Influence of heat treatments on microstructure and pitting corrosion resistance of 15%Cr supermartensitic stainless steel

B.A.R.S. Barbosa, Sérgio Souto Maior Tavares, Ivan Napoleão Bastos, M. R. Silva, Marcelo Camargo Severo de Macêdo

Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control, 49(4), 311–315 · Published 27 February 2014 · DOI 10.1179/1743278214y.0000000156

View at the publisherCite this paper

In brief

“Influence of heat treatments on microstructure and pitting corrosion resistance of 15%Cr supermartensitic stainless steel” is a 2014 journal article by B.A.R.S. Barbosa and 4 co-authors, published in Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control. OpenAlex counts 9 citations as of 22 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
9
Most cited in
2016 (2)
Field-weighted impact
0.57
References
12
Authors
5

Abstract

Supermartensitic is a new class of stainless steels in development and consolidation as commercial products. Significant changes on chemical composition of conventional martensitic stainless steels, such as the reduction of the carbon content to <0·03 wt-%, and the addition of Ni and Mo, marked the development of this new group of alloys. New grades containing… Read the full abstract at the publisher.

Excerpt. This paper is not open access.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Barbosa, B., Tavares, S. S. M., Bastos, I. N., Silva, M. R., & de Macêdo, M. C. S. (2014). Influence of heat treatments on microstructure and pitting corrosion resistance of 15%Cr supermartensitic stainless steel. Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control, 49(4), 311–315. https://doi.org/10.1179/1743278214y.0000000156

MLA 9

Barbosa, B.A.R.S., et al. “Influence of heat treatments on microstructure and pitting corrosion resistance of 15%Cr supermartensitic stainless steel.” Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control, vol. 49, no. 4, 2014, pp. 311–315. https://doi.org/10.1179/1743278214y.0000000156.

Chicago

Barbosa, B.A.R.S., Sérgio Souto Maior Tavares, Ivan Napoleão Bastos, M. R. Silva, and Marcelo Camargo Severo de Macêdo. 2014. “Influence of heat treatments on microstructure and pitting corrosion resistance of 15%Cr supermartensitic stainless steel.” Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control 49 (4): 311–315. https://doi.org/10.1179/1743278214y.0000000156.

Harvard

Barbosa, B. et al. (2014) ‘Influence of heat treatments on microstructure and pitting corrosion resistance of 15%Cr supermartensitic stainless steel’, Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control, 49(4), pp. 311–315. doi:10.1179/1743278214y.0000000156.

IEEE

B. Barbosa, S. S. M. Tavares, I. N. Bastos, M. R. Silva, and M. C. S. de Macêdo, “Influence of heat treatments on microstructure and pitting corrosion resistance of 15%Cr supermartensitic stainless steel,” Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control, vol. 49, no. 4, pp. 311–315, 2014, doi: 10.1179/1743278214y.0000000156.

BibTeX

@article{barbosa2014influence,
  title     = {{Influence of heat treatments on microstructure and pitting corrosion resistance of 15\%Cr supermartensitic stainless steel}},
  author    = {Barbosa, B.A.R.S. and Tavares, Sérgio Souto Maior and Bastos, Ivan Napoleão and Silva, M. R. and de Macêdo, Marcelo Camargo Severo},
  journal   = {Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control},
  year      = {2014},
  volume    = {49},
  number    = {4},
  pages     = {311--315},
  doi       = {10.1179/1743278214y.0000000156},
  url       = {https://doi.org/10.1179/1743278214y.0000000156}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
201622
201911
202222
202322
202411
202511

Its field-weighted citation impact is 0.57: it has been cited 0.57 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Materials Science › Metals and Alloys › Hydrogen embrittlement and corrosion behaviors in metals

  • supermartensitic stainless steel
  • pitting resistance
  • tempering
  • double tempering
  • microstructure
  • martensite
  • pitting potential
  • NaCl solution

Work with this paper

Most-cited papers in Materials Science

All highly cited Materials Science papers

Questions about this paper

How do I cite this paper in APA style?

Barbosa, B., Tavares, S. S. M., Bastos, I. N., Silva, M. R., & de Macêdo, M. C. S. (2014). Influence of heat treatments on microstructure and pitting corrosion resistance of 15%Cr supermartensitic stainless steel. Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control, 49(4), 311–315. https://doi.org/10.1179/1743278214y.0000000156

How many times has this paper been cited?

9 times, according to OpenAlex on 22 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

B.A.R.S. Barbosa, Sérgio Souto Maior Tavares, Ivan Napoleão Bastos, M. R. Silva, Marcelo Camargo Severo de Macêdo.

What is the DOI of this paper?

10.1179/1743278214y.0000000156, permanently at https://doi.org/10.1179/1743278214y.0000000156. Sign in and open it from this page.

Bibliographic data from OpenAlex (CC0), last checked 22 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.