Preprint · 2022 · Open access
Displacement damage in Hydrogenated Amorphous Silicon p-i-n diodes and charge selective contacts detectors
Published 17 April 2022 · DOI 10.36227/techrxiv.19555042.v2
In brief
“Displacement damage in Hydrogenated Amorphous Silicon p-i-n diodes and charge selective contacts detectors” is a 2022 preprint by M. Menichelli and 35 co-authors. OpenAlex counts 1 citations as of 19 November 2026. It is open access under a CC BY-NC-SA licence: the full text is free to read.
- Citations
- 1
- Most cited in
- 2022 (1)
- References
- 9
- Authors
- 36
Abstract
Hydrogenated amorphous silicon is a well known detector material for its radiation resistance. This study concern 10 µm thickness, p-i-n and charge selective contacts planar diode detectors which were irradiated with neutrons at two fluence values: 10 16 n eq /cm 2 and 5 x 10 16 n eq /cm 2 . In order to evaluate their radiation resistance, detector leakage current and response to X-ray photons have been measured. The effect of annealing for performance recovery at 100°C for 12 and 24 hours has also been studied. The results for the 10 16 n eq /cm 2 irradiation show a factor 2 increase in leakage current that is completely recovered after annealing for p-i-n devices while charge selective contacts devices show an overall decrease of the leakage current at the end of the annealing process compared to the measurement before the irradiation. X-ray dosimetric sensitivity degrades, for this fluence, at the end of irradiation but partially recovers for charge selective contacts devices and increases for p-i-n devices at the end of the annealing process. Concerning the 5 x 10 16 n eq /cm 2 irradiation test (for p-i-n structures only), due to the activation occurred during the irradiation phase, the results were taken after 146 days of storage around 0° C when a self-annealing effect may have occurred. Nevertheless the results shows a degradation in leakage current and x-ray sensitivity which changes very little after annealing.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Menichelli, M., Bizzarri, M., Boscardin, M., Calcagnile, L., Caprai, M., Caricato, A. P., Pablo, G. A., Crivellari, M., Cupparo, I., Cuttone, G., Dunand, S., Fanò, L., Gianfelici, B., Hammad, O., Movileanu-Ionica, M., Kanxheri, K., Large, M. J., Maruccio, G., Monteduro, A. G., . . . Wyrsch, N. (2022). Displacement damage in Hydrogenated Amorphous Silicon p-i-n diodes and charge selective contacts detectors. https://doi.org/10.36227/techrxiv.19555042.v2
MLA 9
Menichelli, M., et al. “Displacement damage in Hydrogenated Amorphous Silicon p-i-n diodes and charge selective contacts detectors.” 2022. https://doi.org/10.36227/techrxiv.19555042.v2.
Chicago
Menichelli, M., Marco Bizzarri, M. Boscardin, Lucio Calcagnile, M. Caprai, Anna Paola Caricato, Giuseppe Antonio Pablo, et al. 2022. “Displacement damage in Hydrogenated Amorphous Silicon p-i-n diodes and charge selective contacts detectors.” https://doi.org/10.36227/techrxiv.19555042.v2.
Harvard
Menichelli, M. et al. (2022) ‘Displacement damage in Hydrogenated Amorphous Silicon p-i-n diodes and charge selective contacts detectors’. doi:10.36227/techrxiv.19555042.v2.
IEEE
M. Menichelli et al., “Displacement damage in Hydrogenated Amorphous Silicon p-i-n diodes and charge selective contacts detectors,” 2022, doi: 10.36227/techrxiv.19555042.v2.
BibTeX
@misc{menichelli2022displacement,
title = {{Displacement damage in Hydrogenated Amorphous Silicon p-i-n diodes and charge selective contacts detectors}},
author = {Menichelli, M. and Bizzarri, Marco and Boscardin, M. and Calcagnile, Lucio and Caprai, M. and Caricato, Anna Paola and Pablo, Giuseppe Antonio and Crivellari, Michele and Cupparo, Ilaria and Cuttone, G. and Dunand, Sylvain and Fanò, L. and Gianfelici, Benedetta and Hammad, Omar and Movileanu-Ionica, Maria and Kanxheri, K. and Large, Matthew James and Maruccio, Giuseppe and Monteduro, Anna Grazia and Moscatelli, F. and Morozzi, A. and Papi, Andrea and Passeri, D. and Pedio, M. and Petasecca, Marco and Petringa, Giada and Peverini, Francesca and Quarta, Gianluca and Rizzato, Silvia and Rossi, A. and others},
year = {2022},
doi = {10.36227/techrxiv.19555042.v2},
url = {https://doi.org/10.36227/techrxiv.19555042.v2}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Topic and keywords
Physical Sciences › Physics and Astronomy › Nuclear and High Energy Physics › Particle Detector Development and Performance
- hydrogenated amorphous silicon
- PIN diodes
- charge-selective contacts
- radiation damage
- neutron irradiation
- leakage current
- X-ray dosimetry
- annealing
Work with this paper
Most-cited papers in Physics and Astronomy
- Generalized Gradient Approximation Made SimpleJohn P. Perdew, Kieron Burke, Matthias Ernzerhof · Physical Review Letters · 1996 · 217,345 citations
- Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis setGeorg Kresse, Jürgen Furthmüller · Physical review. B, Condensed matter · 1996 · 125,164 citations
- Density-functional thermochemistry. III. The role of exact exchangeAxel D. Becke · The Journal of Chemical Physics · 1993 · 104,772 citations
- Development of the Colle-Salvetti correlation-energy formula into a functional of the electron densityChengteh Lee, Weitao Yang, Robert G. Parr · Physical review. B, Condensed matter · 1988 · 101,730 citations
- Projector augmented-wave methodPeter E. Blöchl · Physical review. B, Condensed matter · 1994 · 93,520 citations
Questions about this paper
How do I cite this paper in APA style?
Menichelli, M., Bizzarri, M., Boscardin, M., Calcagnile, L., Caprai, M., Caricato, A. P., Pablo, G. A., Crivellari, M., Cupparo, I., Cuttone, G., Dunand, S., Fanò, L., Gianfelici, B., Hammad, O., Movileanu-Ionica, M., Kanxheri, K., Large, M. J., Maruccio, G., Monteduro, A. G., . . . Wyrsch, N. (2022). Displacement damage in Hydrogenated Amorphous Silicon p-i-n diodes and charge selective contacts detectors. https://doi.org/10.36227/techrxiv.19555042.v2
How many times has this paper been cited?
1 times, according to OpenAlex on 19 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access: sign in and open the PDF from this page.
Who wrote this paper?
M. Menichelli, Marco Bizzarri, M. Boscardin, Lucio Calcagnile, M. Caprai, Anna Paola Caricato, Giuseppe Antonio Pablo, Michele Crivellari, Ilaria Cupparo, G. Cuttone, Sylvain Dunand, L. Fanò and 24 more.
What is the DOI of this paper?
10.36227/techrxiv.19555042.v2, permanently at https://doi.org/10.36227/techrxiv.19555042.v2. Sign in and open it from this page.
Bibliographic data from OpenAlex (CC0), last checked 19 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.