Conference paper · 2016 · Open access

Nanoindentation Response of Polycrystalline Graphene by Atomistic Simulations

Ying Ching Lu, Jin Wen Qian

Annual International Conference on Advanced Material Engineering (AME) · Published 1 January 2016 · DOI 10.2991/ame-16.2016.36

Free PDFView at the publisherCite this paper

In brief

“Nanoindentation Response of Polycrystalline Graphene by Atomistic Simulations” is a 2016 conference paper by Ying Ching Lu and Jin Wen Qian, published in Annual International Conference on Advanced Material Engineering (AME). OpenAlex counts 0 citations as of 15 November 2026. It is open access under a CC BY-NC licence: the full text is free to read at Annual International Conference on Advanced Material Engineering (AME).

Citations
0
References
17
Authors
2

Abstract

Nanoindentation has been widely used to determine the mechanical properties of pristine and polycrystalline graphene in experiments.To investigate the effects of grain size on the mechanical properties of polycrystalline graphene, we use molecular dynamics simulations to study the nanoindentation response of suspended polycrystalline graphene layer.The force-displacement behavior from the simulations enables the interpretation of Young's modulus and breaking strength of the 2D material, which are exhibited to strongly depend on the grain size.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Lu, Y. C., & Qian, J. W. (2016). Nanoindentation Response of Polycrystalline Graphene by Atomistic Simulations. Annual International Conference on Advanced Material Engineering (AME). https://doi.org/10.2991/ame-16.2016.36

MLA 9

Lu, Ying Ching, and Jin Wen Qian. “Nanoindentation Response of Polycrystalline Graphene by Atomistic Simulations.” Annual International Conference on Advanced Material Engineering (AME), 2016. https://doi.org/10.2991/ame-16.2016.36.

Chicago

Lu, Ying Ching and Jin Wen Qian. 2016. “Nanoindentation Response of Polycrystalline Graphene by Atomistic Simulations.” Annual International Conference on Advanced Material Engineering (AME). https://doi.org/10.2991/ame-16.2016.36.

Harvard

Lu, Y. C. and Qian, J. W. (2016) ‘Nanoindentation Response of Polycrystalline Graphene by Atomistic Simulations’, Annual International Conference on Advanced Material Engineering (AME). doi:10.2991/ame-16.2016.36.

IEEE

Y. C. Lu and J. W. Qian, “Nanoindentation Response of Polycrystalline Graphene by Atomistic Simulations,” Annual International Conference on Advanced Material Engineering (AME), 2016, doi: 10.2991/ame-16.2016.36.

BibTeX

@inproceedings{lu2016nanoindentation,
  title     = {{Nanoindentation Response of Polycrystalline Graphene by Atomistic Simulations}},
  author    = {Lu, Ying Ching and Qian, Jin Wen},
  booktitle = {Annual International Conference on Advanced Material Engineering (AME)},
  year      = {2016},
  doi       = {10.2991/ame-16.2016.36},
  url       = {https://doi.org/10.2991/ame-16.2016.36}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Topic and keywords

Physical Sciences › Materials Science › Materials Chemistry › Graphene research and applications

  • polycrystalline graphene
  • nanoindentation
  • grain size effects
  • mechanical properties
  • Young's modulus
  • breaking strength
  • force-displacement behavior
  • two-dimensional materials

Work with this paper

Most-cited papers in Materials Science

All highly cited Materials Science papers

Questions about this paper

How do I cite this paper in APA style?

Lu, Y. C., & Qian, J. W. (2016). Nanoindentation Response of Polycrystalline Graphene by Atomistic Simulations. Annual International Conference on Advanced Material Engineering (AME). https://doi.org/10.2991/ame-16.2016.36

How many times has this paper been cited?

0 times, according to OpenAlex on 15 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

Yes. It is open access: read the free full text at Annual International Conference on Advanced Material Engineering (AME).

Who wrote this paper?

Ying Ching Lu, Jin Wen Qian.

What is the DOI of this paper?

10.2991/ame-16.2016.36. The permanent link is https://doi.org/10.2991/ame-16.2016.36.

Bibliographic data from OpenAlex (CC0), last checked 15 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.