Journal article · 2023 · Open access

In Situ Nanoindentation at Elevated Humidities

Kian Tadayon, Benny Bar‐On, Björn Günther, Cordula Vogel, Igor Zlotnikov

Advanced Materials Interfaces, 10(33) · Published 10 August 2023 · DOI 10.1002/admi.202300459

Free PDFView at the publisherCite this paper

In brief

“In Situ Nanoindentation at Elevated Humidities” is a 2023 journal article by Kian Tadayon and 4 co-authors, published in Advanced Materials Interfaces. OpenAlex counts 6 citations as of 16 November 2026, which puts it in the top 9% of works published in 2023 by citations. It is open access under a CC BY licence: the full text is free to read at Advanced Materials Interfaces.

Citations
6
Most cited in
2025 (3)
Field-weighted impact
0.60
References
31
Authors
5

Abstract

Nanoindentation is one of the most widespread methods to measure the mechanical performance of complex materials systems. As it allows for local characterization of composite architectures with sub‐micron spatial features and a large range of properties, nanoindentation is commonly used to measure the properties of biological materials. In situ nanoindentation, a further development of the approach, is a powerful tool for the analysis of plastic deformation and failure of materials. Here, samples can be mechanically manipulated using the indenter, while their behavior is monitored with the resolution of a scanning electron microscope (SEM). Indeed, numerous studies demonstrate the potential of this approach for studying the most fundamental material characteristics. However, so far, these measurements are performed in high‐vacuum conditions inherent to the conventional electron microscopy method, which are irrelevant when studying biological structures that evolved to perform in hydrated conditions. In this work, the ability to conduct nanoindentation experiments under controlled humidity and temperature inside an environmental SEM is developed. This technique has the potential to become crucial for materials design and characterization in many domains where humidity has a significant impact on performance. These include organic/polymer systems, microelectronic and optoelectronic devices, materials for catalysis, batteries, and many more.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Tadayon, K., Bar‐On, B., Günther, B., Vogel, C., & Zlotnikov, I. (2023). In Situ Nanoindentation at Elevated Humidities. Advanced Materials Interfaces, 10(33). https://doi.org/10.1002/admi.202300459

MLA 9

Tadayon, Kian, et al. “In Situ Nanoindentation at Elevated Humidities.” Advanced Materials Interfaces, vol. 10, no. 33, 2023. https://doi.org/10.1002/admi.202300459.

Chicago

Tadayon, Kian, Benny Bar‐On, Björn Günther, Cordula Vogel, and Igor Zlotnikov. 2023. “In Situ Nanoindentation at Elevated Humidities.” Advanced Materials Interfaces 10 (33). https://doi.org/10.1002/admi.202300459.

Harvard

Tadayon, K. et al. (2023) ‘In Situ Nanoindentation at Elevated Humidities’, Advanced Materials Interfaces, 10(33). doi:10.1002/admi.202300459.

IEEE

K. Tadayon, B. Bar‐On, B. Günther, C. Vogel, and I. Zlotnikov, “In Situ Nanoindentation at Elevated Humidities,” Advanced Materials Interfaces, vol. 10, no. 33, 2023, doi: 10.1002/admi.202300459.

BibTeX

@article{tadayon2023situ,
  title     = {{In Situ Nanoindentation at Elevated Humidities}},
  author    = {Tadayon, Kian and Bar‐On, Benny and Günther, Björn and Vogel, Cordula and Zlotnikov, Igor},
  journal   = {Advanced Materials Interfaces},
  year      = {2023},
  volume    = {10},
  number    = {33},
  doi       = {10.1002/admi.202300459},
  url       = {https://doi.org/10.1002/admi.202300459}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
202322
202533
202611

Its field-weighted citation impact is 0.60: it has been cited 0.60 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics

  • in situ nanoindentation
  • environmental scanning electron microscopy
  • biological materials
  • plastic deformation
  • equipment failure
  • polymer systems
  • mechanical characterization

Work with this paper

Most-cited papers in Engineering

All highly cited Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Tadayon, K., Bar‐On, B., Günther, B., Vogel, C., & Zlotnikov, I. (2023). In Situ Nanoindentation at Elevated Humidities. Advanced Materials Interfaces, 10(33). https://doi.org/10.1002/admi.202300459

How many times has this paper been cited?

6 times, according to OpenAlex on 16 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

Yes. It is open access: read the free full text at Advanced Materials Interfaces.

Who wrote this paper?

Kian Tadayon, Benny Bar‐On, Björn Günther, Cordula Vogel, Igor Zlotnikov.

What is the DOI of this paper?

10.1002/admi.202300459. The permanent link is https://doi.org/10.1002/admi.202300459.

Bibliographic data from OpenAlex (CC0), last checked 16 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.