Preparation of boron-doped ZnO thin films by photo-atomic layer deposition

Yukio Yamamoto, K. Saito, Kiyoshi Takahashi, Makoto Konagai

Solar Energy Materials and Solar Cells, 65(1-4), 125–132 · Published 1 January 2001 · DOI 10.1016/s0927-0248(00)00086-6

View at the publisherCite this paper

In brief

“Preparation of boron-doped ZnO thin films by photo-atomic layer deposition” is a 2001 journal article by Yukio Yamamoto and 3 co-authors, published in Solar Energy Materials and Solar Cells. OpenAlex counts 102 citations as of 16 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
102
Most cited in
2016 (6)
Field-weighted impact
2.02
References
3
Authors
4

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Yamamoto, Y., Saito, K., Takahashi, K., & Konagai, M. (2001). Preparation of boron-doped ZnO thin films by photo-atomic layer deposition. Solar Energy Materials and Solar Cells, 65(1-4), 125–132. https://doi.org/10.1016/s0927-0248(00)00086-6

MLA 9

Yamamoto, Yukio, et al. “Preparation of boron-doped ZnO thin films by photo-atomic layer deposition.” Solar Energy Materials and Solar Cells, vol. 65, no. 1-4, 2001, pp. 125–132. https://doi.org/10.1016/s0927-0248(00)00086-6.

Chicago

Yamamoto, Yukio, K. Saito, Kiyoshi Takahashi, and Makoto Konagai. 2001. “Preparation of boron-doped ZnO thin films by photo-atomic layer deposition.” Solar Energy Materials and Solar Cells 65 (1-4): 125–132. https://doi.org/10.1016/s0927-0248(00)00086-6.

Harvard

Yamamoto, Y. et al. (2001) ‘Preparation of boron-doped ZnO thin films by photo-atomic layer deposition’, Solar Energy Materials and Solar Cells, 65(1-4), pp. 125–132. doi:10.1016/s0927-0248(00)00086-6.

IEEE

Y. Yamamoto, K. Saito, K. Takahashi, and M. Konagai, “Preparation of boron-doped ZnO thin films by photo-atomic layer deposition,” Solar Energy Materials and Solar Cells, vol. 65, no. 1-4, pp. 125–132, 2001, doi: 10.1016/s0927-0248(00)00086-6.

BibTeX

@article{yamamoto2001preparation,
  title     = {{Preparation of boron-doped ZnO thin films by photo-atomic layer deposition}},
  author    = {Yamamoto, Yukio and Saito, K. and Takahashi, Kiyoshi and Konagai, Makoto},
  journal   = {Solar Energy Materials and Solar Cells},
  year      = {2001},
  volume    = {65},
  number    = {1-4},
  pages     = {125--132},
  doi       = {10.1016/s0927-0248(00)00086-6},
  url       = {https://doi.org/10.1016/s0927-0248(00)00086-6}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
201666
201733
201866
201966
202011
202144
202211
202322
202422
202522

Its field-weighted citation impact is 2.02: it has been cited 2.02 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Materials Science › Materials Chemistry › ZnO doping and properties

  • boron-doped ZnO
  • thin films
  • UV irradiation
  • n-type doping
  • diborane
  • electrical resistivity
  • film growth mechanism
  • air stability

Work with this paper

Most-cited papers in Materials Science

All highly cited Materials Science papers

Questions about this paper

How do I cite this paper in APA style?

Yamamoto, Y., Saito, K., Takahashi, K., & Konagai, M. (2001). Preparation of boron-doped ZnO thin films by photo-atomic layer deposition. Solar Energy Materials and Solar Cells, 65(1-4), 125–132. https://doi.org/10.1016/s0927-0248(00)00086-6

How many times has this paper been cited?

102 times, according to OpenAlex on 16 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Yukio Yamamoto, K. Saito, Kiyoshi Takahashi, Makoto Konagai.

What is the DOI of this paper?

10.1016/s0927-0248(00)00086-6. The permanent link is https://doi.org/10.1016/s0927-0248(00)00086-6.

Bibliographic data from OpenAlex (CC0), last checked 16 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.