish Roy, Thomas Koch, Andreas Pauschitz.
What is the DOI of this paper?
10.1016/j.apsusc.2010.04.100, permanently at https://doi.org/10.1016/j.apsusc.2010.04.100. Sign in and open it from this page.
Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.