Journal article · 2016
Investigation of pitting corrosion of diamond-like carbon films using synchrotron-based spectromicroscopy
Journal of Applied Physics, 120(19) · Published 18 November 2016 · DOI 10.1063/1.4967799
In brief
“Investigation of pitting corrosion of diamond-like carbon films using synchrotron-based spectromicroscopy” is a 2016 journal article by Sarayut Tunmee and 9 co-authors, published in Journal of Applied Physics. OpenAlex counts 25 citations as of 20 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.
- Citations
- 25
- Most cited in
- 2021 (5)
- Field-weighted impact
- 0.94
- References
- 54
- Authors
- 10
Abstract
Corrosion behavior of diamond-like carbon (DLC) films was evaluated via potentiodynamic polarization in a 3.5 wt. % NaCl solution with pH 2 at room temperature. The polarization results elucidated that the corrosion resistance of the films was enhanced with the variation of the chemical compositions and film thicknesses. The use of the spectromicroscopy method in… Read the full abstract at the publisher.
Excerpt. This paper is not open access.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Tunmee, S., Photongkam, P., Euaruksakul, C., Takamatsu, H., Zhou, X., Wongpanya, P., Komatsu, K., Kanda, K., Ito, H., & Saitoh, H. (2016). Investigation of pitting corrosion of diamond-like carbon films using synchrotron-based spectromicroscopy. Journal of Applied Physics, 120(19). https://doi.org/10.1063/1.4967799
MLA 9
Tunmee, Sarayut, et al. “Investigation of pitting corrosion of diamond-like carbon films using synchrotron-based spectromicroscopy.” Journal of Applied Physics, vol. 120, no. 19, 2016. https://doi.org/10.1063/1.4967799.
Chicago
Tunmee, Sarayut, Pat Photongkam, Chanan Euaruksakul, Hiroki Takamatsu, Xiaolong Zhou, Pornwasa Wongpanya, Keiji Komatsu, Kazuhiro Kanda, Haruhiko Ito, and Hidetoshi Saitoh. 2016. “Investigation of pitting corrosion of diamond-like carbon films using synchrotron-based spectromicroscopy.” Journal of Applied Physics 120 (19). https://doi.org/10.1063/1.4967799.
Harvard
Tunmee, S. et al. (2016) ‘Investigation of pitting corrosion of diamond-like carbon films using synchrotron-based spectromicroscopy’, Journal of Applied Physics, 120(19). doi:10.1063/1.4967799.
IEEE
S. Tunmee et al., “Investigation of pitting corrosion of diamond-like carbon films using synchrotron-based spectromicroscopy,” Journal of Applied Physics, vol. 120, no. 19, 2016, doi: 10.1063/1.4967799.
BibTeX
@article{tunmee2016investigation,
title = {{Investigation of pitting corrosion of diamond-like carbon films using synchrotron-based spectromicroscopy}},
author = {Tunmee, Sarayut and Photongkam, Pat and Euaruksakul, Chanan and Takamatsu, Hiroki and Zhou, Xiaolong and Wongpanya, Pornwasa and Komatsu, Keiji and Kanda, Kazuhiro and Ito, Haruhiko and Saitoh, Hidetoshi},
journal = {Journal of Applied Physics},
year = {2016},
volume = {120},
number = {19},
doi = {10.1063/1.4967799},
url = {https://doi.org/10.1063/1.4967799}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2017 | 4 | |
| 2019 | 1 | |
| 2020 | 1 | |
| 2021 | 5 | |
| 2022 | 5 | |
| 2023 | 4 | |
| 2025 | 3 | |
| 2026 | 2 |
Its field-weighted citation impact is 0.94: it has been cited 0.94 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics
- diamond-like carbon films
- pitting corrosion
- corrosion resistance
- potentiodynamic polarization
- NaCl solution
- film thickness
- chemical composition
- sp2 content
Work with this paper
Most-cited papers in Engineering
- A Closed‐form Equation for Predicting the Hydraulic Conductivity of Unsaturated SoilsMartinus Th. van Genuchten · Soil Science Society of America Journal · 1980 · 28,197 citations
- An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experimentsW. C. Oliver, George M. Pharr · Journal of materials research/Pratt's guide to venture capital sources · 1992 · 27,379 citations
- Digital communicationsOwen Bishop · Routledge eBooks · 2007 · 24,890 citations
- The empirical mode decomposition and the Hilbert spectrum for nonlinear and non-stationary time series analysisNorden Eh Huang, Zhengwei Shen, Steven R. Long and 6 more · Proceedings of the Royal Society A Mathematical Physical and Engineering Sciences · 1998 · 24,008 citations
- Numerical Heat Transfer and Fluid FlowSuhas V. Patankar · CRC Press eBooks · 2018 · 23,491 citations
Questions about this paper
How do I cite this paper in APA style?
Tunmee, S., Photongkam, P., Euaruksakul, C., Takamatsu, H., Zhou, X., Wongpanya, P., Komatsu, K., Kanda, K., Ito, H., & Saitoh, H. (2016). Investigation of pitting corrosion of diamond-like carbon films using synchrotron-based spectromicroscopy. Journal of Applied Physics, 120(19). https://doi.org/10.1063/1.4967799
How many times has this paper been cited?
25 times, according to OpenAlex on 20 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.
Who wrote this paper?
Sarayut Tunmee, Pat Photongkam, Chanan Euaruksakul, Hiroki Takamatsu, Xiaolong Zhou, Pornwasa Wongpanya, Keiji Komatsu, Kazuhiro Kanda, Haruhiko Ito, Hidetoshi Saitoh.
What is the DOI of this paper?
10.1063/1.4967799, permanently at https://doi.org/10.1063/1.4967799. Sign in and open it from this page.
Bibliographic data from OpenAlex (CC0), last checked 20 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.