Atomic Layer Deposition and Atomic Scale Processing of Molybdenum Oxide and Sulfide Thin Films
ScholarWorks (Boise State University) · Published 1 December 2025 · DOI 10.18122/td.2458.boisestate
In brief
“Atomic Layer Deposition and Atomic Scale Processing of Molybdenum Oxide and Sulfide Thin Films” is a 2025 dissertation by Wesley Jen, published in ScholarWorks (Boise State University). OpenAlex counts 0 citations as of 17 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.
- Citations
- 0
- Authors
- 1
Abstract
As new microelectronic device architectures continue to shrink in size while simultaneously increasing in complexity and performance, traditional channel materials such as polysilicon begin to face increasing difficulty in meeting performance goals. Layered two-dimensional (2D) transition metal dichalcogenides (TMDs) such as molybdenum disulfide (MoS2) are prime candidates to meet these challenges. Although monolayer MoS2 is… Read the full abstract at the publisher.
Excerpt. This paper is not open access.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Jen, W. (2025). Atomic Layer Deposition and Atomic Scale Processing of Molybdenum Oxide and Sulfide Thin Films. ScholarWorks (Boise State University). https://doi.org/10.18122/td.2458.boisestate
MLA 9
Jen, Wesley. “Atomic Layer Deposition and Atomic Scale Processing of Molybdenum Oxide and Sulfide Thin Films.” ScholarWorks (Boise State University), 2025. https://doi.org/10.18122/td.2458.boisestate.
Chicago
Jen, Wesley. 2025. “Atomic Layer Deposition and Atomic Scale Processing of Molybdenum Oxide and Sulfide Thin Films.” ScholarWorks (Boise State University). https://doi.org/10.18122/td.2458.boisestate.
Harvard
Jen, W. (2025) ‘Atomic Layer Deposition and Atomic Scale Processing of Molybdenum Oxide and Sulfide Thin Films’, ScholarWorks (Boise State University). doi:10.18122/td.2458.boisestate.
IEEE
W. Jen, “Atomic Layer Deposition and Atomic Scale Processing of Molybdenum Oxide and Sulfide Thin Films,” ScholarWorks (Boise State University), 2025, doi: 10.18122/td.2458.boisestate.
BibTeX
@phdthesis{jen2025atomic,
title = {{Atomic Layer Deposition and Atomic Scale Processing of Molybdenum Oxide and Sulfide Thin Films}},
author = {Jen, Wesley},
year = {2025},
doi = {10.18122/td.2458.boisestate},
url = {https://doi.org/10.18122/td.2458.boisestate}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Topic and keywords
Physical Sciences › Materials Science › Materials Chemistry › 2D Materials and Applications
- atomic layer deposition
- MoS2
- monolayer MoS2
- molybdenum oxide
- transition metal dichalcogenides
- two-dimensional materials
- thin film deposition
- conformal films
Work with this paper
Most-cited papers in Materials Science
- Electric Field Effect in Atomically Thin Carbon FilmsKostya S. Novoselov, Andre K. Geim, Sergey V. Morozov and 5 more · Science · 2004 · 67,474 citations
- Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenidesROBERT D. SHANNON · Acta Crystallographica Section A · 1976 · 66,944 citations
- Ab initio molecular dynamics for liquid metalsGeorg Kresse, J. Häfner · Physical review. B, Condensed matter · 1993 · 46,320 citations
- Helical microtubules of graphitic carbonSumio Iijima · Nature · 1991 · 43,639 citations
- The rise of grapheneAndre K. Geim, Kostya S. Novoselov · Nature Materials · 2007 · 40,328 citations
Questions about this paper
How do I cite this paper in APA style?
Jen, W. (2025). Atomic Layer Deposition and Atomic Scale Processing of Molybdenum Oxide and Sulfide Thin Films. ScholarWorks (Boise State University). https://doi.org/10.18122/td.2458.boisestate
How many times has this paper been cited?
0 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.
Who wrote this paper?
Wesley Jen.
What is the DOI of this paper?
10.18122/td.2458.boisestate, permanently at https://doi.org/10.18122/td.2458.boisestate. Sign in and open it from this page.
Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.