In brief

“Nanoindentation and Tribological Behavior of TiN-TiCN-TiAlN Multilayer Coatings on AISI D3 Tool Steel” is a 2022 journal article by AmirReza Naghashzadeh and 2 co-authors, published in Journal of Materials Engineering and Performance. OpenAlex counts 33 citations as of 17 November 2026, which puts it in the top 7% of works published in 2022 by citations. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
33
Most cited in
2025 (9)
Field-weighted impact
2.44
References
36
Authors
3

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Naghashzadeh, A., Shafyei, A., & Sourani, F. (2022). Nanoindentation and Tribological Behavior of TiN-TiCN-TiAlN Multilayer Coatings on AISI D3 Tool Steel. Journal of Materials Engineering and Performance, 31(6), 4335–4342. https://doi.org/10.1007/s11665-021-06533-2

MLA 9

Naghashzadeh, AmirReza, et al. “Nanoindentation and Tribological Behavior of TiN-TiCN-TiAlN Multilayer Coatings on AISI D3 Tool Steel.” Journal of Materials Engineering and Performance, vol. 31, no. 6, 2022, pp. 4335–4342. https://doi.org/10.1007/s11665-021-06533-2.

Chicago

Naghashzadeh, AmirReza, Ali Shafyei, and Fereshteh Sourani. 2022. “Nanoindentation and Tribological Behavior of TiN-TiCN-TiAlN Multilayer Coatings on AISI D3 Tool Steel.” Journal of Materials Engineering and Performance 31 (6): 4335–4342. https://doi.org/10.1007/s11665-021-06533-2.

Harvard

Naghashzadeh, A., Shafyei, A. and Sourani, F. (2022) ‘Nanoindentation and Tribological Behavior of TiN-TiCN-TiAlN Multilayer Coatings on AISI D3 Tool Steel’, Journal of Materials Engineering and Performance, 31(6), pp. 4335–4342. doi:10.1007/s11665-021-06533-2.

IEEE

A. Naghashzadeh, A. Shafyei, and F. Sourani, “Nanoindentation and Tribological Behavior of TiN-TiCN-TiAlN Multilayer Coatings on AISI D3 Tool Steel,” Journal of Materials Engineering and Performance, vol. 31, no. 6, pp. 4335–4342, 2022, doi: 10.1007/s11665-021-06533-2.

BibTeX

@article{naghashzadeh2022nanoindentation,
  title     = {{Nanoindentation and Tribological Behavior of TiN-TiCN-TiAlN Multilayer Coatings on AISI D3 Tool Steel}},
  author    = {Naghashzadeh, AmirReza and Shafyei, Ali and Sourani, Fereshteh},
  journal   = {Journal of Materials Engineering and Performance},
  year      = {2022},
  volume    = {31},
  number    = {6},
  pages     = {4335--4342},
  doi       = {10.1007/s11665-021-06533-2},
  url       = {https://doi.org/10.1007/s11665-021-06533-2}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
202233
202377
202477
202599
202677

Its field-weighted citation impact is 2.44: it has been cited 2.44 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics

  • AISI D3 tool steel
  • cathodic arc physical vapor deposition
  • nanoindentation
  • hardness
  • elastic modulus
  • tribological properties
  • friction coefficient
  • wear resistance

Work with this paper

Most-cited papers in Engineering

All highly cited Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Naghashzadeh, A., Shafyei, A., & Sourani, F. (2022). Nanoindentation and Tribological Behavior of TiN-TiCN-TiAlN Multilayer Coatings on AISI D3 Tool Steel. Journal of Materials Engineering and Performance, 31(6), 4335–4342. https://doi.org/10.1007/s11665-021-06533-2

How many times has this paper been cited?

33 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

AmirReza Naghashzadeh, Ali Shafyei, Fereshteh Sourani.

What is the DOI of this paper?

10.1007/s11665-021-06533-2, permanently at https://doi.org/10.1007/s11665-021-06533-2. Sign in and open it from this page.

Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.