Journal article · 1998

Nanoindentation hardness, abrasive wear, and microstructure of TiN/NbN polycrystalline nanostructured multilayer films grown by reactive magnetron sputtering

Henrik Ljungcrantz, C. Engström, Lars Hultman, Maryam K. Olsson, Xiaoyu Chu, Ming‐Show Wong, W.D. Sproul

Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 16(5), 3104–3113 · Published 1 September 1998 · DOI 10.1116/1.581466

View at the publisherCite this paper

In brief

“Nanoindentation hardness, abrasive wear, and microstructure of TiN/NbN polycrystalline nanostructured multilayer films grown by reactive magnetron sputtering” is a 1998 journal article by Henrik Ljungcrantz and 6 co-authors, published in Journal of Vacuum Science & Technology A Vacuum Surfaces and Films. OpenAlex counts 85 citations as of 17 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
85
Most cited in
2014 (3)
Field-weighted impact
12.63
References
33
Authors
7

Abstract

TiN, NbN, and TiN/NbN polycrystalline nanostructured multilayer films were deposited on high-speed steel substrates by unbalanced reactive magnetron sputtering of Ti and Nb targets in Ar–N2 discharges. Two techniques were used for obtaining a series of multilayers with compositional modulation period, Λ, in the range 3.8–100 nm; rotation of a cylindrical substrate holder between two… Read the full abstract at the publisher.

Excerpt. This paper is not open access.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Ljungcrantz, H., Engström, C., Hultman, L., Olsson, M. K., Chu, X., Wong, M., & Sproul, W. (1998). Nanoindentation hardness, abrasive wear, and microstructure of TiN/NbN polycrystalline nanostructured multilayer films grown by reactive magnetron sputtering. Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 16(5), 3104–3113. https://doi.org/10.1116/1.581466

MLA 9

Ljungcrantz, Henrik, et al. “Nanoindentation hardness, abrasive wear, and microstructure of TiN/NbN polycrystalline nanostructured multilayer films grown by reactive magnetron sputtering.” Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, vol. 16, no. 5, 1998, pp. 3104–3113. https://doi.org/10.1116/1.581466.

Chicago

Ljungcrantz, Henrik, C. Engström, Lars Hultman, Maryam K. Olsson, Xiaoyu Chu, Ming‐Show Wong, and W.D. Sproul. 1998. “Nanoindentation hardness, abrasive wear, and microstructure of TiN/NbN polycrystalline nanostructured multilayer films grown by reactive magnetron sputtering.” Journal of Vacuum Science & Technology A Vacuum Surfaces and Films 16 (5): 3104–3113. https://doi.org/10.1116/1.581466.

Harvard

Ljungcrantz, H. et al. (1998) ‘Nanoindentation hardness, abrasive wear, and microstructure of TiN/NbN polycrystalline nanostructured multilayer films grown by reactive magnetron sputtering’, Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 16(5), pp. 3104–3113. doi:10.1116/1.581466.

IEEE

H. Ljungcrantz et al., “Nanoindentation hardness, abrasive wear, and microstructure of TiN/NbN polycrystalline nanostructured multilayer films grown by reactive magnetron sputtering,” Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, vol. 16, no. 5, pp. 3104–3113, 1998, doi: 10.1116/1.581466.

BibTeX

@article{ljungcrantz1998nanoindentation,
  title     = {{Nanoindentation hardness, abrasive wear, and microstructure of TiN/NbN polycrystalline nanostructured multilayer films grown by reactive magnetron sputtering}},
  author    = {Ljungcrantz, Henrik and Engström, C. and Hultman, Lars and Olsson, Maryam K. and Chu, Xiaoyu and Wong, Ming‐Show and Sproul, W.D.},
  journal   = {Journal of Vacuum Science \& Technology A Vacuum Surfaces and Films},
  year      = {1998},
  volume    = {16},
  number    = {5},
  pages     = {3104--3113},
  doi       = {10.1116/1.581466},
  url       = {https://doi.org/10.1116/1.581466}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
201433
201522
201711
201822
201922
202011
202111
202211
202322
202511

Its field-weighted citation impact is 12.63: it has been cited 12.63 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics

  • reactive magnetron sputtering
  • nanohardness
  • abrasive wear resistance
  • residual stress
  • grain size
  • substrate bias
  • high-speed steel substrates

Work with this paper

Most-cited papers in Engineering

All highly cited Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Ljungcrantz, H., Engström, C., Hultman, L., Olsson, M. K., Chu, X., Wong, M., & Sproul, W. (1998). Nanoindentation hardness, abrasive wear, and microstructure of TiN/NbN polycrystalline nanostructured multilayer films grown by reactive magnetron sputtering. Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 16(5), 3104–3113. https://doi.org/10.1116/1.581466

How many times has this paper been cited?

85 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Henrik Ljungcrantz, C. Engström, Lars Hultman, Maryam K. Olsson, Xiaoyu Chu, Ming‐Show Wong, W.D. Sproul.

What is the DOI of this paper?

10.1116/1.581466, permanently at https://doi.org/10.1116/1.581466. Sign in and open it from this page.

Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.