Hot nanoindentation in inert environments
Review of Scientific Instruments, 81(7), 073901 · Published 1 July 2010 · DOI 10.1063/1.3436633
In brief
“Hot nanoindentation in inert environments” is a 2010 journal article by Jonathan C. Trenkle and 2 co-authors, published in Review of Scientific Instruments. OpenAlex counts 95 citations as of 16 November 2026. It is open access under a CC BY-NC-SA licence: the full text is free to read at DSpace@MIT (Massachusetts Institute of Technology).
- Citations
- 95
- Most cited in
- 2020 (10)
- Field-weighted impact
- 6.51
- References
- 78
- Authors
- 3
Abstract
An instrument capable of performing nanoindentation at temperatures up to 500 degrees C in inert atmospheres, including partial vacuum and gas near atmospheric pressures, is described. Technical issues associated with the technique (such as drift and noise) and the instrument (such as tip erosion and radiative heating of the transducer) are identified and addressed. Based on these considerations, preferred operation conditions are identified for testing on various materials. As a proof-of-concept demonstration, the hardness and elastic modulus of three materials are measured: fused silica (nonoxidizing), aluminum, and copper (both oxidizing). In all cases, the properties match reasonably well with published data acquired by more conventional test methods.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Trenkle, J. C., Packard, C. E., & Schuh, C. A. (2010). Hot nanoindentation in inert environments. Review of Scientific Instruments, 81(7), 073901. https://doi.org/10.1063/1.3436633
MLA 9
Trenkle, Jonathan C., et al. “Hot nanoindentation in inert environments.” Review of Scientific Instruments, vol. 81, no. 7, 2010, p. 073901. https://doi.org/10.1063/1.3436633.
Chicago
Trenkle, Jonathan C., Corinne E. Packard, and Christopher Allan Schuh. 2010. “Hot nanoindentation in inert environments.” Review of Scientific Instruments 81 (7): 073901. https://doi.org/10.1063/1.3436633.
Harvard
Trenkle, J. C., Packard, C. E. and Schuh, C. A. (2010) ‘Hot nanoindentation in inert environments’, Review of Scientific Instruments, 81(7), p. 073901. doi:10.1063/1.3436633.
IEEE
J. C. Trenkle, C. E. Packard, and C. A. Schuh, “Hot nanoindentation in inert environments,” Review of Scientific Instruments, vol. 81, no. 7, p. 073901, 2010, doi: 10.1063/1.3436633.
BibTeX
@article{trenkle2010nanoindentation,
title = {{Hot nanoindentation in inert environments}},
author = {Trenkle, Jonathan C. and Packard, Corinne E. and Schuh, Christopher Allan},
journal = {Review of Scientific Instruments},
year = {2010},
volume = {81},
number = {7},
pages = {073901},
doi = {10.1063/1.3436633},
url = {https://doi.org/10.1063/1.3436633}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2017 | 9 | |
| 2018 | 7 | |
| 2019 | 8 | |
| 2020 | 10 | |
| 2021 | 4 | |
| 2022 | 4 | |
| 2023 | 1 | |
| 2024 | 3 | |
| 2025 | 3 | |
| 2026 | 2 |
Its field-weighted citation impact is 6.51: it has been cited 6.51 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics
- inert atmosphere
- high-temperature mechanical testing
- hardness
- elastic modulus
- fused silica
- aluminum
- copper
- oxidation
Work with this paper
Most-cited papers in Engineering
- A Closed‐form Equation for Predicting the Hydraulic Conductivity of Unsaturated SoilsMartinus Th. van Genuchten · Soil Science Society of America Journal · 1980 · 28,197 citations
- An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experimentsW. C. Oliver, George M. Pharr · Journal of materials research/Pratt's guide to venture capital sources · 1992 · 27,379 citations
- Digital communicationsOwen Bishop · Routledge eBooks · 2007 · 24,890 citations
- The empirical mode decomposition and the Hilbert spectrum for nonlinear and non-stationary time series analysisNorden Eh Huang, Zhengwei Shen, Steven R. Long and 6 more · Proceedings of the Royal Society A Mathematical Physical and Engineering Sciences · 1998 · 24,008 citations
- Numerical Heat Transfer and Fluid FlowSuhas V. Patankar · CRC Press eBooks · 2018 · 23,491 citations
Questions about this paper
How do I cite this paper in APA style?
Trenkle, J. C., Packard, C. E., & Schuh, C. A. (2010). Hot nanoindentation in inert environments. Review of Scientific Instruments, 81(7), 073901. https://doi.org/10.1063/1.3436633
How many times has this paper been cited?
95 times, according to OpenAlex on 16 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access: read the free full text at DSpace@MIT (Massachusetts Institute of Technology).
Who wrote this paper?
Jonathan C. Trenkle, Corinne E. Packard, Christopher Allan Schuh.
What is the DOI of this paper?
10.1063/1.3436633. The permanent link is https://doi.org/10.1063/1.3436633.
Bibliographic data from OpenAlex (CC0), last checked 16 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.