Journal article · 2011 · Open access
Aluminum-doped zinc oxide films grown by atomic layer deposition for transparent electrode applications
Journal of Materials Science Materials in Electronics, 22(12), 1810–1815 · Published 18 April 2011 · DOI 10.1007/s10854-011-0367-0
In brief
“Aluminum-doped zinc oxide films grown by atomic layer deposition for transparent electrode applications” is a 2011 journal article by Grzegorz Łuka and 6 co-authors, published in Journal of Materials Science Materials in Electronics. OpenAlex counts 126 citations as of 20 November 2026, which puts it in the top 7% of works published in 2011 by citations. It is open access under a CC BY-NC licence: the full text is free to read at Journal of Materials Science Materials in Electronics.
- Citations
- 126
- Most cited in
- 2017 (15)
- Field-weighted impact
- 3.47
- References
- 22
- Authors
- 7
Abstract
We obtained zinc oxide films doped with aluminum using atomic layer deposition (ALD). Their morphology, growth mode, optical and electrical properties are studied. Al content dependence is analyzed. Carrier scattering mechanisms in ZnO:Al (AZO) films are investigated from conductivity versus temperature measurements. We also discuss how the film thickness affects its resistivity and optical transmission. The obtained film resistivities, i.e. 7 × 10−4 Ωcm, belong to the lowest reported so far for transparent ZnO:Al films grown by the ALD method.
Cite this paper
Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.
APA 7
Łuka, G., Krajewski, T., Witkowski, B., Wisz, G., Virt, I., Guziewicz, E., & Godlewski, M. (2011). Aluminum-doped zinc oxide films grown by atomic layer deposition for transparent electrode applications. Journal of Materials Science Materials in Electronics, 22(12), 1810–1815. https://doi.org/10.1007/s10854-011-0367-0
MLA 9
Łuka, Grzegorz, et al. “Aluminum-doped zinc oxide films grown by atomic layer deposition for transparent electrode applications.” Journal of Materials Science Materials in Electronics, vol. 22, no. 12, 2011, pp. 1810–1815. https://doi.org/10.1007/s10854-011-0367-0.
Chicago
Łuka, Grzegorz, T. Krajewski, B.S. Witkowski, G. Wisz, I.S. Virt, E. Guziewicz, and M. Godlewski. 2011. “Aluminum-doped zinc oxide films grown by atomic layer deposition for transparent electrode applications.” Journal of Materials Science Materials in Electronics 22 (12): 1810–1815. https://doi.org/10.1007/s10854-011-0367-0.
Harvard
Łuka, G. et al. (2011) ‘Aluminum-doped zinc oxide films grown by atomic layer deposition for transparent electrode applications’, Journal of Materials Science Materials in Electronics, 22(12), pp. 1810–1815. doi:10.1007/s10854-011-0367-0.
IEEE
G. Łuka et al., “Aluminum-doped zinc oxide films grown by atomic layer deposition for transparent electrode applications,” Journal of Materials Science Materials in Electronics, vol. 22, no. 12, pp. 1810–1815, 2011, doi: 10.1007/s10854-011-0367-0.
BibTeX
@article{uka2011aluminum,
title = {{Aluminum-doped zinc oxide films grown by atomic layer deposition for transparent electrode applications}},
author = {Łuka, Grzegorz and Krajewski, T. and Witkowski, B.S. and Wisz, G. and Virt, I.S. and Guziewicz, E. and Godlewski, M.},
journal = {Journal of Materials Science Materials in Electronics},
year = {2011},
volume = {22},
number = {12},
pages = {1810--1815},
doi = {10.1007/s10854-011-0367-0},
url = {https://doi.org/10.1007/s10854-011-0367-0}
}
Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)
Citations by year
| Year | Citations | Share of the best year |
|---|---|---|
| 2017 | 15 | |
| 2018 | 14 | |
| 2019 | 10 | |
| 2020 | 7 | |
| 2021 | 10 | |
| 2022 | 6 | |
| 2023 | 7 | |
| 2024 | 7 | |
| 2025 | 2 | |
| 2026 | 2 |
Its field-weighted citation impact is 3.47: it has been cited 3.47 times as often as the average work of the same field, type and year (1.00 is the world average).
Topic and keywords
Physical Sciences › Materials Science › Materials Chemistry › ZnO doping and properties
- Al-doped ZnO
- transparent electrodes
- atomic layer deposition
- carrier scattering mechanisms
- electrical resistivity
- optical transmission
- film thickness dependence
- temperature dependence of conductivity
Work with this paper
Most-cited papers in Materials Science
- Electric Field Effect in Atomically Thin Carbon FilmsKostya S. Novoselov, Andre K. Geim, Sergey V. Morozov and 5 more · Science · 2004 · 67,474 citations
- Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenidesROBERT D. SHANNON · Acta Crystallographica Section A · 1976 · 66,944 citations
- Ab initio molecular dynamics for liquid metalsGeorg Kresse, J. Häfner · Physical review. B, Condensed matter · 1993 · 46,320 citations
- Helical microtubules of graphitic carbonSumio Iijima · Nature · 1991 · 43,639 citations
- The rise of grapheneAndre K. Geim, Kostya S. Novoselov · Nature Materials · 2007 · 40,328 citations
Questions about this paper
How do I cite this paper in APA style?
Łuka, G., Krajewski, T., Witkowski, B., Wisz, G., Virt, I., Guziewicz, E., & Godlewski, M. (2011). Aluminum-doped zinc oxide films grown by atomic layer deposition for transparent electrode applications. Journal of Materials Science Materials in Electronics, 22(12), 1810–1815. https://doi.org/10.1007/s10854-011-0367-0
How many times has this paper been cited?
126 times, according to OpenAlex on 20 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.
Is this paper free to read?
Yes. It is open access at Journal of Materials Science Materials in Electronics: sign in and open the PDF from this page.
Who wrote this paper?
Grzegorz Łuka, T. Krajewski, B.S. Witkowski, G. Wisz, I.S. Virt, E. Guziewicz, M. Godlewski.
What is the DOI of this paper?
10.1007/s10854-011-0367-0, permanently at https://doi.org/10.1007/s10854-011-0367-0. Sign in and open it from this page.
Bibliographic data from OpenAlex (CC0), last checked 20 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.