Conference paper · 2013

Molecular dynamics simulation of nanoindentation for single-layer rectangular graphene film

Weidong Wang, Yongjie Zhan, Minglin Li

IEEE International Conference on Nano/Micro Engineered and Molecular Systems, 1240–1243 · Published 1 April 2013 · DOI 10.1109/nems.2013.6559943

View at the publisherCite this paper

In brief

“Molecular dynamics simulation of nanoindentation for single-layer rectangular graphene film” is a 2013 conference paper by Weidong Wang and 2 co-authors, published in IEEE International Conference on Nano/Micro Engineered and Molecular Systems. OpenAlex counts 2 citations as of 15 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
2
Most cited in
2017 (1)
References
24
Authors
3

Abstract

Base on Tersoff and Lernnard-Jones potentials, molecular dynamics simulation of nanoindentation experiment on single layer rectangular graphene film is carried out. A typical force-displacement curve is obtained and the effects of various factors including indenter radius, velocities as well as boundary conditions on the simulation results are discussed. The Young's modulus and the strength of… Read the full abstract at the publisher.

Excerpt. This paper is not open access.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Wang, W., Zhan, Y., & Li, M. (2013). Molecular dynamics simulation of nanoindentation for single-layer rectangular graphene film. IEEE International Conference on Nano/Micro Engineered and Molecular Systems, 1240–1243. https://doi.org/10.1109/nems.2013.6559943

MLA 9

Wang, Weidong, et al. “Molecular dynamics simulation of nanoindentation for single-layer rectangular graphene film.” IEEE International Conference on Nano/Micro Engineered and Molecular Systems, 2013, pp. 1240–1243. https://doi.org/10.1109/nems.2013.6559943.

Chicago

Wang, Weidong, Yongjie Zhan, and Minglin Li. 2013. “Molecular dynamics simulation of nanoindentation for single-layer rectangular graphene film.” IEEE International Conference on Nano/Micro Engineered and Molecular Systems: 1240–1243. https://doi.org/10.1109/nems.2013.6559943.

Harvard

Wang, W., Zhan, Y. and Li, M. (2013) ‘Molecular dynamics simulation of nanoindentation for single-layer rectangular graphene film’, IEEE International Conference on Nano/Micro Engineered and Molecular Systems, pp. 1240–1243. doi:10.1109/nems.2013.6559943.

IEEE

W. Wang, Y. Zhan, and M. Li, “Molecular dynamics simulation of nanoindentation for single-layer rectangular graphene film,” IEEE International Conference on Nano/Micro Engineered and Molecular Systems, pp. 1240–1243, 2013, doi: 10.1109/nems.2013.6559943.

BibTeX

@inproceedings{wang2013molecular,
  title     = {{Molecular dynamics simulation of nanoindentation for single-layer rectangular graphene film}},
  author    = {Wang, Weidong and Zhan, Yongjie and Li, Minglin},
  booktitle = {IEEE International Conference on Nano/Micro Engineered and Molecular Systems},
  year      = {2013},
  pages     = {1240--1243},
  doi       = {10.1109/nems.2013.6559943},
  url       = {https://doi.org/10.1109/nems.2013.6559943}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Topic and keywords

Physical Sciences › Materials Science › Materials Chemistry › Graphene research and applications

  • nanoindentation
  • monolayer graphene
  • Tersoff potential
  • Lennard-Jones potential
  • force-displacement curves
  • indenter radius
  • boundary conditions
  • Young's modulus

Work with this paper

Most-cited papers in Materials Science

All highly cited Materials Science papers

Questions about this paper

How do I cite this paper in APA style?

Wang, W., Zhan, Y., & Li, M. (2013). Molecular dynamics simulation of nanoindentation for single-layer rectangular graphene film. IEEE International Conference on Nano/Micro Engineered and Molecular Systems, 1240–1243. https://doi.org/10.1109/nems.2013.6559943

How many times has this paper been cited?

2 times, according to OpenAlex on 15 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Weidong Wang, Yongjie Zhan, Minglin Li.

What is the DOI of this paper?

10.1109/nems.2013.6559943. The permanent link is https://doi.org/10.1109/nems.2013.6559943.

Bibliographic data from OpenAlex (CC0), last checked 15 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.