Journal article · 2003 · Open access

Stages of Filamentary Carbon Growth from Hydrocarbons on Nickelcontaining Catalysts and Causes of their Deactivation

Vladimir V. Chesnokov, Roman A. Buyanov, В. И. Зайковский

Eurasian Chemico-Technological Journal, 5(4), 253–260 · Published 10 December 2003 · DOI 10.18321/ectj324

Free PDFView at the publisherCite this paper

In brief

“Stages of Filamentary Carbon Growth from Hydrocarbons on Nickelcontaining Catalysts and Causes of their Deactivation” is a 2003 journal article by Vladimir V. Chesnokov and 2 co-authors, published in Eurasian Chemico-Technological Journal. OpenAlex counts 2 citations as of 16 November 2026. It is open access under a CC BY licence: the full text is free to read at Eurasian Chemico-Technological Journal.

Citations
2
Most cited in
2020 (1)
References
1
Authors
3

Abstract

Methane decomposition to carbon and hydrogen has been studied using the Ni/Al2O3, Ni-Cu/Al2O3 andNi-Cu/MgO catalysts at 550 °C. The S-shaped kinetic curves of carbon formation from methane exhibit thefollowing periods: induction, acceleration, stationary state and deactivation. The induction period is characterized by oversaturation of metal or alloy particles with carbon atoms and predominant formation of the graphite phase at the (111) faces of the catalyst particles. After formation of the graphite crystallization centers, the acceleration period is accompanied by the growth of graphite filaments and simultaneous reconstruction of the metal particles. After termination of the above processes, the carbon deposition rate becomes constant. Deactivation of the catalyst is caused by blocking of the front side of the metal particle with a carbon film. When the reaction temperature increases to 700 °C, deactivation of the nickel-containing catalyst follows a different mechanism. During the growth of the filamentary carbon, the metal particle becomes viscous-flowing. This fact allows for its partial capturing by the inner filament channel. As a result, the formed carbon filament has an internal channel filled either with metal or its alloy. Hydrogen addition to methane leads a decrease in the carbon formation rate on the catalyst and a change in the filamentary carbon morphology: now it contains a hollow channel.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Chesnokov, V. V., Buyanov, R. A., & Зайковский, В. И. (2003). Stages of Filamentary Carbon Growth from Hydrocarbons on Nickelcontaining Catalysts and Causes of their Deactivation. Eurasian Chemico-Technological Journal, 5(4), 253–260. https://doi.org/10.18321/ectj324

MLA 9

Chesnokov, Vladimir V., et al. “Stages of Filamentary Carbon Growth from Hydrocarbons on Nickelcontaining Catalysts and Causes of their Deactivation.” Eurasian Chemico-Technological Journal, vol. 5, no. 4, 2003, pp. 253–260. https://doi.org/10.18321/ectj324.

Chicago

Chesnokov, Vladimir V., Roman A. Buyanov, and В. И. Зайковский. 2003. “Stages of Filamentary Carbon Growth from Hydrocarbons on Nickelcontaining Catalysts and Causes of their Deactivation.” Eurasian Chemico-Technological Journal 5 (4): 253–260. https://doi.org/10.18321/ectj324.

Harvard

Chesnokov, V. V., Buyanov, R. A. and Зайковский, В. И. (2003) ‘Stages of Filamentary Carbon Growth from Hydrocarbons on Nickelcontaining Catalysts and Causes of their Deactivation’, Eurasian Chemico-Technological Journal, 5(4), pp. 253–260. doi:10.18321/ectj324.

IEEE

V. V. Chesnokov, R. A. Buyanov, and В. И. Зайковский, “Stages of Filamentary Carbon Growth from Hydrocarbons on Nickelcontaining Catalysts and Causes of their Deactivation,” Eurasian Chemico-Technological Journal, vol. 5, no. 4, pp. 253–260, 2003, doi: 10.18321/ectj324.

BibTeX

@article{chesnokov2003stages,
  title     = {{Stages of Filamentary Carbon Growth from Hydrocarbons on Nickelcontaining Catalysts and Causes of their Deactivation}},
  author    = {Chesnokov, Vladimir V. and Buyanov, Roman A. and Зайковский, В. И.},
  journal   = {Eurasian Chemico-Technological Journal},
  year      = {2003},
  volume    = {5},
  number    = {4},
  pages     = {253--260},
  doi       = {10.18321/ectj324},
  url       = {https://doi.org/10.18321/ectj324}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Topic and keywords

Physical Sciences › Chemical Engineering › Catalysis › Catalysts for Methane Reforming

  • methane decomposition
  • carbon deposition
  • nickel catalysts
  • Ni-Cu catalyst
  • catalyst deactivation
  • induction period
  • hydrogen addition
  • carbon morphology

Work with this paper

Most-cited papers in Chemical Engineering

All highly cited Chemical Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Chesnokov, V. V., Buyanov, R. A., & Зайковский, В. И. (2003). Stages of Filamentary Carbon Growth from Hydrocarbons on Nickelcontaining Catalysts and Causes of their Deactivation. Eurasian Chemico-Technological Journal, 5(4), 253–260. https://doi.org/10.18321/ectj324

How many times has this paper been cited?

2 times, according to OpenAlex on 16 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

Yes. It is open access: read the free full text at Eurasian Chemico-Technological Journal.

Who wrote this paper?

Vladimir V. Chesnokov, Roman A. Buyanov, В. И. Зайковский.

What is the DOI of this paper?

10.18321/ectj324. The permanent link is https://doi.org/10.18321/ectj324.

Bibliographic data from OpenAlex (CC0), last checked 16 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.