Mikrostrukturuntersuchungen an porösen Feststoffen durch Physisorptionsmessungen

Jürgen Seifert, Gerhard Emig

Chemie Ingenieur Technik, 59(6), 475–484 · Published 1 June 1987 · DOI 10.1002/cite.330590606

View at the publisherCite this paper

In brief

“Mikrostrukturuntersuchungen an porösen Feststoffen durch Physisorptionsmessungen” is a 1987 journal article by Jürgen Seifert and Gerhard Emig, published in Chemie Ingenieur Technik. OpenAlex counts 36 citations as of 15 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
36
Most cited in
2013 (2)
Field-weighted impact
1.28
References
36
Authors
2

Abstract

Studies of the microstructure of porous solids by physisorption measurements. The principal experimental methods for studying the microstructure of porous solids are based on physisorption measurements. The resulting sorption isotherms can yield data such as surface area and pore radius distribution, which are of great importance for development and characterization of porous catalysts. After a… Read the full abstract at the publisher.

Excerpt. This paper is not open access.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Seifert, J., & Emig, G. (1987). Mikrostrukturuntersuchungen an porösen Feststoffen durch Physisorptionsmessungen. Chemie Ingenieur Technik, 59(6), 475–484. https://doi.org/10.1002/cite.330590606

MLA 9

Seifert, Jürgen, and Gerhard Emig. “Mikrostrukturuntersuchungen an porösen Feststoffen durch Physisorptionsmessungen.” Chemie Ingenieur Technik, vol. 59, no. 6, 1987, pp. 475–484. https://doi.org/10.1002/cite.330590606.

Chicago

Seifert, Jürgen and Gerhard Emig. 1987. “Mikrostrukturuntersuchungen an porösen Feststoffen durch Physisorptionsmessungen.” Chemie Ingenieur Technik 59 (6): 475–484. https://doi.org/10.1002/cite.330590606.

Harvard

Seifert, J. and Emig, G. (1987) ‘Mikrostrukturuntersuchungen an porösen Feststoffen durch Physisorptionsmessungen’, Chemie Ingenieur Technik, 59(6), pp. 475–484. doi:10.1002/cite.330590606.

IEEE

J. Seifert and G. Emig, “Mikrostrukturuntersuchungen an porösen Feststoffen durch Physisorptionsmessungen,” Chemie Ingenieur Technik, vol. 59, no. 6, pp. 475–484, 1987, doi: 10.1002/cite.330590606.

BibTeX

@article{seifert1987mikrostrukturuntersuchungen,
  title     = {{Mikrostrukturuntersuchungen an porösen Feststoffen durch Physisorptionsmessungen}},
  author    = {Seifert, Jürgen and Emig, Gerhard},
  journal   = {Chemie Ingenieur Technik},
  year      = {1987},
  volume    = {59},
  number    = {6},
  pages     = {475--484},
  doi       = {10.1002/cite.330590606},
  url       = {https://doi.org/10.1002/cite.330590606}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
201322
201511
201622
201811
201922
202011
202511

Its field-weighted citation impact is 1.28: it has been cited 1.28 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Chemistry › Physical and Theoretical Chemistry › Adsorption, diffusion, and thermodynamic properties of materials

  • porous media
  • microstructure characterization
  • physisorption
  • sorption isotherms
  • surface area
  • pore size distribution
  • micropores
  • micropore volume

Work with this paper

Most-cited papers in Chemistry

All highly cited Chemistry papers

Questions about this paper

How do I cite this paper in APA style?

Seifert, J., & Emig, G. (1987). Mikrostrukturuntersuchungen an porösen Feststoffen durch Physisorptionsmessungen. Chemie Ingenieur Technik, 59(6), 475–484. https://doi.org/10.1002/cite.330590606

How many times has this paper been cited?

36 times, according to OpenAlex on 15 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Jürgen Seifert, Gerhard Emig.

What is the DOI of this paper?

10.1002/cite.330590606. The permanent link is https://doi.org/10.1002/cite.330590606.

Bibliographic data from OpenAlex (CC0), last checked 15 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.