Journal article · 1999
HREM and nanoindentation studies of BN:C films deposited by reactive sputtering from a B4C target
Vacuum, 53(3-4), 451–457 · Published 1 June 1999 · DOI 10.1016/s0042-207x(99)00109-8
In brief
“HREM and nanoindentation studies of BN:C films deposited by reactive sputtering from a B4C target” is a 1999 journal article by Mats Johansson and 2 co-authors, published in Vacuum. OpenAlex counts 15 citations as of 17 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.
- Citations
- 15
- Most cited in
- 2013 (1)
- Field-weighted impact
- 1.37
- Authors
- 3
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Johansson, M., Sjöström, H., & Hultman, L. (1999). HREM and nanoindentation studies of BN:C films deposited by reactive sputtering from a B4C target. Vacuum, 53(3-4), 451–457. https://doi.org/10.1016/s0042-207x(99)00109-8
MLA 9
Johansson, Mats, et al. “HREM and nanoindentation studies of BN:C films deposited by reactive sputtering from a B4C target.” Vacuum, vol. 53, no. 3-4, 1999, pp. 451–457. https://doi.org/10.1016/s0042-207x(99)00109-8.
Chicago
Johansson, Mats, H. Sjöström, and Lars Hultman. 1999. “HREM and nanoindentation studies of BN:C films deposited by reactive sputtering from a B4C target.” Vacuum 53 (3-4): 451–457. https://doi.org/10.1016/s0042-207x(99)00109-8.
Harvard
Johansson, M., Sjöström, H. and Hultman, L. (1999) ‘HREM and nanoindentation studies of BN:C films deposited by reactive sputtering from a B4C target’, Vacuum, 53(3-4), pp. 451–457. doi:10.1016/s0042-207x(99)00109-8.
IEEE
M. Johansson, H. Sjöström, and L. Hultman, “HREM and nanoindentation studies of BN:C films deposited by reactive sputtering from a B4C target,” Vacuum, vol. 53, no. 3-4, pp. 451–457, 1999, doi: 10.1016/s0042-207x(99)00109-8.
BibTeX
@article{johansson1999hrem,
title = {{HREM and nanoindentation studies of BN:C films deposited by reactive sputtering from a B4C target}},
author = {Johansson, Mats and Sjöström, H. and Hultman, Lars},
journal = {Vacuum},
year = {1999},
volume = {53},
number = {3-4},
pages = {451--457},
doi = {10.1016/s0042-207x(99)00109-8},
url = {https://doi.org/10.1016/s0042-207x(99)00109-8}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2013 | 1 | |
| 2016 | 1 | |
| 2022 | 1 |
Its field-weighted citation impact is 1.37: it has been cited 1.37 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Materials Science › Materials Chemistry › Boron and Carbon Nanomaterials Research
- reactive sputtering
- ion bombardment
- hexagonal boron nitride
- cubic boron nitride
- film texture
- carbon content
- mechanical properties
- hardness
Work with this paper
Most-cited papers in Materials Science
- Electric Field Effect in Atomically Thin Carbon FilmsKostya S. Novoselov, Andre K. Geim, Sergey V. Morozov and 5 more · Science · 2004 · 67,474 citations
- Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenidesROBERT D. SHANNON · Acta Crystallographica Section A · 1976 · 66,944 citations
- Ab initio molecular dynamics for liquid metalsGeorg Kresse, J. Häfner · Physical review. B, Condensed matter · 1993 · 46,320 citations
- Helical microtubules of graphitic carbonSumio Iijima · Nature · 1991 · 43,639 citations
- The rise of grapheneAndre K. Geim, Kostya S. Novoselov · Nature Materials · 2007 · 40,328 citations
Questions about this paper
How do I cite this paper in APA style?
Johansson, M., Sjöström, H., & Hultman, L. (1999). HREM and nanoindentation studies of BN:C films deposited by reactive sputtering from a B4C target. Vacuum, 53(3-4), 451–457. https://doi.org/10.1016/s0042-207x(99)00109-8
How many times has this paper been cited?
15 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.
Who wrote this paper?
Mats Johansson, H. Sjöström, Lars Hultman.
What is the DOI of this paper?
10.1016/s0042-207x(99)00109-8, permanently at https://doi.org/10.1016/s0042-207x(99)00109-8. Sign in and open it from this page.
Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.