Journal article · 2017

Study of MIG/MAG welding procedures for application of coatings of Inconel 625 nickel alloy on ASTM A387 Gr.11 structural steel

Nathália Escóssio Cavalcante, Tathiane Caminha Andrade, Pedro Helton Magalhães Pinheiro, Hélio Cordeiro de Miranda, Marcelo Ferreira Motta, Willys Machado Aguiar

Welding International, 32(2), 112–121 · Published 20 October 2017 · DOI 10.1080/09507116.2017.1347324

View at the publisherCite this paper

In brief

“Study of MIG/MAG welding procedures for application of coatings of Inconel 625 nickel alloy on ASTM A387 Gr.11 structural steel” is a 2017 journal article by Nathália Escóssio Cavalcante and 5 co-authors, published in Welding International. OpenAlex counts 8 citations as of 22 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
8
Most cited in
2024 (4)
References
3
Authors
6

Abstract

This work aims to study welding techniques applied to repair of components made of ASTM A387 Gr.11 steel, widely used in the oil and gas industry. Due to the working conditions, it is necessary to use materials having good strength and corrosion resistance. UNS N06625 Ni-based alloy (Inconel 625) was used as the filler metal.… Read the full abstract at the publisher.

Excerpt. This paper is not open access.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Cavalcante, N. E., Andrade, T. C., Pinheiro, P. H. M., de Miranda, H. C., Motta, M. F., & Aguiar, W. M. (2017). Study of MIG/MAG welding procedures for application of coatings of Inconel 625 nickel alloy on ASTM A387 Gr.11 structural steel. Welding International, 32(2), 112–121. https://doi.org/10.1080/09507116.2017.1347324

MLA 9

Cavalcante, Nathália Escóssio, et al. “Study of MIG/MAG welding procedures for application of coatings of Inconel 625 nickel alloy on ASTM A387 Gr.11 structural steel.” Welding International, vol. 32, no. 2, 2017, pp. 112–121. https://doi.org/10.1080/09507116.2017.1347324.

Chicago

Cavalcante, Nathália Escóssio, Tathiane Caminha Andrade, Pedro Helton Magalhães Pinheiro, Hélio Cordeiro de Miranda, Marcelo Ferreira Motta, and Willys Machado Aguiar. 2017. “Study of MIG/MAG welding procedures for application of coatings of Inconel 625 nickel alloy on ASTM A387 Gr.11 structural steel.” Welding International 32 (2): 112–121. https://doi.org/10.1080/09507116.2017.1347324.

Harvard

Cavalcante, N. E. et al. (2017) ‘Study of MIG/MAG welding procedures for application of coatings of Inconel 625 nickel alloy on ASTM A387 Gr.11 structural steel’, Welding International, 32(2), pp. 112–121. doi:10.1080/09507116.2017.1347324.

IEEE

N. E. Cavalcante, T. C. Andrade, P. H. M. Pinheiro, H. C. de Miranda, M. F. Motta, and W. M. Aguiar, “Study of MIG/MAG welding procedures for application of coatings of Inconel 625 nickel alloy on ASTM A387 Gr.11 structural steel,” Welding International, vol. 32, no. 2, pp. 112–121, 2017, doi: 10.1080/09507116.2017.1347324.

BibTeX

@article{cavalcante2017study,
  title     = {{Study of MIG/MAG welding procedures for application of coatings of Inconel 625 nickel alloy on ASTM A387 Gr.11 structural steel}},
  author    = {Cavalcante, Nathália Escóssio and Andrade, Tathiane Caminha and Pinheiro, Pedro Helton Magalhães and de Miranda, Hélio Cordeiro and Motta, Marcelo Ferreira and Aguiar, Willys Machado},
  journal   = {Welding International},
  year      = {2017},
  volume    = {32},
  number    = {2},
  pages     = {112--121},
  doi       = {10.1080/09507116.2017.1347324},
  url       = {https://doi.org/10.1080/09507116.2017.1347324}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
202111
202211
202444
202511
202611

Topic and keywords

Physical Sciences › Engineering › Mechanical Engineering › Welding Techniques and Residual Stresses

  • Inconel 625
  • nickel-based alloy coatings
  • temper bead welding
  • MIG/MAG welding
  • heat input
  • heat-affected zone
  • grain refinement
  • microhardness

Work with this paper

Most-cited papers in Engineering

All highly cited Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Cavalcante, N. E., Andrade, T. C., Pinheiro, P. H. M., de Miranda, H. C., Motta, M. F., & Aguiar, W. M. (2017). Study of MIG/MAG welding procedures for application of coatings of Inconel 625 nickel alloy on ASTM A387 Gr.11 structural steel. Welding International, 32(2), 112–121. https://doi.org/10.1080/09507116.2017.1347324

How many times has this paper been cited?

8 times, according to OpenAlex on 22 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Nathália Escóssio Cavalcante, Tathiane Caminha Andrade, Pedro Helton Magalhães Pinheiro, Hélio Cordeiro de Miranda, Marcelo Ferreira Motta, Willys Machado Aguiar.

What is the DOI of this paper?

10.1080/09507116.2017.1347324, permanently at https://doi.org/10.1080/09507116.2017.1347324. Sign in and open it from this page.

Bibliographic data from OpenAlex (CC0), last checked 22 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.