Journal article · 2024 · Open access
Structural Aspects of MoSx Prepared by Atomic Layer Deposition for Hydrogen Evolution Reaction
ACS Catalysis, 14(13), 10089–10101 · Published 20 June 2024 · DOI 10.1021/acscatal.4c01445
In brief
“Structural Aspects of MoSx Prepared by Atomic Layer Deposition for Hydrogen Evolution Reaction” is a 2024 journal article by Miika Mattinen and 6 co-authors, published in ACS Catalysis. OpenAlex counts 20 citations as of 16 November 2026, which puts it in the top 5% of works published in 2024 by citations. It is open access under a CC BY licence: the full text is free to read at ACS Catalysis.
- Citations
- 20
- Most cited in
- 2026 (11)
- Field-weighted impact
- 1.33
- References
- 83
- Authors
- 7
Abstract
High Resolution Image Download MS PowerPoint Slide Molybdenum sulfides (MoS x ) in both crystalline and amorphous forms are promising earth-abundant electrocatalysts for hydrogen evolution reaction (HER) in acid. Plasma-enhanced atomic layer deposition was used to prepare thin films of both amorphous MoS x with adjustable S/Mo ratio (2.8–4.7) and crystalline MoS 2 with tailored crystallinity, morphology, and electrical properties. All the amorphous MoS x films transform into highly HER-active amorphous MoS 2 (overpotential 210–250 mV at 10 mA/cm 2 in 0.5 M H 2 SO 4 ) after electrochemical activation at approximately −0.3 V vs reversible hydrogen electrode. However, the initial film stoichiometry affects the structure and consequently the HER activity and stability. The material changes occurring during activation are studied using ex situ and quasi in situ X-ray photoelectron spectroscopy. Possible structures of as-deposited and activated catalysts are proposed. In contrast to amorphous MoS x, no changes in the structure of crystalline MoS 2 catalysts are observed. The overpotentials of the crystalline films range from 300 to 520 mV at 10 mA/cm 2, being the lowest for the most defective catalysts. This work provides a practical method for deposition of tailored MoS x HER electrocatalysts as well as new insights into their activity and structure.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Mattinen, M., Chen, W., Dawley, R. A., Verheijen, M. A., Hensen, E. J. M., Kessels, W. M. M., & Bol, A. A. (2024). Structural Aspects of MoSx Prepared by Atomic Layer Deposition for Hydrogen Evolution Reaction. ACS Catalysis, 14(13), 10089–10101. https://doi.org/10.1021/acscatal.4c01445
MLA 9
Mattinen, Miika, et al. “Structural Aspects of MoSx Prepared by Atomic Layer Deposition for Hydrogen Evolution Reaction.” ACS Catalysis, vol. 14, no. 13, 2024, pp. 10089–10101. https://doi.org/10.1021/acscatal.4c01445.
Chicago
Mattinen, Miika, Wei Chen, Rebecca A. Dawley, Marcel A. Verheijen, Emiel J. M. Hensen, W. M. M. Kessels, and Ageeth Anke Bol. 2024. “Structural Aspects of MoSx Prepared by Atomic Layer Deposition for Hydrogen Evolution Reaction.” ACS Catalysis 14 (13): 10089–10101. https://doi.org/10.1021/acscatal.4c01445.
Harvard
Mattinen, M. et al. (2024) ‘Structural Aspects of MoSx Prepared by Atomic Layer Deposition for Hydrogen Evolution Reaction’, ACS Catalysis, 14(13), pp. 10089–10101. doi:10.1021/acscatal.4c01445.
IEEE
M. Mattinen et al., “Structural Aspects of MoSx Prepared by Atomic Layer Deposition for Hydrogen Evolution Reaction,” ACS Catalysis, vol. 14, no. 13, pp. 10089–10101, 2024, doi: 10.1021/acscatal.4c01445.
BibTeX
@article{mattinen2024structural,
title = {{Structural Aspects of MoSx Prepared by Atomic Layer Deposition for Hydrogen Evolution Reaction}},
author = {Mattinen, Miika and Chen, Wei and Dawley, Rebecca A. and Verheijen, Marcel A. and Hensen, Emiel J. M. and Kessels, W. M. M. and Bol, Ageeth Anke},
journal = {ACS Catalysis},
year = {2024},
volume = {14},
number = {13},
pages = {10089--10101},
doi = {10.1021/acscatal.4c01445},
url = {https://doi.org/10.1021/acscatal.4c01445}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2024 | 3 | |
| 2025 | 6 | |
| 2026 | 11 |
Its field-weighted citation impact is 1.33: it has been cited 1.33 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › Electrocatalysts for Energy Conversion
- molybdenum sulfide
- MoS2
- hydrogen evolution reaction
- electrocatalysts
- plasma-enhanced atomic layer deposition
- thin films
- electrochemical activation
- crystallinity
Work with this paper
Most-cited papers in Energy
- Electrochemical Photolysis of Water at a Semiconductor ElectrodeAkira Fujishima, Kenichi Honda · Nature · 1972 · 34,586 citations
- A low-cost, high-efficiency solar cell based on dye-sensitized colloidal TiO2 filmsBrian C. O’Regan, Michaël Grätzel · Nature · 1991 · 28,861 citations
- Environmental Applications of Semiconductor PhotocatalysisMichael Robert Hoffmann, Scot T. Martin, Wonyong Choi and 1 more · Chemical Reviews · 1995 · 18,693 citations
- Electrical Energy Storage for the Grid: A Battery of ChoicesBruce Dunn, Haresh Kamath, Jean‐Marie Tarascon · Science · 2011 · 15,286 citations
- Origin of the Overpotential for Oxygen Reduction at a Fuel-Cell CathodeJens K. Nørskov, Jan Rossmeisl, Áshildur Logadóttir and 4 more · The Journal of Physical Chemistry B · 2004 · 13,331 citations
Questions about this paper
How do I cite this paper in APA style?
Mattinen, M., Chen, W., Dawley, R. A., Verheijen, M. A., Hensen, E. J. M., Kessels, W. M. M., & Bol, A. A. (2024). Structural Aspects of MoSx Prepared by Atomic Layer Deposition for Hydrogen Evolution Reaction. ACS Catalysis, 14(13), 10089–10101. https://doi.org/10.1021/acscatal.4c01445
How many times has this paper been cited?
20 times, according to OpenAlex on 16 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access: read the free full text at ACS Catalysis.
Who wrote this paper?
Miika Mattinen, Wei Chen, Rebecca A. Dawley, Marcel A. Verheijen, Emiel J. M. Hensen, W. M. M. Kessels, Ageeth Anke Bol.
What is the DOI of this paper?
10.1021/acscatal.4c01445. The permanent link is https://doi.org/10.1021/acscatal.4c01445.
Bibliographic data from OpenAlex (CC0), last checked 16 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.