Dissertation · 2006

Estimation of the load ratios by quantitative fractographic analysis of the ratio between height and the striation spacing of an aeronautical aluminium alloy AI AMS 7475-T7351

Aristides Alves Messias Filho

LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas) · Published 19 May 2006

View at the publisherCite this paper

In brief

“Estimation of the load ratios by quantitative fractographic analysis of the ratio between height and the striation spacing of an aeronautical aluminium alloy AI AMS 7475-T7351” is a 2006 dissertation by Aristides Alves Messias Filho, published in LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas). OpenAlex counts 0 citations as of 22 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
0
Authors
1

Abstract

Este trabalho visa determinar a razão de carga cíclica R através da medida, na superficie de fratura, da relação entre a largura inter-estrias (s) e a altura da estria (H). É de conhecimento que o espaçamento (s) se correlaciona com a taxa de crescimento da trinca da/dN, enquanto que a curva da/dN x ΔK depende… Read the full abstract at the publisher.

Excerpt. This paper is not open access.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Filho, A. A. M. (2006). Estimation of the load ratios by quantitative fractographic analysis of the ratio between height and the striation spacing of an aeronautical aluminium alloy AI AMS 7475-T7351. LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas). http://www.teses.usp.br/teses/disponiveis/18/18150/tde-01022016-153904/

MLA 9

Filho, Aristides Alves Messias. “Estimation of the load ratios by quantitative fractographic analysis of the ratio between height and the striation spacing of an aeronautical aluminium alloy AI AMS 7475-T7351.” LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas), 2006. http://www.teses.usp.br/teses/disponiveis/18/18150/tde-01022016-153904/.

Chicago

Filho, Aristides Alves Messias. 2006. “Estimation of the load ratios by quantitative fractographic analysis of the ratio between height and the striation spacing of an aeronautical aluminium alloy AI AMS 7475-T7351.” LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas). http://www.teses.usp.br/teses/disponiveis/18/18150/tde-01022016-153904/.

Harvard

Filho, A. A. M. (2006) ‘Estimation of the load ratios by quantitative fractographic analysis of the ratio between height and the striation spacing of an aeronautical aluminium alloy AI AMS 7475-T7351’, LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas). Available at: http://www.teses.usp.br/teses/disponiveis/18/18150/tde-01022016-153904/.

IEEE

A. A. M. Filho, “Estimation of the load ratios by quantitative fractographic analysis of the ratio between height and the striation spacing of an aeronautical aluminium alloy AI AMS 7475-T7351,” LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas), 2006.

BibTeX

@phdthesis{filho2006estimation,
  title     = {{Estimation of the load ratios by quantitative fractographic analysis of the ratio between height and the striation spacing of an aeronautical aluminium alloy AI AMS 7475-T7351}},
  author    = {Filho, Aristides Alves Messias},
  year      = {2006},
  url       = {http://www.teses.usp.br/teses/disponiveis/18/18150/tde-01022016-153904/}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Topic and keywords

Physical Sciences › Engineering › Mechanics of Materials › Fatigue and fracture mechanics

  • striation spacing
  • stress ratio
  • fatigue crack growth rate
  • Paris law
  • stress intensity factor
  • fractography
  • crack tip morphology
  • compact tension specimens

Work with this paper

Most-cited papers in Engineering

All highly cited Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Filho, A. A. M. (2006). Estimation of the load ratios by quantitative fractographic analysis of the ratio between height and the striation spacing of an aeronautical aluminium alloy AI AMS 7475-T7351. LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas). http://www.teses.usp.br/teses/disponiveis/18/18150/tde-01022016-153904/

How many times has this paper been cited?

0 times, according to OpenAlex on 22 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Aristides Alves Messias Filho.

Bibliographic data from OpenAlex (CC0), last checked 22 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.