Journal article · 2023 · Open access

Oxidation and wear behavior of CrAlMoN with varied Mo-content for cutting Ti6Al4V

Kirsten Bobzin, C. Kalscheuer, Nina Stachowski, Jan Hendrik Dege, Wolfgang Hintze, Carsten Möller, P. Ploog

Production Engineering, 18(1), 87–97 · Published 3 August 2023 · DOI 10.1007/s11740-023-01218-2

Open PDFView at the publisherCite this paper

In brief

“Oxidation and wear behavior of CrAlMoN with varied Mo-content for cutting Ti6Al4V” is a 2023 journal article by Kirsten Bobzin and 6 co-authors, published in Production Engineering. OpenAlex counts 2 citations as of 17 November 2026. It is open access under a CC BY licence: the full text is free to read at Production Engineering.

Citations
2
Most cited in
2024 (1)
Field-weighted impact
0.20
References
23
Authors
7

Abstract

The cutting of difficult to machine materials such as titanium alloys is challenging for the machining industry. In case of the titanium alloy Ti6Al4V, the properties of the material cause high temperatures, mechanical loads as well as high frequency vibrations at the cutting edge, leading to premature tool failure. The use of uncoated carbide tools is very common for machining of Ti based alloys. However, temperature active, self-lubricating physical vapor deposition (PVD) coatings like CrAlMoN showed promising results to reduce friction and wear during turning of Ti6Al4V. In the present study, self-lubricating (Cr34Al41Mo25)N, (Cr29Al36Mo35)N and (Cr25Al31Mo44)N coatings were investigated on cemented carbide tools. These were deposited by a hybrid process combining direct current Magnetron Sputtering and High Power Pulsed Magnetron Sputtering. Coating morphology, thickness, chemical composition, indentation hardness and modulus at ϑ = 20 °C, ϑ = 200 °C, ϑ = 400 °C and ϑ = 600 °C as well as the oxidation behavior were analyzed. Moreover, wear development after cutting tests using a CNC-lathe was investigated. Independent of Mo-content, all coating variants possessed a dense morphology and a smooth surface topography, as well as a coating adhesion class of HF1 to the cemented carbide substrate in Rockwell indentation tests according to DIN 4856. With an increasing amount of Mo, heat treatment temperature and time, more self-lubricating molybdenum oxides such as MoO3 and Mo4O11 were detected by Raman spectroscopy. Therefore, the coating with the highest amount of Mo possessed the highest amount of molybdenum oxides. After cutting tests, molybdenum oxides were also found on the tool flank face by Raman spectroscopy. The level of flank wear land width decreased with increasing amount of Mo.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Bobzin, K., Kalscheuer, C., Stachowski, N., Dege, J. H., Hintze, W., Möller, C., & Ploog, P. (2023). Oxidation and wear behavior of CrAlMoN with varied Mo-content for cutting Ti6Al4V. Production Engineering, 18(1), 87–97. https://doi.org/10.1007/s11740-023-01218-2

MLA 9

Bobzin, Kirsten, et al. “Oxidation and wear behavior of CrAlMoN with varied Mo-content for cutting Ti6Al4V.” Production Engineering, vol. 18, no. 1, 2023, pp. 87–97. https://doi.org/10.1007/s11740-023-01218-2.

Chicago

Bobzin, Kirsten, C. Kalscheuer, Nina Stachowski, Jan Hendrik Dege, Wolfgang Hintze, Carsten Möller, and P. Ploog. 2023. “Oxidation and wear behavior of CrAlMoN with varied Mo-content for cutting Ti6Al4V.” Production Engineering 18 (1): 87–97. https://doi.org/10.1007/s11740-023-01218-2.

Harvard

Bobzin, K. et al. (2023) ‘Oxidation and wear behavior of CrAlMoN with varied Mo-content for cutting Ti6Al4V’, Production Engineering, 18(1), pp. 87–97. doi:10.1007/s11740-023-01218-2.

IEEE

K. Bobzin et al., “Oxidation and wear behavior of CrAlMoN with varied Mo-content for cutting Ti6Al4V,” Production Engineering, vol. 18, no. 1, pp. 87–97, 2023, doi: 10.1007/s11740-023-01218-2.

BibTeX

@article{bobzin2023oxidation,
  title     = {{Oxidation and wear behavior of CrAlMoN with varied Mo-content for cutting Ti6Al4V}},
  author    = {Bobzin, Kirsten and Kalscheuer, C. and Stachowski, Nina and Dege, Jan Hendrik and Hintze, Wolfgang and Möller, Carsten and Ploog, P.},
  journal   = {Production Engineering},
  year      = {2023},
  volume    = {18},
  number    = {1},
  pages     = {87--97},
  doi       = {10.1007/s11740-023-01218-2},
  url       = {https://doi.org/10.1007/s11740-023-01218-2}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Topic and keywords

Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics

  • Ti-6Al-4V
  • titanium alloy machining
  • self-lubricating coatings
  • molybdenum content
  • oxidation behavior
  • tool wear
  • cemented carbide tools
  • high power impulse magnetron sputtering

Work with this paper

Most-cited papers in Engineering

All highly cited Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Bobzin, K., Kalscheuer, C., Stachowski, N., Dege, J. H., Hintze, W., Möller, C., & Ploog, P. (2023). Oxidation and wear behavior of CrAlMoN with varied Mo-content for cutting Ti6Al4V. Production Engineering, 18(1), 87–97. https://doi.org/10.1007/s11740-023-01218-2

How many times has this paper been cited?

2 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

Yes. It is open access at Production Engineering: sign in and open the PDF from this page.

Who wrote this paper?

Kirsten Bobzin, C. Kalscheuer, Nina Stachowski, Jan Hendrik Dege, Wolfgang Hintze, Carsten Möller, P. Ploog.

What is the DOI of this paper?

10.1007/s11740-023-01218-2, permanently at https://doi.org/10.1007/s11740-023-01218-2. Sign in and open it from this page.

Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.