Nanoindentation Models of Monolayer Graphene and Graphyne under Point Load Pattern Studied by Molecular Dynamics

Lang Xiang, Jian Wu, Shuangying Ma, Fang Wang, Kaiwang Zhang

Chinese Physics Letters, 32(9), 096801 · Published 1 September 2015 · DOI 10.1088/0256-307x/32/9/096801

View at the publisherCite this paper

In brief

“Nanoindentation Models of Monolayer Graphene and Graphyne under Point Load Pattern Studied by Molecular Dynamics” is a 2015 journal article by Lang Xiang and 4 co-authors, published in Chinese Physics Letters. OpenAlex counts 10 citations as of 15 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
10
Most cited in
2020 (3)
Field-weighted impact
0.46
References
30
Authors
5

Abstract

Molecular dynamics simulations are performed to study the nanoindentation models of monolayer suspended graphene and graphyne. Fullerenes are selected as indenters. Our results show that Young's modulus of monolayer-thick graphyne is almost half of that of graphene, which is estimated to be 0.50 TPa. The mechanical properties of graphene and graphyne are different in the… Read the full abstract at the publisher.

Excerpt. This paper is not open access.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Xiang, L., Wu, J., Ma, S., Wang, F., & Zhang, K. (2015). Nanoindentation Models of Monolayer Graphene and Graphyne under Point Load Pattern Studied by Molecular Dynamics. Chinese Physics Letters, 32(9), 096801. https://doi.org/10.1088/0256-307x/32/9/096801

MLA 9

Xiang, Lang, et al. “Nanoindentation Models of Monolayer Graphene and Graphyne under Point Load Pattern Studied by Molecular Dynamics.” Chinese Physics Letters, vol. 32, no. 9, 2015, p. 096801. https://doi.org/10.1088/0256-307x/32/9/096801.

Chicago

Xiang, Lang, Jian Wu, Shuangying Ma, Fang Wang, and Kaiwang Zhang. 2015. “Nanoindentation Models of Monolayer Graphene and Graphyne under Point Load Pattern Studied by Molecular Dynamics.” Chinese Physics Letters 32 (9): 096801. https://doi.org/10.1088/0256-307x/32/9/096801.

Harvard

Xiang, L. et al. (2015) ‘Nanoindentation Models of Monolayer Graphene and Graphyne under Point Load Pattern Studied by Molecular Dynamics’, Chinese Physics Letters, 32(9), p. 096801. doi:10.1088/0256-307x/32/9/096801.

IEEE

L. Xiang, J. Wu, S. Ma, F. Wang, and K. Zhang, “Nanoindentation Models of Monolayer Graphene and Graphyne under Point Load Pattern Studied by Molecular Dynamics,” Chinese Physics Letters, vol. 32, no. 9, p. 096801, 2015, doi: 10.1088/0256-307x/32/9/096801.

BibTeX

@article{xiang2015nanoindentation,
  title     = {{Nanoindentation Models of Monolayer Graphene and Graphyne under Point Load Pattern Studied by Molecular Dynamics}},
  author    = {Xiang, Lang and Wu, Jian and Ma, Shuangying and Wang, Fang and Zhang, Kaiwang},
  journal   = {Chinese Physics Letters},
  year      = {2015},
  volume    = {32},
  number    = {9},
  pages     = {096801},
  doi       = {10.1088/0256-307x/32/9/096801},
  url       = {https://doi.org/10.1088/0256-307x/32/9/096801}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
201611
201722
201811
201911
202033
202222

Its field-weighted citation impact is 0.46: it has been cited 0.46 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Materials Science › Materials Chemistry › Graphene research and applications

  • nanoindentation
  • monolayer graphene
  • graphyne
  • suspended graphene
  • Young's modulus
  • pretension
  • strain effects
  • toughness

Work with this paper

Most-cited papers in Materials Science

All highly cited Materials Science papers

Questions about this paper

How do I cite this paper in APA style?

Xiang, L., Wu, J., Ma, S., Wang, F., & Zhang, K. (2015). Nanoindentation Models of Monolayer Graphene and Graphyne under Point Load Pattern Studied by Molecular Dynamics. Chinese Physics Letters, 32(9), 096801. https://doi.org/10.1088/0256-307x/32/9/096801

How many times has this paper been cited?

10 times, according to OpenAlex on 15 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Lang Xiang, Jian Wu, Shuangying Ma, Fang Wang, Kaiwang Zhang.

What is the DOI of this paper?

10.1088/0256-307x/32/9/096801. The permanent link is https://doi.org/10.1088/0256-307x/32/9/096801.

Bibliographic data from OpenAlex (CC0), last checked 15 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.