Nanoindentation of a circular sheet of bilayer graphene
Physical Review B, 81(23) · Published 11 June 2010 · DOI 10.1103/physrevb.81.235421
In brief
“Nanoindentation of a circular sheet of bilayer graphene” is a 2010 journal article by M. Neek-Amal and François Maria Peeters, published in Physical Review B. OpenAlex counts 147 citations as of 15 November 2026, which puts it in the top 4% of works published in 2010 by citations. It is open access: the full text is free to read at arXiv (Cornell University).
- Citations
- 147
- Most cited in
- 2018 (16)
- Field-weighted impact
- 3.36
- References
- 25
- Authors
- 2
Abstract
Nanoindentation of bilayer graphene is studied using molecular-dynamics simulations. We compared our simulation results with those from elasticity theory as based on the nonlinear F\"oppl-Hencky equations with rigid boundary condition. The force-deflection values of bilayer graphene are compared to those of monolayer graphene. Young's modulus of bilayer graphene is estimated to be 0.8 TPa which is close to the value for graphite. Moreover, an almost flat bilayer membrane at low temperature under central load has a 14% smaller Young's modulus as compared to the one at room temperature.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Neek-Amal, M., & Peeters, F. M. (2010). Nanoindentation of a circular sheet of bilayer graphene. Physical Review B, 81(23). https://doi.org/10.1103/physrevb.81.235421
MLA 9
Neek-Amal, M., and François Maria Peeters. “Nanoindentation of a circular sheet of bilayer graphene.” Physical Review B, vol. 81, no. 23, 2010. https://doi.org/10.1103/physrevb.81.235421.
Chicago
Neek-Amal, M. and François Maria Peeters. 2010. “Nanoindentation of a circular sheet of bilayer graphene.” Physical Review B 81 (23). https://doi.org/10.1103/physrevb.81.235421.
Harvard
Neek-Amal, M. and Peeters, F. M. (2010) ‘Nanoindentation of a circular sheet of bilayer graphene’, Physical Review B, 81(23). doi:10.1103/physrevb.81.235421.
IEEE
M. Neek-Amal and F. M. Peeters, “Nanoindentation of a circular sheet of bilayer graphene,” Physical Review B, vol. 81, no. 23, 2010, doi: 10.1103/physrevb.81.235421.
BibTeX
@article{neekamal2010nanoindentation,
title = {{Nanoindentation of a circular sheet of bilayer graphene}},
author = {Neek-Amal, M. and Peeters, François Maria},
journal = {Physical Review B},
year = {2010},
volume = {81},
number = {23},
doi = {10.1103/physrevb.81.235421},
url = {https://doi.org/10.1103/physrevb.81.235421}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2017 | 10 | |
| 2018 | 16 | |
| 2019 | 11 | |
| 2020 | 13 | |
| 2021 | 10 | |
| 2022 | 8 | |
| 2023 | 5 | |
| 2024 | 4 | |
| 2025 | 8 | |
| 2026 | 7 |
Its field-weighted citation impact is 3.36: it has been cited 3.36 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Materials Science › Materials Chemistry › Graphene research and applications
- bilayer graphene
- nanoindentation
- Young's modulus
- load-deflection behavior
- rigid boundary conditions
- monolayer graphene
- temperature dependence
Work with this paper
Most-cited papers in Materials Science
- Electric Field Effect in Atomically Thin Carbon FilmsKostya S. Novoselov, Andre K. Geim, Sergey V. Morozov and 5 more · Science · 2004 · 67,474 citations
- Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenidesROBERT D. SHANNON · Acta Crystallographica Section A · 1976 · 66,944 citations
- Ab initio molecular dynamics for liquid metalsGeorg Kresse, J. Häfner · Physical review. B, Condensed matter · 1993 · 46,320 citations
- Helical microtubules of graphitic carbonSumio Iijima · Nature · 1991 · 43,639 citations
- The rise of grapheneAndre K. Geim, Kostya S. Novoselov · Nature Materials · 2007 · 40,328 citations
Questions about this paper
How do I cite this paper in APA style?
Neek-Amal, M., & Peeters, F. M. (2010). Nanoindentation of a circular sheet of bilayer graphene. Physical Review B, 81(23). https://doi.org/10.1103/physrevb.81.235421
How many times has this paper been cited?
147 times, according to OpenAlex on 15 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access: read the free full text at arXiv (Cornell University).
Who wrote this paper?
M. Neek-Amal, François Maria Peeters.
What is the DOI of this paper?
10.1103/physrevb.81.235421. The permanent link is https://doi.org/10.1103/physrevb.81.235421.
Bibliographic data from OpenAlex (CC0), last checked 15 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.