Dissertation · 2007 · Open access

Evaluation of pitting corrosion of stainless steel aisi-sae 630 hardened by precipitation in sea synthetic water by means of technique electrochemical*.

Oscar Ignacio Peña Ordóñez

Universidad Industrial de Santander · Published 1 January 2007

Open PDFView at the publisherCite this paper

In brief

“Evaluation of pitting corrosion of stainless steel aisi-sae 630 hardened by precipitation in sea synthetic water by means of technique electrochemical*.” is a 2007 dissertation by Oscar Ignacio Peña Ordóñez, published in Universidad Industrial de Santander. OpenAlex counts 0 citations as of 22 November 2026. It is open access under a CC BY licence: the full text is free to read at Universidad Industrial de Santander.

Citations
0
References
6
Authors
1

Abstract

Los aceros inoxidables endurecidos por precipitación son una alternativa a los demás aceros inoxidables, un caso especial es el acero inoxidable AISI-SAE 630, el cual contiene en su composición química elementos aleantes como Nb y Ta evitando así la formación de carburos ricos en cromo, los cuales disminuyen la resistencia a la corrosión. Sin embargo, se ha encontrado que este material puede presentar corrosión localizada en ambientes agresivos como el agua de mar, dado que los iones cloruro afectan estos materiales. En la presente investigación se estudió el acero inoxidable AISI-SAE 630 en estado de entrega y después de un tratamiento térmico, con el fin de eliminar tensiones posiblemente producidas durante el tiempo de servicio, en un medio que simulo las condiciones del agua de mar, para conocer el comportamiento del material bajo estas condiciones, en un tiempo de treinta y cinco días. Se emplearon las técnicas electroquímicas resistencia a la polarización (Rp), espectroscopia de impedancias (EIS), polarización cíclica, y las pruebas de aireación diferencial y temperatura critica de picado (CPT), con el fin de determinar la velocidad de corrosión por picado, y la CPT. Los resultados mostraron que las técnicas de EIS y Rp no son las más adecuadas para medir la velocidad de corrosión por picado. La probeta “Blanco” presento una mayor susceptibilidad a la corrosión por picado dado que el valor de Ep fue menor, además para esta probeta la profundidad de picado fue mayor, lo cual se confirmo por el perfil de profundidad, dando como resultado una velocidad de corrosión más alta, probablemente por la ausencia de Ta en este material. La CPT para el acero inoxidable AISI-SAE 630 fue de 29±1°C, la cual esta muy cercana a la temperatura de servicio, siendo esta variable (Temperatura) quien haya sido la causante del deterioro del material.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Ordóñez, O. I. P. (2007). Evaluation of pitting corrosion of stainless steel aisi-sae 630 hardened by precipitation in sea synthetic water by means of technique electrochemical*. Universidad Industrial de Santander. https://noesis.uis.edu.co/handle/20.500.14071/19971

MLA 9

Ordóñez, Oscar Ignacio Peña. “Evaluation of pitting corrosion of stainless steel aisi-sae 630 hardened by precipitation in sea synthetic water by means of technique electrochemical*.” Universidad Industrial de Santander, 2007. https://noesis.uis.edu.co/handle/20.500.14071/19971.

Chicago

Ordóñez, Oscar Ignacio Peña. 2007. “Evaluation of pitting corrosion of stainless steel aisi-sae 630 hardened by precipitation in sea synthetic water by means of technique electrochemical*.” Universidad Industrial de Santander. https://noesis.uis.edu.co/handle/20.500.14071/19971.

Harvard

Ordóñez, O. I. P. (2007) ‘Evaluation of pitting corrosion of stainless steel aisi-sae 630 hardened by precipitation in sea synthetic water by means of technique electrochemical*.’, Universidad Industrial de Santander. Available at: https://noesis.uis.edu.co/handle/20.500.14071/19971.

IEEE

O. I. P. Ordóñez, “Evaluation of pitting corrosion of stainless steel aisi-sae 630 hardened by precipitation in sea synthetic water by means of technique electrochemical*.,” Universidad Industrial de Santander, 2007.

BibTeX

@phdthesis{ordonez2007evaluation,
  title     = {{Evaluation of pitting corrosion of stainless steel aisi-sae 630 hardened by precipitation in sea synthetic water by means of technique electrochemical*.}},
  author    = {Ordóñez, Oscar Ignacio Peña},
  year      = {2007},
  url       = {https://noesis.uis.edu.co/handle/20.500.14071/19971}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Topic and keywords

Physical Sciences › Materials Science › Metals and Alloys › Hydrogen embrittlement and corrosion behaviors in metals

  • pitting corrosion
  • precipitation hardening stainless steel
  • seawater corrosion
  • chloride
  • critical pitting temperature
  • heat treatment
  • electrochemical impedance spectroscopy
  • polarization resistance

Work with this paper

Most-cited papers in Materials Science

All highly cited Materials Science papers

Questions about this paper

How do I cite this paper in APA style?

Ordóñez, O. I. P. (2007). Evaluation of pitting corrosion of stainless steel aisi-sae 630 hardened by precipitation in sea synthetic water by means of technique electrochemical*. Universidad Industrial de Santander. https://noesis.uis.edu.co/handle/20.500.14071/19971

How many times has this paper been cited?

0 times, according to OpenAlex on 22 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

Yes. It is open access at Universidad Industrial de Santander: sign in and open the PDF from this page.

Who wrote this paper?

Oscar Ignacio Peña Ordóñez.

Bibliographic data from OpenAlex (CC0), last checked 22 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.