Journal article · 2016
Nanoindentation of a hard ceramic coating formed on a soft substrate
Technical Physics, 61(9), 1370–1376 · Published 1 September 2016 · DOI 10.1134/s1063784216090279
In brief
“Nanoindentation of a hard ceramic coating formed on a soft substrate” is a 2016 journal article by Maria A. Surmeneva and 4 co-authors, published in Technical Physics. OpenAlex counts 3 citations as of 17 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.
- Citations
- 3
- Most cited in
- 2018 (1)
- Field-weighted impact
- 0.21
- References
- 27
- Authors
- 5
Abstract
The hardness and Young’s modulus of the thin hydroxyapatite-based coatings deposited by RF magnetron sputtering onto magnesium alloy, titanium, and steel substrates are studied. As the penetration depth increases, the hardness and Young’s modulus of these coatings are found to tend toward the values that are characteristic of the substrates. It is shown that the… Read the full abstract at the publisher.
Excerpt. This paper is not open access.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Surmeneva, M. A., Анатольевич, С. Р., Tyurin, A. I., Пирожкова, Т. С., & Александрович, Ш. И. (2016). Nanoindentation of a hard ceramic coating formed on a soft substrate. Technical Physics, 61(9), 1370–1376. https://doi.org/10.1134/s1063784216090279
MLA 9
Surmeneva, Maria A., et al. “Nanoindentation of a hard ceramic coating formed on a soft substrate.” Technical Physics, vol. 61, no. 9, 2016, pp. 1370–1376. https://doi.org/10.1134/s1063784216090279.
Chicago
Surmeneva, Maria A., Сурменев Роман Анатольевич, Alexander I. Tyurin, Т. С. Пирожкова, and Шуварин Иван Александрович. 2016. “Nanoindentation of a hard ceramic coating formed on a soft substrate.” Technical Physics 61 (9): 1370–1376. https://doi.org/10.1134/s1063784216090279.
Harvard
Surmeneva, M. A. et al. (2016) ‘Nanoindentation of a hard ceramic coating formed on a soft substrate’, Technical Physics, 61(9), pp. 1370–1376. doi:10.1134/s1063784216090279.
IEEE
M. A. Surmeneva, С. Р. Анатольевич, A. I. Tyurin, Т. С. Пирожкова, and Ш. И. Александрович, “Nanoindentation of a hard ceramic coating formed on a soft substrate,” Technical Physics, vol. 61, no. 9, pp. 1370–1376, 2016, doi: 10.1134/s1063784216090279.
BibTeX
@article{surmeneva2016nanoindentation,
title = {{Nanoindentation of a hard ceramic coating formed on a soft substrate}},
author = {Surmeneva, Maria A. and Анатольевич, Сурменев Роман and Tyurin, Alexander I. and Пирожкова, Т. С. and Александрович, Шуварин Иван},
journal = {Technical Physics},
year = {2016},
volume = {61},
number = {9},
pages = {1370--1376},
doi = {10.1134/s1063784216090279},
url = {https://doi.org/10.1134/s1063784216090279}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2018 | 1 | |
| 2020 | 1 | |
| 2021 | 1 |
Its field-weighted citation impact is 0.21: it has been cited 0.21 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics
- nanoindentation
- hydroxyapatite coating
- ceramic coatings
- hardness
- Young's modulus
- penetration depth
- substrate effects
- RF magnetron sputtering
Work with this paper
Most-cited papers in Engineering
- A Closed‐form Equation for Predicting the Hydraulic Conductivity of Unsaturated SoilsMartinus Th. van Genuchten · Soil Science Society of America Journal · 1980 · 28,197 citations
- An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experimentsW. C. Oliver, George M. Pharr · Journal of materials research/Pratt's guide to venture capital sources · 1992 · 27,379 citations
- Digital communicationsOwen Bishop · Routledge eBooks · 2007 · 24,890 citations
- The empirical mode decomposition and the Hilbert spectrum for nonlinear and non-stationary time series analysisNorden Eh Huang, Zhengwei Shen, Steven R. Long and 6 more · Proceedings of the Royal Society A Mathematical Physical and Engineering Sciences · 1998 · 24,008 citations
- Numerical Heat Transfer and Fluid FlowSuhas V. Patankar · CRC Press eBooks · 2018 · 23,491 citations
Questions about this paper
How do I cite this paper in APA style?
Surmeneva, M. A., Анатольевич, С. Р., Tyurin, A. I., Пирожкова, Т. С., & Александрович, Ш. И. (2016). Nanoindentation of a hard ceramic coating formed on a soft substrate. Technical Physics, 61(9), 1370–1376. https://doi.org/10.1134/s1063784216090279
How many times has this paper been cited?
3 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.
Who wrote this paper?
Maria A. Surmeneva, Сурменев Роман Анатольевич, Alexander I. Tyurin, Т. С. Пирожкова, Шуварин Иван Александрович.
What is the DOI of this paper?
10.1134/s1063784216090279, permanently at https://doi.org/10.1134/s1063784216090279. Sign in and open it from this page.
Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.