Review article · 2025 · Open access
Extending nanoindentation testing toward extreme strain rates and temperatures for probing materials evolution at the nanoscale
MRS Bulletin, 50(6), 705–714 · Published 21 May 2025 · DOI 10.1557/s43577-025-00918-7
In brief
“Extending nanoindentation testing toward extreme strain rates and temperatures for probing materials evolution at the nanoscale” is a 2025 review article by Benoit Merle and 2 co-authors, published in MRS Bulletin. OpenAlex counts 9 citations as of 16 November 2026, which puts it in the top 7% of works published in 2025 by citations. It is open access under a CC BY licence: the full text is free to read at MRS Bulletin.
- Citations
- 9
- Most cited in
- 2026 (7)
- Field-weighted impact
- 0.51
- References
- 90
- Authors
- 3
Abstract
For the past 30 years, nanoindentation has provided critical insights into the microstructure–strength relationship for a wide range of materials. However, it has traditionally been limited to quasistatic testing at room temperature, which has hindered a holistic understanding of microstructurally induced deformation mechanisms and their dynamic evolution as a function of the temperature and strain rate. Over the past decade, the operational scope of nanoindentation has expanded dramatically. Temperatures up to 1100°C and strain rates as high as 10 +4 s −1 and as low as 10 −8 s −1 have become accessible. In addition, advanced techniques allow tracking microstructural evolution and corresponding changes in mechanical behavior during deformation under extreme conditions. These advancements have transformed nanoindentation into a versatile tool for comprehensive materials characterization, enabling high-throughput investigations under multimodal conditions. Graphical abstract
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Merle, B., Tiphéne, G., & Kermouche, G. (2025). Extending nanoindentation testing toward extreme strain rates and temperatures for probing materials evolution at the nanoscale. MRS Bulletin, 50(6), 705–714. https://doi.org/10.1557/s43577-025-00918-7
MLA 9
Merle, Benoit, et al. “Extending nanoindentation testing toward extreme strain rates and temperatures for probing materials evolution at the nanoscale.” MRS Bulletin, vol. 50, no. 6, 2025, pp. 705–714. https://doi.org/10.1557/s43577-025-00918-7.
Chicago
Merle, Benoit, Gabrielle Tiphéne, and Guillaume Kermouche. 2025. “Extending nanoindentation testing toward extreme strain rates and temperatures for probing materials evolution at the nanoscale.” MRS Bulletin 50 (6): 705–714. https://doi.org/10.1557/s43577-025-00918-7.
Harvard
Merle, B., Tiphéne, G. and Kermouche, G. (2025) ‘Extending nanoindentation testing toward extreme strain rates and temperatures for probing materials evolution at the nanoscale’, MRS Bulletin, 50(6), pp. 705–714. doi:10.1557/s43577-025-00918-7.
IEEE
B. Merle, G. Tiphéne, and G. Kermouche, “Extending nanoindentation testing toward extreme strain rates and temperatures for probing materials evolution at the nanoscale,” MRS Bulletin, vol. 50, no. 6, pp. 705–714, 2025, doi: 10.1557/s43577-025-00918-7.
BibTeX
@article{merle2025extending,
title = {{Extending nanoindentation testing toward extreme strain rates and temperatures for probing materials evolution at the nanoscale}},
author = {Merle, Benoit and Tiphéne, Gabrielle and Kermouche, Guillaume},
journal = {MRS Bulletin},
year = {2025},
volume = {50},
number = {6},
pages = {705--714},
doi = {10.1557/s43577-025-00918-7},
url = {https://doi.org/10.1557/s43577-025-00918-7}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Topic and keywords
Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics
- nanoindentation
- high-temperature deformation
- microstructure evolution
- high strain rate testing
- material characterization
Work with this paper
Most-cited papers in Engineering
- A Closed‐form Equation for Predicting the Hydraulic Conductivity of Unsaturated SoilsMartinus Th. van Genuchten · Soil Science Society of America Journal · 1980 · 28,197 citations
- An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experimentsW. C. Oliver, George M. Pharr · Journal of materials research/Pratt's guide to venture capital sources · 1992 · 27,379 citations
- Digital communicationsOwen Bishop · Routledge eBooks · 2007 · 24,890 citations
- The empirical mode decomposition and the Hilbert spectrum for nonlinear and non-stationary time series analysisNorden Eh Huang, Zhengwei Shen, Steven R. Long and 6 more · Proceedings of the Royal Society A Mathematical Physical and Engineering Sciences · 1998 · 24,008 citations
- Numerical Heat Transfer and Fluid FlowSuhas V. Patankar · CRC Press eBooks · 2018 · 23,491 citations
Questions about this paper
How do I cite this paper in APA style?
Merle, B., Tiphéne, G., & Kermouche, G. (2025). Extending nanoindentation testing toward extreme strain rates and temperatures for probing materials evolution at the nanoscale. MRS Bulletin, 50(6), 705–714. https://doi.org/10.1557/s43577-025-00918-7
How many times has this paper been cited?
9 times, according to OpenAlex on 16 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access: read the free full text at MRS Bulletin.
Who wrote this paper?
Benoit Merle, Gabrielle Tiphéne, Guillaume Kermouche.
What is the DOI of this paper?
10.1557/s43577-025-00918-7. The permanent link is https://doi.org/10.1557/s43577-025-00918-7.
Bibliographic data from OpenAlex (CC0), last checked 16 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.