Surface analysis of a- $Si_{x}C_{1-x}$ : H deposited by RF plasma-enhanced CVD

Yong-Tak Kim, Wooseok Yang, Hyun Lee, Byungyou Hong, Dae Ho Yoon

Journal of the Korean Crystal Growth and Crystal Technology, 10(1), 1–4 · Published 1 January 2000

View at the publisherCite this paper

In brief

“Surface analysis of a- $Si_{x}C_{1-x}$ : H deposited by RF plasma-enhanced CVD” is a 2000 journal article by Yong-Tak Kim and 4 co-authors, published in Journal of the Korean Crystal Growth and Crystal Technology. OpenAlex counts 0 citations as of 16 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
0
Authors
5

Abstract

Thin films of hydrogenated amorphous silicon carbide compounds () of different compositions were deposited on Si substrate by RF plasma-enhanced chemical vapor deposition (PECVD). Experiments were carried out using silane (SiH) and methane () as the gas precursors at 1 Torr and at a low substrate temperature (). The gas flow rate was changed with… Read the full abstract at the publisher.

Excerpt. This paper is not open access.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Kim, Y.-T., Yang, W., Lee, H., Hong, B., & Yoon, D. H. (2000). Surface analysis of a- $Si_{x}C_{1-x}$ : H deposited by RF plasma-enhanced CVD. Journal of the Korean Crystal Growth and Crystal Technology, 10(1), 1–4. https://www.koreascience.kr/article/ArticleFullRecord.jsp?cn=GJSJBE_2000_v10n1_1

MLA 9

Kim, Yong-Tak, et al. “Surface analysis of a- $Si_{x}C_{1-x}$ : H deposited by RF plasma-enhanced CVD.” Journal of the Korean Crystal Growth and Crystal Technology, vol. 10, no. 1, 2000, pp. 1–4. https://www.koreascience.kr/article/ArticleFullRecord.jsp?cn=GJSJBE_2000_v10n1_1.

Chicago

Kim, Yong-Tak, Wooseok Yang, Hyun Lee, Byungyou Hong, and Dae Ho Yoon. 2000. “Surface analysis of a- $Si_{x}C_{1-x}$ : H deposited by RF plasma-enhanced CVD.” Journal of the Korean Crystal Growth and Crystal Technology 10 (1): 1–4. https://www.koreascience.kr/article/ArticleFullRecord.jsp?cn=GJSJBE_2000_v10n1_1.

Harvard

Kim, Y.-T. et al. (2000) ‘Surface analysis of a- $Si_{x}C_{1-x}$ : H deposited by RF plasma-enhanced CVD’, Journal of the Korean Crystal Growth and Crystal Technology, 10(1), pp. 1–4. Available at: https://www.koreascience.kr/article/ArticleFullRecord.jsp?cn=GJSJBE_2000_v10n1_1.

IEEE

Y.-T. Kim, W. Yang, H. Lee, B. Hong, and D. H. Yoon, “Surface analysis of a- $Si_{x}C_{1-x}$ : H deposited by RF plasma-enhanced CVD,” Journal of the Korean Crystal Growth and Crystal Technology, vol. 10, no. 1, pp. 1–4, 2000.

BibTeX

@article{kim2000surface,
  title     = {{Surface analysis of a- \$Si\_{x}C\_{1-x}\$ : H deposited by RF plasma-enhanced CVD}},
  author    = {Kim, Yong-Tak and Yang, Wooseok and Lee, Hyun and Hong, Byungyou and Yoon, Dae Ho},
  journal   = {Journal of the Korean Crystal Growth and Crystal Technology},
  year      = {2000},
  volume    = {10},
  number    = {1},
  pages     = {1--4},
  url       = {https://www.koreascience.kr/article/ArticleFullRecord.jsp?cn=GJSJBE_2000_v10n1_1}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Topic and keywords

Physical Sciences › Engineering › Electrical and Electronic Engineering › Silicon Carbide Semiconductor Technologies

  • hydrogenated amorphous silicon carbide
  • hydrogenated amorphous silicon
  • thin films
  • RF plasma-enhanced chemical vapor deposition
  • silane
  • methane
  • surface morphology
  • bonding structure

Work with this paper

Most-cited papers in Engineering

All highly cited Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Kim, Y.-T., Yang, W., Lee, H., Hong, B., & Yoon, D. H. (2000). Surface analysis of a- $Si_{x}C_{1-x}$ : H deposited by RF plasma-enhanced CVD. Journal of the Korean Crystal Growth and Crystal Technology, 10(1), 1–4. https://www.koreascience.kr/article/ArticleFullRecord.jsp?cn=GJSJBE_2000_v10n1_1

How many times has this paper been cited?

0 times, according to OpenAlex on 16 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Yong-Tak Kim, Wooseok Yang, Hyun Lee, Byungyou Hong, Dae Ho Yoon.

Bibliographic data from OpenAlex (CC0), last checked 16 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.