Journal article · 2026 · Open access
Surface analysis of carbon allotropes
Lithuanian Journal of Physics, 65(4) · Published 10 February 2026 · DOI 10.3952/physics.2025.65.4.6
In brief
“Surface analysis of carbon allotropes” is a 2026 journal article by Saulius Kaciulis, published in Lithuanian Journal of Physics. OpenAlex counts 0 citations as of 18 November 2026. It is open access: the full text is free to read at Lithuanian Journal of Physics.
- Citations
- 0
- References
- 98
- Authors
- 1
Abstract
The spectroscopy of carbon is very important in surface analysis of solids, because its content indicates the grade of surface contamination. Adventitious carbon from air ambient is practically present on any solid material and the C 1s photoelectron spectrum is often used as a reference for the scale calibration of binding energy. Moreover, during the last two decades, new 2D carbon materials have been developed and intensively investigated: graphene, fullerenes, nanotubes and nanowalls, quantum dots, etc. Also, the growing applications of amorphous carbon (a-C), e.g. diamond-like carbon (DLC), carbon quantum dots (CQDs), etc., require the characterization of these materials.This short overview is dedicated to the analysis of new carbon-based materials by widely used surface-sensitive techniques: X-ray photoelectron spectroscopy (XPS) and Auger electron spectroscopy (AES). The combination of XPS and AES techniques permits one to investigate the electron hybridization in carbon materials, i.e. to determine the ratio of sp 2 /sp 3 configurations, which defines their main mechanical, electrical and optical properties. In addition, it was demonstrated that the same experimental approach could be successfully used for the investigation of bulk composite materials containing 2D carbon, e.g. graphene or nanotubes.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Kaciulis, S. (2026). Surface analysis of carbon allotropes. Lithuanian Journal of Physics, 65(4). https://doi.org/10.3952/physics.2025.65.4.6
MLA 9
Kaciulis, Saulius. “Surface analysis of carbon allotropes.” Lithuanian Journal of Physics, vol. 65, no. 4, 2026. https://doi.org/10.3952/physics.2025.65.4.6.
Chicago
Kaciulis, Saulius. 2026. “Surface analysis of carbon allotropes.” Lithuanian Journal of Physics 65 (4). https://doi.org/10.3952/physics.2025.65.4.6.
Harvard
Kaciulis, S. (2026) ‘Surface analysis of carbon allotropes’, Lithuanian Journal of Physics, 65(4). doi:10.3952/physics.2025.65.4.6.
IEEE
S. Kaciulis, “Surface analysis of carbon allotropes,” Lithuanian Journal of Physics, vol. 65, no. 4, 2026, doi: 10.3952/physics.2025.65.4.6.
BibTeX
@article{kaciulis2026surface,
title = {{Surface analysis of carbon allotropes}},
author = {Kaciulis, Saulius},
journal = {Lithuanian Journal of Physics},
year = {2026},
volume = {65},
number = {4},
doi = {10.3952/physics.2025.65.4.6},
url = {https://doi.org/10.3952/physics.2025.65.4.6}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Topic and keywords
Physical Sciences › Materials Science › Surfaces, Coatings and Films › Electron and X-Ray Spectroscopy Techniques
- carbon allotropes
- surface contamination
- graphene
- C60
- carbon nanotubes
- nanowalls
- carbon quantum dots
- diamond-like carbon
Work with this paper
Most-cited papers in Materials Science
- Electric Field Effect in Atomically Thin Carbon FilmsKostya S. Novoselov, Andre K. Geim, Sergey V. Morozov and 5 more · Science · 2004 · 67,474 citations
- Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenidesROBERT D. SHANNON · Acta Crystallographica Section A · 1976 · 66,944 citations
- Ab initio molecular dynamics for liquid metalsGeorg Kresse, J. Häfner · Physical review. B, Condensed matter · 1993 · 46,320 citations
- Helical microtubules of graphitic carbonSumio Iijima · Nature · 1991 · 43,639 citations
- The rise of grapheneAndre K. Geim, Kostya S. Novoselov · Nature Materials · 2007 · 40,328 citations
Questions about this paper
How do I cite this paper in APA style?
Kaciulis, S. (2026). Surface analysis of carbon allotropes. Lithuanian Journal of Physics, 65(4). https://doi.org/10.3952/physics.2025.65.4.6
How many times has this paper been cited?
0 times, according to OpenAlex on 18 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access at Lithuanian Journal of Physics: sign in and open the PDF from this page.
Who wrote this paper?
Saulius Kaciulis.
What is the DOI of this paper?
10.3952/physics.2025.65.4.6, permanently at https://doi.org/10.3952/physics.2025.65.4.6. Sign in and open it from this page.
Bibliographic data from OpenAlex (CC0), last checked 18 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.