Paper · 2014
Nanoindentation of Hard Coatings
Published 1 January 2014
In brief
“Nanoindentation of Hard Coatings” is a 2014 paper by N. Consten. OpenAlex counts 0 citations as of 19 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.
- Citations
- 0
- References
- 8
- Authors
- 1
Abstract
Nanoindentation measurements were carried out using the coatings CrAlTiN, CrAlSiN (with high Cr/Al ratio), AlCrSiN (with low Cr/Al ratio) and CrAlN deposited by cathodic arc technology on tungsten carbide substrates. For this purposes use is made NanoTest Vantage Platform 4 of Micro Materials with a diamond Berkovich indenter. The maximum depth of penetration in a… Read the full abstract at the publisher.
Excerpt. This paper is not open access.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Consten, N. (2014). Nanoindentation of Hard Coatings. https://essay.utwente.nl/69336/1/Internship%20Report%20Niels%20Consten.pdf
MLA 9
Consten, N. “Nanoindentation of Hard Coatings.” 2014. https://essay.utwente.nl/69336/1/Internship%20Report%20Niels%20Consten.pdf.
Chicago
Consten, N. 2014. “Nanoindentation of Hard Coatings.” https://essay.utwente.nl/69336/1/Internship%20Report%20Niels%20Consten.pdf.
Harvard
Consten, N. (2014) ‘Nanoindentation of Hard Coatings’. Available at: https://essay.utwente.nl/69336/1/Internship%20Report%20Niels%20Consten.pdf.
IEEE
N. Consten, “Nanoindentation of Hard Coatings,” 2014.
BibTeX
@article{consten2014nanoindentation,
title = {{Nanoindentation of Hard Coatings}},
author = {Consten, N.},
year = {2014},
url = {https://essay.utwente.nl/69336/1/Internship%20Report%20Niels%20Consten.pdf}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Topic and keywords
Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics
- nanoindentation
- hard coatings
- CrAlN
- tungsten carbide substrate
- cathodic arc deposition
- hardness
- reduced Young's modulus
- load-displacement curve
Work with this paper
Most-cited papers in Engineering
- A Closed‐form Equation for Predicting the Hydraulic Conductivity of Unsaturated SoilsMartinus Th. van Genuchten · Soil Science Society of America Journal · 1980 · 28,197 citations
- An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experimentsW. C. Oliver, George M. Pharr · Journal of materials research/Pratt's guide to venture capital sources · 1992 · 27,379 citations
- Digital communicationsOwen Bishop · Routledge eBooks · 2007 · 24,890 citations
- The empirical mode decomposition and the Hilbert spectrum for nonlinear and non-stationary time series analysisNorden Eh Huang, Zhengwei Shen, Steven R. Long and 6 more · Proceedings of the Royal Society A Mathematical Physical and Engineering Sciences · 1998 · 24,008 citations
- Numerical Heat Transfer and Fluid FlowSuhas V. Patankar · CRC Press eBooks · 2018 · 23,491 citations
Questions about this paper
How do I cite this paper in APA style?
Consten, N. (2014). Nanoindentation of Hard Coatings. https://essay.utwente.nl/69336/1/Internship%20Report%20Niels%20Consten.pdf
How many times has this paper been cited?
0 times, according to OpenAlex on 19 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.
Who wrote this paper?
N. Consten.
Bibliographic data from OpenAlex (CC0), last checked 19 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.