Journal article · 2009 · Open access
Surface Analysis of Carbon–Hydrogen Bonds in Diamondlike Carbon Films by X-ray Photoelectron Spectroscopy
Japanese Journal of Applied Physics, 48(9), 092304 · Published 24 September 2009 · DOI 10.1143/jjap.48.092304
In brief
“Surface Analysis of Carbon–Hydrogen Bonds in Diamondlike Carbon Films by X-ray Photoelectron Spectroscopy” is a 2009 journal article by Susumu Takabayashi and 4 co-authors, published in Japanese Journal of Applied Physics. OpenAlex counts 25 citations as of 16 November 2026. It is open access: the full text is free to read at Japanese Journal of Applied Physics.
- Citations
- 25
- Most cited in
- 2024 (4)
- Field-weighted impact
- 1.97
- References
- 41
- Authors
- 5
Abstract
X-ray photoelectron spectroscopy (XPS) was used to analyze the carbon–hydrogen bonds near the surfaces of two types of diamondlike carbon (DLC) film with different hydrogen distribution, which were prepared by the unbalanced magnetron sputtering (UBMS) and ionized deposition (ID) methods, respectively. Elastic recoil detection (ERD) analysis revealed that, in the UBMS films, hydrogen is distributed homogeneously along the depth axis, while in the ID film it is distributed inhomogeneously and concentrated at the surface. The C 1s spectra of the UBMS films with different hydrogen concentrations suggested that the spectra are decomposed into four components, corresponding to the carbon–hydrogen and carbon–carbon bonds of the sp 2 and sp 3 carbons. A correlation between the hydrogen concentrations obtained by the XPS and ERD analyses was observed. The C 1s spectrum of the ID film depended on the emission angle, suggesting that the carbon–hydrogen bonds concentrate at the surface. This result agreed with the ERD result. Both correlations suggested that XPS can analyze hydrogen as an atom bound to a carbon atom and be a comprehensive surface analytical tool for DLC films.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Takabayashi, S., Okamoto, K., Nakatani, T., Sakaue, H., & Takahagi, T. (2009). Surface Analysis of Carbon–Hydrogen Bonds in Diamondlike Carbon Films by X-ray Photoelectron Spectroscopy. Japanese Journal of Applied Physics, 48(9), 092304. https://doi.org/10.1143/jjap.48.092304
MLA 9
Takabayashi, Susumu, et al. “Surface Analysis of Carbon–Hydrogen Bonds in Diamondlike Carbon Films by X-ray Photoelectron Spectroscopy.” Japanese Journal of Applied Physics, vol. 48, no. 9, 2009, p. 092304. https://doi.org/10.1143/jjap.48.092304.
Chicago
Takabayashi, Susumu, Keishi Okamoto, Tatsuyuki Nakatani, Hiroyuki Sakaue, and Takayuki Takahagi. 2009. “Surface Analysis of Carbon–Hydrogen Bonds in Diamondlike Carbon Films by X-ray Photoelectron Spectroscopy.” Japanese Journal of Applied Physics 48 (9): 092304. https://doi.org/10.1143/jjap.48.092304.
Harvard
Takabayashi, S. et al. (2009) ‘Surface Analysis of Carbon–Hydrogen Bonds in Diamondlike Carbon Films by X-ray Photoelectron Spectroscopy’, Japanese Journal of Applied Physics, 48(9), p. 092304. doi:10.1143/jjap.48.092304.
IEEE
S. Takabayashi, K. Okamoto, T. Nakatani, H. Sakaue, and T. Takahagi, “Surface Analysis of Carbon–Hydrogen Bonds in Diamondlike Carbon Films by X-ray Photoelectron Spectroscopy,” Japanese Journal of Applied Physics, vol. 48, no. 9, p. 092304, 2009, doi: 10.1143/jjap.48.092304.
BibTeX
@article{takabayashi2009surface,
title = {{Surface Analysis of Carbon–Hydrogen Bonds in Diamondlike Carbon Films by X-ray Photoelectron Spectroscopy}},
author = {Takabayashi, Susumu and Okamoto, Keishi and Nakatani, Tatsuyuki and Sakaue, Hiroyuki and Takahagi, Takayuki},
journal = {Japanese Journal of Applied Physics},
year = {2009},
volume = {48},
number = {9},
pages = {092304},
doi = {10.1143/jjap.48.092304},
url = {https://doi.org/10.1143/jjap.48.092304}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2013 | 2 | |
| 2014 | 2 | |
| 2015 | 1 | |
| 2016 | 2 | |
| 2018 | 1 | |
| 2019 | 1 | |
| 2021 | 1 | |
| 2022 | 1 | |
| 2023 | 1 | |
| 2024 | 4 |
Its field-weighted citation impact is 1.97: it has been cited 1.97 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Materials Science › Surfaces, Coatings and Films › Electron and X-Ray Spectroscopy Techniques
- diamond-like carbon films
- carbon-hydrogen bonds
- hydrogen distribution
- unbalanced magnetron sputtering
- C 1s spectra
- sp2 and sp3 carbon
- surface hydrogen concentration
- emission angle dependence
Work with this paper
Most-cited papers in Materials Science
- Electric Field Effect in Atomically Thin Carbon FilmsKostya S. Novoselov, Andre K. Geim, Sergey V. Morozov and 5 more · Science · 2004 · 67,474 citations
- Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenidesROBERT D. SHANNON · Acta Crystallographica Section A · 1976 · 66,944 citations
- Ab initio molecular dynamics for liquid metalsGeorg Kresse, J. Häfner · Physical review. B, Condensed matter · 1993 · 46,320 citations
- Helical microtubules of graphitic carbonSumio Iijima · Nature · 1991 · 43,639 citations
- The rise of grapheneAndre K. Geim, Kostya S. Novoselov · Nature Materials · 2007 · 40,328 citations
Questions about this paper
How do I cite this paper in APA style?
Takabayashi, S., Okamoto, K., Nakatani, T., Sakaue, H., & Takahagi, T. (2009). Surface Analysis of Carbon–Hydrogen Bonds in Diamondlike Carbon Films by X-ray Photoelectron Spectroscopy. Japanese Journal of Applied Physics, 48(9), 092304. https://doi.org/10.1143/jjap.48.092304
How many times has this paper been cited?
25 times, according to OpenAlex on 16 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access: read the free full text at Japanese Journal of Applied Physics.
Who wrote this paper?
Susumu Takabayashi, Keishi Okamoto, Tatsuyuki Nakatani, Hiroyuki Sakaue, Takayuki Takahagi.
What is the DOI of this paper?
10.1143/jjap.48.092304. The permanent link is https://doi.org/10.1143/jjap.48.092304.
Bibliographic data from OpenAlex (CC0), last checked 16 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.