Paper · 2015
How to perform nanoindentation in difficult conditions? Applications to ultra soft materials and temperature environment
Published 1 January 2015
In brief
“How to perform nanoindentation in difficult conditions? Applications to ultra soft materials and temperature environment” is a 2015 paper by Michel Fajfrowski and Vincent D. Jardret. OpenAlex counts 0 citations as of 16 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.
- Citations
- 0
- Authors
- 2
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Fajfrowski, M., & Jardret, V. D. (2015). How to perform nanoindentation in difficult conditions? Applications to ultra soft materials and temperature environment. https://dc.engconfintl.org/cgi/viewcontent.cgi?article=1044&context=nanomechtest_v
MLA 9
Fajfrowski, Michel, and Vincent D. Jardret. “How to perform nanoindentation in difficult conditions? Applications to ultra soft materials and temperature environment.” 2015. https://dc.engconfintl.org/cgi/viewcontent.cgi?article=1044&context=nanomechtest_v.
Chicago
Fajfrowski, Michel and Vincent D. Jardret. 2015. “How to perform nanoindentation in difficult conditions? Applications to ultra soft materials and temperature environment.” https://dc.engconfintl.org/cgi/viewcontent.cgi?article=1044&context=nanomechtest_v.
Harvard
Fajfrowski, M. and Jardret, V. D. (2015) ‘How to perform nanoindentation in difficult conditions? Applications to ultra soft materials and temperature environment’. Available at: https://dc.engconfintl.org/cgi/viewcontent.cgi?article=1044&context=nanomechtest_v.
IEEE
M. Fajfrowski and V. D. Jardret, “How to perform nanoindentation in difficult conditions? Applications to ultra soft materials and temperature environment,” 2015.
BibTeX
@article{fajfrowski2015perform,
title = {{How to perform nanoindentation in difficult conditions? Applications to ultra soft materials and temperature environment}},
author = {Fajfrowski, Michel and Jardret, Vincent D.},
year = {2015},
url = {https://dc.engconfintl.org/cgi/viewcontent.cgi?article=1044&context=nanomechtest_v}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Topic and keywords
Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics
- nanoindentation
- temperature effects
Work with this paper
Most-cited papers in Engineering
- A Closed‐form Equation for Predicting the Hydraulic Conductivity of Unsaturated SoilsMartinus Th. van Genuchten · Soil Science Society of America Journal · 1980 · 28,197 citations
- An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experimentsW. C. Oliver, George M. Pharr · Journal of materials research/Pratt's guide to venture capital sources · 1992 · 27,379 citations
- Digital communicationsOwen Bishop · Routledge eBooks · 2007 · 24,890 citations
- The empirical mode decomposition and the Hilbert spectrum for nonlinear and non-stationary time series analysisNorden Eh Huang, Zhengwei Shen, Steven R. Long and 6 more · Proceedings of the Royal Society A Mathematical Physical and Engineering Sciences · 1998 · 24,008 citations
- Numerical Heat Transfer and Fluid FlowSuhas V. Patankar · CRC Press eBooks · 2018 · 23,491 citations
Questions about this paper
How do I cite this paper in APA style?
Fajfrowski, M., & Jardret, V. D. (2015). How to perform nanoindentation in difficult conditions? Applications to ultra soft materials and temperature environment. https://dc.engconfintl.org/cgi/viewcontent.cgi?article=1044&context=nanomechtest_v
How many times has this paper been cited?
0 times, according to OpenAlex on 16 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.
Who wrote this paper?
Michel Fajfrowski, Vincent D. Jardret.
Bibliographic data from OpenAlex (CC0), last checked 16 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.