Advanced nanoindentation testing: Beyond the Oliver–Pharr method

Verena Maier‐Kiener, Sandra Korte‐Kerzel

MRS Bulletin, 50(6), 689–694 · Published 22 May 2025 · DOI 10.1557/s43577-025-00921-y

View at the publisherCite this paper

In brief

“Advanced nanoindentation testing: Beyond the Oliver–Pharr method” is a 2025 journal article by Verena Maier‐Kiener and Sandra Korte‐Kerzel, published in MRS Bulletin. OpenAlex counts 15 citations as of 16 November 2026, which puts it in the top 3% of works published in 2025 by citations. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
15
Most cited in
2026 (10)
Field-weighted impact
3.95
References
35
Authors
2

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Maier‐Kiener, V., & Korte‐Kerzel, S. (2025). Advanced nanoindentation testing: Beyond the Oliver–Pharr method. MRS Bulletin, 50(6), 689–694. https://doi.org/10.1557/s43577-025-00921-y

MLA 9

Maier‐Kiener, Verena, and Sandra Korte‐Kerzel. “Advanced nanoindentation testing: Beyond the Oliver–Pharr method.” MRS Bulletin, vol. 50, no. 6, 2025, pp. 689–694. https://doi.org/10.1557/s43577-025-00921-y.

Chicago

Maier‐Kiener, Verena and Sandra Korte‐Kerzel. 2025. “Advanced nanoindentation testing: Beyond the Oliver–Pharr method.” MRS Bulletin 50 (6): 689–694. https://doi.org/10.1557/s43577-025-00921-y.

Harvard

Maier‐Kiener, V. and Korte‐Kerzel, S. (2025) ‘Advanced nanoindentation testing: Beyond the Oliver–Pharr method’, MRS Bulletin, 50(6), pp. 689–694. doi:10.1557/s43577-025-00921-y.

IEEE

V. Maier‐Kiener and S. Korte‐Kerzel, “Advanced nanoindentation testing: Beyond the Oliver–Pharr method,” MRS Bulletin, vol. 50, no. 6, pp. 689–694, 2025, doi: 10.1557/s43577-025-00921-y.

BibTeX

@article{maierkiener2025advanced,
  title     = {{Advanced nanoindentation testing: Beyond the Oliver–Pharr method}},
  author    = {Maier‐Kiener, Verena and Korte‐Kerzel, Sandra},
  journal   = {MRS Bulletin},
  year      = {2025},
  volume    = {50},
  number    = {6},
  pages     = {689--694},
  doi       = {10.1557/s43577-025-00921-y},
  url       = {https://doi.org/10.1557/s43577-025-00921-y}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Topic and keywords

Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics

  • nanoindentation
  • Oliver-Pharr method
  • contact stiffness
  • hardness
  • elastic modulus
  • instrumented indentation
  • heterogeneous materials
  • composite materials

Work with this paper

Most-cited papers in Engineering

All highly cited Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Maier‐Kiener, V., & Korte‐Kerzel, S. (2025). Advanced nanoindentation testing: Beyond the Oliver–Pharr method. MRS Bulletin, 50(6), 689–694. https://doi.org/10.1557/s43577-025-00921-y

How many times has this paper been cited?

15 times, according to OpenAlex on 16 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Verena Maier‐Kiener, Sandra Korte‐Kerzel.

What is the DOI of this paper?

10.1557/s43577-025-00921-y. The permanent link is https://doi.org/10.1557/s43577-025-00921-y.

Bibliographic data from OpenAlex (CC0), last checked 16 November 2026. ResearchGuru does not host this paper; the links go to the publisher or the repository that does.