Journal article · 2026 · Open access

Decoding Hydrogen-Bond Network of Electrolyte for Cryogenic Durable Aqueous Zinc-Ion Batteries

Xiyan Wei, Jinpeng Guan, Yongbiao Mu, Yuhan Zou, Xianbin Wei, Lin Yang, Quanyan Man, C. Y. Yang, Limin Zang, Jingyu Sun, Lin Zeng

Nano-Micro Letters, 18(1), 127 · Published 3 January 2026 · DOI 10.1007/s40820-025-01970-3

Open PDFView at the publisherCite this paper

In brief

“Decoding Hydrogen-Bond Network of Electrolyte for Cryogenic Durable Aqueous Zinc-Ion Batteries” is a 2026 journal article by Xiyan Wei and 10 co-authors, published in Nano-Micro Letters. OpenAlex counts 72 citations as of 25 November 2026, which puts it in the top 1% of works published in 2026 by citations. It is open access under a CC BY licence: the full text is free to read at Nano-Micro Letters.

Citations
72
Most cited in
2026 (72)
Field-weighted impact
73.54
References
68
Authors
11

Abstract

Aqueous zinc-ion batteries (AZIBs) hold great promise for next-generation energy storage but face challenges such as Zn dendrite growth, side reactions, and limited performance at low temperatures. Here, we propose an electrolyte design strategy that reconstructs the hydrogen-bond network through the synergistic effect of glycerol (GL) and methylsulfonamide (MSA), enabling the formation of a (100)-oriented Zn anode. This design significantly broadens the operating current and temperature windows of AZIBs. As a result, Zn||Zn symmetric cells exhibit remarkable cycling stability, achieving 4,000 h at 1 mA cm −2 and 600 h at 40 mA cm −2 (both at 1 mAh cm −2 capacity); even at −20 °C, Zn||Zn symmetric cells deliver ultra-stable cycling for over 5,400 h. Furthermore, Zn||VO 2 full cells retain 77.3% of their capacity after 2,000 cycles at 30 °C with a current density of 0.5 A g −1 and 85.4% capacity retention after 2,000 cycles at −20 °C and 0.25 A g −1 . These results demonstrate a robust pathway for enhancing the practicality and low-temperature adaptability of AZIBs.

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Wei, X., Guan, J., Mu, Y., Zou, Y., Wei, X., Yang, L., Man, Q., Yang, C. Y., Zang, L., Sun, J., & Zeng, L. (2026). Decoding Hydrogen-Bond Network of Electrolyte for Cryogenic Durable Aqueous Zinc-Ion Batteries. Nano-Micro Letters, 18(1), 127. https://doi.org/10.1007/s40820-025-01970-3

MLA 9

Wei, Xiyan, et al. “Decoding Hydrogen-Bond Network of Electrolyte for Cryogenic Durable Aqueous Zinc-Ion Batteries.” Nano-Micro Letters, vol. 18, no. 1, 2026, p. 127. https://doi.org/10.1007/s40820-025-01970-3.

Chicago

Wei, Xiyan, Jinpeng Guan, Yongbiao Mu, Yuhan Zou, Xianbin Wei, Lin Yang, Quanyan Man, et al. 2026. “Decoding Hydrogen-Bond Network of Electrolyte for Cryogenic Durable Aqueous Zinc-Ion Batteries.” Nano-Micro Letters 18 (1): 127. https://doi.org/10.1007/s40820-025-01970-3.

Harvard

Wei, X. et al. (2026) ‘Decoding Hydrogen-Bond Network of Electrolyte for Cryogenic Durable Aqueous Zinc-Ion Batteries’, Nano-Micro Letters, 18(1), p. 127. doi:10.1007/s40820-025-01970-3.

IEEE

X. Wei et al., “Decoding Hydrogen-Bond Network of Electrolyte for Cryogenic Durable Aqueous Zinc-Ion Batteries,” Nano-Micro Letters, vol. 18, no. 1, p. 127, 2026, doi: 10.1007/s40820-025-01970-3.

BibTeX

@article{wei2026decoding,
  title     = {{Decoding Hydrogen-Bond Network of Electrolyte for Cryogenic Durable Aqueous Zinc-Ion Batteries}},
  author    = {Wei, Xiyan and Guan, Jinpeng and Mu, Yongbiao and Zou, Yuhan and Wei, Xianbin and Yang, Lin and Man, Quanyan and Yang, C. Y. and Zang, Limin and Sun, Jingyu and Zeng, Lin},
  journal   = {Nano-Micro Letters},
  year      = {2026},
  volume    = {18},
  number    = {1},
  pages     = {127},
  doi       = {10.1007/s40820-025-01970-3},
  url       = {https://doi.org/10.1007/s40820-025-01970-3}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Topic and keywords

Physical Sciences › Engineering › Electrical and Electronic Engineering › Aqueous and Flow Batteries

  • aqueous zinc-ion batteries
  • hydrogen bond network
  • electrolyte design
  • glycerol
  • zinc dendrite suppression
  • low-temperature cycling stability
  • cycling stability

Work with this paper

Most-cited papers in Engineering

All highly cited Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Wei, X., Guan, J., Mu, Y., Zou, Y., Wei, X., Yang, L., Man, Q., Yang, C. Y., Zang, L., Sun, J., & Zeng, L. (2026). Decoding Hydrogen-Bond Network of Electrolyte for Cryogenic Durable Aqueous Zinc-Ion Batteries. Nano-Micro Letters, 18(1), 127. https://doi.org/10.1007/s40820-025-01970-3

How many times has this paper been cited?

72 times, according to OpenAlex on 25 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

Yes. It is open access at Nano-Micro Letters: sign in and open the PDF from this page.

Who wrote this paper?

Xiyan Wei, Jinpeng Guan, Yongbiao Mu, Yuhan Zou, Xianbin Wei, Lin Yang, Quanyan Man, C. Y. Yang, Limin Zang, Jingyu Sun, Lin Zeng.

What is the DOI of this paper?

10.1007/s40820-025-01970-3, permanently at https://doi.org/10.1007/s40820-025-01970-3. Sign in and open it from this page.

Bibliographic data from OpenAlex (CC0), last checked 25 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.