Journal article · 2024 · Open access
Larger Recovery Strains in Cast Fe–Mn–Si‐Based Shape Memory Alloys by Reducing Thermal Activation and Optimizing Mn Content
Advanced Engineering Materials, 26(14), 2400475 · Published 16 June 2024 · DOI 10.1002/adem.202400475
In brief
“Larger Recovery Strains in Cast Fe–Mn–Si‐Based Shape Memory Alloys by Reducing Thermal Activation and Optimizing Mn Content” is a 2024 journal article by Yanni Luo and 4 co-authors, published in Advanced Engineering Materials. OpenAlex counts 5 citations as of 22 November 2026. It is open access under a CC BY licence: the full text is free to read at Advanced Engineering Materials.
- Citations
- 5
- Most cited in
- 2024 (3)
- Field-weighted impact
- 0.41
- References
- 43
- Authors
- 5
Abstract
Previous work shows that a maximal recovery strain of 8.4% after being bent at room temperature is realized in annealed cast polycrystalline Fe–Mn–Si‐based alloys because of the reduced annealing twin boundaries. Theoretically, higher recovery strains can be expected at cryogenic deformation by reducing thermal activation. To confirm this idea, martensitic transformation behaviors and the recovery strains after being bent at 77 K are investigated in the cast Fe–(20–26)Mn–5.5Si–8.5Cr–5Ni alloys. Herein, larger recovery strains as high as ≈10.0% are realized in an annealed cast Fe–23Mn–5.5Si–8.5Cr–5Ni alloy after being bent at 77 K. The reduced thermal activation together with suppressed formation of thermal‐induced martensite by optimizing Mn content can account for the larger recovery strain. In these results, a new avenue is opened up for further enhancement of the recovery strain in Fe–Mn–Si‐based shape memory alloys.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Luo, Y., Fu, Y., He, W., Peng, H., & Wen, Y. (2024). Larger Recovery Strains in Cast Fe–Mn–Si‐Based Shape Memory Alloys by Reducing Thermal Activation and Optimizing Mn Content. Advanced Engineering Materials, 26(14), 2400475. https://doi.org/10.1002/adem.202400475
MLA 9
Luo, Yanni, et al. “Larger Recovery Strains in Cast Fe–Mn–Si‐Based Shape Memory Alloys by Reducing Thermal Activation and Optimizing Mn Content.” Advanced Engineering Materials, vol. 26, no. 14, 2024, p. 2400475. https://doi.org/10.1002/adem.202400475.
Chicago
Luo, Yanni, Yu Fu, Wei He, Huabei Peng, and Yuhua Wen. 2024. “Larger Recovery Strains in Cast Fe–Mn–Si‐Based Shape Memory Alloys by Reducing Thermal Activation and Optimizing Mn Content.” Advanced Engineering Materials 26 (14): 2400475. https://doi.org/10.1002/adem.202400475.
Harvard
Luo, Y. et al. (2024) ‘Larger Recovery Strains in Cast Fe–Mn–Si‐Based Shape Memory Alloys by Reducing Thermal Activation and Optimizing Mn Content’, Advanced Engineering Materials, 26(14), p. 2400475. doi:10.1002/adem.202400475.
IEEE
Y. Luo, Y. Fu, W. He, H. Peng, and Y. Wen, “Larger Recovery Strains in Cast Fe–Mn–Si‐Based Shape Memory Alloys by Reducing Thermal Activation and Optimizing Mn Content,” Advanced Engineering Materials, vol. 26, no. 14, p. 2400475, 2024, doi: 10.1002/adem.202400475.
BibTeX
@article{luo2024larger,
title = {{Larger Recovery Strains in Cast Fe–Mn–Si‐Based Shape Memory Alloys by Reducing Thermal Activation and Optimizing Mn Content}},
author = {Luo, Yanni and Fu, Yu and He, Wei and Peng, Huabei and Wen, Yuhua},
journal = {Advanced Engineering Materials},
year = {2024},
volume = {26},
number = {14},
pages = {2400475},
doi = {10.1002/adem.202400475},
url = {https://doi.org/10.1002/adem.202400475}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2024 | 3 | |
| 2025 | 1 | |
| 2026 | 1 |
Its field-weighted citation impact is 0.41: it has been cited 0.41 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Materials Science › Materials Chemistry › Shape Memory Alloy Transformations
- Fe-Mn-Si shape memory alloy
- recovery strain
- cryogenic deformation
- thermal activation
- martensitic transformation
- annealing twin boundaries
Work with this paper
Most-cited papers in Materials Science
- Electric Field Effect in Atomically Thin Carbon FilmsKostya S. Novoselov, Andre K. Geim, Sergey V. Morozov and 5 more · Science · 2004 · 67,474 citations
- Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenidesROBERT D. SHANNON · Acta Crystallographica Section A · 1976 · 66,944 citations
- Ab initio molecular dynamics for liquid metalsGeorg Kresse, J. Häfner · Physical review. B, Condensed matter · 1993 · 46,320 citations
- Helical microtubules of graphitic carbonSumio Iijima · Nature · 1991 · 43,639 citations
- The rise of grapheneAndre K. Geim, Kostya S. Novoselov · Nature Materials · 2007 · 40,328 citations
Questions about this paper
How do I cite this paper in APA style?
Luo, Y., Fu, Y., He, W., Peng, H., & Wen, Y. (2024). Larger Recovery Strains in Cast Fe–Mn–Si‐Based Shape Memory Alloys by Reducing Thermal Activation and Optimizing Mn Content. Advanced Engineering Materials, 26(14), 2400475. https://doi.org/10.1002/adem.202400475
How many times has this paper been cited?
5 times, according to OpenAlex on 22 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access at Advanced Engineering Materials: sign in and open the PDF from this page.
Who wrote this paper?
Yanni Luo, Yu Fu, Wei He, Huabei Peng, Yuhua Wen.
What is the DOI of this paper?
10.1002/adem.202400475, permanently at https://doi.org/10.1002/adem.202400475. Sign in and open it from this page.
Bibliographic data from OpenAlex (CC0), last checked 22 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.