Journal article · 2016

A direct atomic layer deposition method for growth of ultra-thin lubricant tungsten disulfide films

Yongfeng Sun, Zhimin Chai, Xinchun Lu, Dannong He

Science China Technological Sciences, 60(1), 51–57 · Published 23 November 2016 · DOI 10.1007/s11431-016-0538-x

View at the publisherCite this paper

In brief

“A direct atomic layer deposition method for growth of ultra-thin lubricant tungsten disulfide films” is a 2016 journal article by Yongfeng Sun and 3 co-authors, published in Science China Technological Sciences. OpenAlex counts 20 citations as of 17 November 2026. The publisher's version is not open access, and OpenAlex records no free legal copy.

Citations
20
Most cited in
2020 (5)
Field-weighted impact
1.44
References
36
Authors
4

Cite this paper

Formatted from the catalogue record. Check names, capitals and page numbers against the paper before you submit.

APA 7

Sun, Y., Chai, Z., Lu, X., & He, D. (2016). A direct atomic layer deposition method for growth of ultra-thin lubricant tungsten disulfide films. Science China Technological Sciences, 60(1), 51–57. https://doi.org/10.1007/s11431-016-0538-x

MLA 9

Sun, Yongfeng, et al. “A direct atomic layer deposition method for growth of ultra-thin lubricant tungsten disulfide films.” Science China Technological Sciences, vol. 60, no. 1, 2016, pp. 51–57. https://doi.org/10.1007/s11431-016-0538-x.

Chicago

Sun, Yongfeng, Zhimin Chai, Xinchun Lu, and Dannong He. 2016. “A direct atomic layer deposition method for growth of ultra-thin lubricant tungsten disulfide films.” Science China Technological Sciences 60 (1): 51–57. https://doi.org/10.1007/s11431-016-0538-x.

Harvard

Sun, Y. et al. (2016) ‘A direct atomic layer deposition method for growth of ultra-thin lubricant tungsten disulfide films’, Science China Technological Sciences, 60(1), pp. 51–57. doi:10.1007/s11431-016-0538-x.

IEEE

Y. Sun, Z. Chai, X. Lu, and D. He, “A direct atomic layer deposition method for growth of ultra-thin lubricant tungsten disulfide films,” Science China Technological Sciences, vol. 60, no. 1, pp. 51–57, 2016, doi: 10.1007/s11431-016-0538-x.

BibTeX

@article{sun2016direct,
  title     = {{A direct atomic layer deposition method for growth of ultra-thin lubricant tungsten disulfide films}},
  author    = {Sun, Yongfeng and Chai, Zhimin and Lu, Xinchun and He, Dannong},
  journal   = {Science China Technological Sciences},
  year      = {2016},
  volume    = {60},
  number    = {1},
  pages     = {51--57},
  doi       = {10.1007/s11431-016-0538-x},
  url       = {https://doi.org/10.1007/s11431-016-0538-x}
}

Download for a reference manager: BibTeX (.bib) · RIS for Zotero, Mendeley and EndNote (.ris)

Citations by year

YearCitationsShare of the best year
201711
201822
201944
202055
202111
202233
202311
202422
202511

Its field-weighted citation impact is 1.44: it has been cited 1.44 times as often as the average work of the same field, type and year (1.00 is the world average).

Topic and keywords

Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics

  • tungsten disulfide
  • WS2 thin films
  • atomic layer deposition
  • lubricant coatings
  • tungsten hexacarbonyl
  • crystal orientation
  • (002) orientation
  • friction coefficient

Work with this paper

Most-cited papers in Engineering

All highly cited Engineering papers

Questions about this paper

How do I cite this paper in APA style?

Sun, Y., Chai, Z., Lu, X., & He, D. (2016). A direct atomic layer deposition method for growth of ultra-thin lubricant tungsten disulfide films. Science China Technological Sciences, 60(1), 51–57. https://doi.org/10.1007/s11431-016-0538-x

How many times has this paper been cited?

20 times, according to OpenAlex on 17 November 2026. Google Scholar and Scopus count different sets of sources, so their numbers differ.

Is this paper free to read?

OpenAlex records no free legal copy. Check your library's access, the authors' pages or a repository, or ask the corresponding author for a copy.

Who wrote this paper?

Yongfeng Sun, Zhimin Chai, Xinchun Lu, Dannong He.

What is the DOI of this paper?

10.1007/s11431-016-0538-x, permanently at https://doi.org/10.1007/s11431-016-0538-x. Sign in and open it from this page.

Bibliographic data from OpenAlex (CC0), last checked 17 November 2026. ResearchGuru does not host this paper; once you are signed in, the links open it at the publisher or the repository that does.